Abstract
The poor interface incompatibility with Li anode and low ionic conductivity have hindered perovskite-type electrolyte’s practical application. In this work, solid electrolytes of Li 0.33La 0.557TiO 3 + x wt% Bi 2O 3 for solid state batteries were prepared by solid-phase sintering method. The ionic conductivity of LLTO reaches a maximum of 2.71 × 10 –5 S·cm –1 at 1 wt% Bi 2O 3 doping. The critical current density of Li 0.33La 0.557TiO 3 + 1 wt%Bi 2O 3 can reach 0.16 mA and still operate normally after 300 h of cycling. Li 0.33La 0.557TiO 3 + 1 wt% Bi 2O 3 solid-state battery displays a high initial discharge capacity of 133.1 mAh/g and capacity retention of 98.0% after 40 cycles.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Thermal Expansion and Ionic Conductivity
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Recent development in the field of ceramics solid-state electrolytes: I—oxide ceramic solid-state electrolytes [J]10.1007/s10008-022-05206-x ↗
2. All-solid-state lithium batteries with long cycle life [J]10.1016/j.matt.2021.11.010 ↗
3. Perovskite‐type Li‐ion solid electrolytes: a review [J]
4. Investigations on pure and Ag doped lithium lanthanum titanate (LLTO) nanocrystalline ceramic electrolytes for rechargeable lithium-ion batteries [J]10.1016/j.ceramint.2012.07.011 ↗
5. High Performance Single-Crystal Ni-Rich Cathode Modification via Crystalline LLTO Nanocoating for All-Solid-State Lithium Batteries [J]10.1021/acsami.1c18264 ↗
6. Few-layer bismuthene enabled solid-state Li batteries [J]. Energy Storage
7. The quest for the holy grail of solid-state lithium batteries [J]10.1039/D2EE00842D ↗
8. Effect of Sn or Ta doping on the microstructure and total conductivity of perovskite Li0.24La0.587TiO3 solid electrolyte [J]10.1016/j.jallcom.2020.156023 ↗
9. Revealing the dominant factor of domain boundary resistance on bulk conductivity in lanthanum lithium titanates [J]10.1016/j.jechem.2022.06.020 ↗
10. Exaggerated grain growth and the development of coarse-grained microstructures in lithium lanthanum titanate perovskite ceramics [J]10.1016/j.jeurceramsoc.2022.11.004 ↗
11. Moisture stability of sulfide solid-state electrolytes [J]
12. Lithium/sulfide all-solid-state batteries using sulfide electrolytes [J]10.1002/adma.202000751 ↗
13. Research progress and prospect in typical sulfide solid-state electrolytes [J]
14. Interface engineering of sulfide electrolytes for all-solid-state lithium batteries [J]10.1016/j.nanoen.2018.09.061 ↗
15. Designing composite polymer electrolytes for all-solid-state lithium batteries [J]. Current Opinion in
16. Polymer electrolytes and interfaces in solid-state lithium metal batteries [J]10.1016/j.mattod.2021.08.005 ↗
17. Research progress and application of PEO-based solid state polymer composite electrolytes [J]
18. Lithium lanthanum titanate single crystals: dependence of lithium-ion conductivity on crystal domain orientation [J]10.1021/acs.nanolett.2c01655 ↗
19. Short-range order and Li+ ion diffusion mechanisms in Li5La9□2(TiO3)16 (LLTO) [J]10.1016/j.ssi.2010.12.016 ↗
20. Structure, stability, and ionic conductivity of perovskite Li2x-ySr1−x-yLayTiO3 solid electrolytes [J]10.1016/j.ceramint.2019.11.277 ↗
21. Perovskite membranes with vertically aligned microchannels for all-solid-state lithium batteries [J]10.1002/aenm.201801433 ↗
22. Characterization of the Li-ionic conductivity of La(2/3−x)Li3xTiO3 ceramics used for all-solid-state batteries [J]10.1016/j.ssi.2015.05.027 ↗
23. Oriented Crystal Growth of La0.557Li0.330TiO3 in Bulk Ceramics Induced by LaAlO3 Single-Crystal Fibers [J]10.1021/acs.cgd.0c01518 ↗
24. Synthesis of textured Li0.33La0.55TiO3 solid electrolytes by molten salt method [J]10.1016/j.ceramint.2021.01.003 ↗
25. Comparative study of solid-state reaction and sol-gel process for synthesis of Zr-doped Li0.5La0.5TiO3 solid electrolytes [J]10.1007/s11581-016-1744-8 ↗
26. Atomistic Origin of Li-Ion Conductivity Reduction at (Li(3x)La(2/3−x))TiO(3) Grain Boundary [J]10.1021/acs.nanolett.1c02174 ↗
27. Influence of Li2O-B2O3 glass on ionic migration and interfacial properties of La2/3−xLi3xTiO3 solid electrolyte [J]10.1016/j.jallcom.2017.02.059 ↗
28. Sr Doped Amorphous LLTO as Solid Electrolyte Material [J]10.1149/1945-7111/ab8c87 ↗
29. Fluoroethylene carbonate-Li-ion enabling composite solid-state electrolyte and lithium metal interface self-healing for dendrite-free lithium deposition [J]
30. Structural origin of low Li-ion conductivity in perovskite solid-state electrolyte [J]
31. Enhanced Li+ conduction in perovskite Li3xLa2/3−x□1/3−2xTiO3 solid-electrolytes via microstructural engineering [J]10.1039/C7TA00196G ↗
32. Experimental and theoretical Raman study on the structure and microstructure of Li0.30La0.57TiO3 electrolyte prepared by the sol-gel method in acetic medium [J]10.1016/j.ceramint.2016.06.192 ↗
33. Characterization of thin film Li0.5La0.5Ti1−xAlxO3 electrolyte for all-solid-state Li-ion batteries [J]10.1016/j.ssi.2018.07.005 ↗
34. A correlation between formation enthalpy and ionic conductivity in perovskite-structured Li3xLa0.67−xTiO3 solid lithium ion conductors [J]
35. Order–disorder of the A-site ions and lithium ion conductivity in the perovskite solid solution La0.67−xLi3xTiO3 (x=0.11) 1 [J]10.1016/S0167-2738(99)00043-0 ↗
36. Polyvinylpyrrolidone-modified Bi2O3 and Bi2S3 nanocomposites for improved supercapacitive performance [J]
37. Ionic conduction, colossal permittivity and dielectric relaxation behavior of solid electrolyte Li3xLa2/3−xTiO3 ceramics [J]10.1016/j.jeurceramsoc.2018.05.023 ↗
38. LiF-Assisted Synthesis of Perovskite-Type Li0.35La0.55TiO3 Solid Electrolyte for Rechargeable Lithium-Metal Batteries [J]10.1007/s11664-021-09331-7 ↗
39. Tuning Solid Interfaces via Varying Electrolyte Distributions Enables High‐Performance Solid‐State Batteries [J]10.1002/eem2.12308 ↗
40. Lithium-Salt-Rich PEO/Li(0.3)La(0.557)TiO(3) Interpenetrating Composite Electrolyte with Three-Dimensional Ceramic Nano-Backbone for All-Solid-State Lithium-Ion Batteries [J]10.1021/acsami.8b06658 ↗
41. Synergistic effect of cation ordered structure and grain boundary engineering on long-term cycling of Li0.35La0.55TiO3-based solid batteries [J]10.1016/j.jeurceramsoc.2019.04.045 ↗
42. Nikhil B., Hans B., et al. Influence of bismuth oxide as a sintering aid on the densification of cold sintering of zirconia [J]. Ceramics International, 2023.
43. Effect of bismuth oxide as sintering aid for gadolinia-doped ceria at 1050℃ [J].
44. Low temperature synthesis of Li0.33La0.55TiO3 solid electrolyte with Al3+ doping by a modified Pechini method [J]10.1007/s11581-021-04422-1 ↗
45. Critical current density in solid-state lithium metal batteries: mechanism, influences, and strategies [J]10.1002/adfm.202009925 ↗
46. Expansion-Tolerant Lithium Anode with Built-In LiF-Rich Interface for Stable 400 Wh kg–1 Lithium Metal Pouch Cells [J]10.1021/acsmaterialslett.2c00443 ↗
47. All-solid-state lithium batteries with sulfide electrolytes and oxide cathodes [J]10.1007/s41918-020-00081-4 ↗
48. Lithium/sulfide all-solid-state batteries using sulfide electrolytes [J]10.1002/adma.202000751 ↗
49. Sulfide solid electrolytes for all-solid-state lithium batteries: Structure, conductivity, stability and application [J]10.1016/j.ensm.2018.02.020 ↗