Texture refinement and mechanical improvement in beam oscillation superimposed laser welding of TiAl-based alloy
Source abstract
Abstract
Cracking and coarse textured grains are responsible for insufficient mechanical properties of laser beam welded TiAl alloys. Conventional method for grain refinement such as addition of boride is suppressed by high cooling rate during laser welding. This article delineates texture refinement by laser beam oscillation for TiAl alloy. Large textured grains are formed with no beam oscillation. When the oscillation increases to 300 Hz, the vortex and turbulence severely disturb the welding pool solidification and cause reduction of grain size down to 41% of the size without oscillation. The size of textured grain does not show a further reduction with 500 Hz oscillation. Both ultimate tensile strength and elongation are improved with refined grain size.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · High-Temperature Coating Behaviors · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Appel · 2011
2. Processing and applications of intermetallic γ-TiAl-based alloys10.1002/1527-2648(200009)2:9<551::AID-ADEM551>3.0.CO;2-U ↗
3. Design, processing, microstructure, properties, and applications of advanced intermetallic TiAl alloys10.1002/adem.201200231 ↗
4. In situ study of phase transformations during laser-beam welding of a TiAl alloy for grain refinement and mechanical property optimization10.1016/j.intermet.2015.03.003 ↗
5. New insights into perovskite-Ti3AlC precipitate splitting in a Ti-45Al-5Nb-0.75C alloy by transmission electron microscopy10.1016/j.intermet.2018.06.006 ↗
6. Ordered intermetallic alloys, part III: Gamma titanium aluminides10.1007/BF03220745 ↗
7. Crack growth in a nearly fully-lamellar gamma TiAl alloy at 650 °C and 800 °C under constant load conditions10.1007/s11661-002-0270-7 ↗
8. New insights into high-temperature deformation and phase transformation mechanisms of lamellar structures in high Nb-containing TiAl alloys10.1016/j.actamat.2020.01.021 ↗
9. Evidence for deformation twinning of the D0(19)-alpha(2) phase in a high Nb containing TiAl alloy10.1016/j.intermet.2019.03.014 ↗
10. Microstructure and fracture toughness of a β phase containing TiAl alloy10.1016/j.intermet.2011.05.006 ↗
11. The effect of heat treatment on crack control and grain refinement in laser beam welded beta-solidifying TiAl-based alloy10.1016/j.intermet.2013.04.007 ↗
12. Friction weldability of a high Nb containing TiAl alloy10.3390/ma12213556 ↗
13. Microstructure and properties of friction welding joint of Ti-45Al-8.5Nb-0. 2W-0. 2B-0. 02Y alloy10.1016/j.intermet.2019.106540 ↗
14. Microstructural refinement of boron-containing beta-solidifying gamma-titanium aluminide alloys through heat treatments in the beta phase field10.1016/j.intermet.2012.08.010 ↗
15. Role of boron in TiAl alloy development: a review10.1007/s12598-015-0615-1 ↗
16. Appel · 2011
17. The mechanism of grain refinement in TiAl alloys by boron addition — an alternative hypothesis10.1016/S0966-9795(99)00063-1 ↗
18. Grain refinement by low boron additions in niobium-rich TiAl-based alloys10.1016/j.intermet.2008.04.019 ↗
19. Phase transformation and residual stress in a laser beam spot-welded TiAl-based alloy, metallurgical and materials transactions a-physical metallurgy and materials
20. Phase transformations during solidification of a laser-beam-welded TiAl alloy-an in situ synchrotron study, metallurgical and materials transactions a-physical metallurgy and materials
21. In situ observation of competitive growth of α grains during β → α transformation in laser beam manufactured TiAl alloys10.1016/j.matchar.2021.111371 ↗
22. Melt flow and microstructural characteristics in beam oscillation superimposed laser welding of 304 stainless steel10.1016/j.jmapro.2019.12.053 ↗
23. Grain refinement and laser energy distribution during laser oscillating welding of invar alloy
24. A study on laser beam oscillating welding characteristics for the 5083 aluminum alloy: morphology, microstructure and mechanical properties10.1016/j.jmapro.2020.01.018 ↗
25. Effects of beam oscillation modes on microstructure and mechanical properties of laser welded 2060 Al-Li alloy joints10.1016/j.optlastec.2021.107389 ↗
26. Numerical research on melt pool dynamics of oscillating laser-arc hybrid welding10.1016/j.ijheatmasstransfer.2021.122421 ↗
27. Investigation of in situ and conventional post-weld heat treatments on dual-laser-beam-welded gamma-TiAl-based alloy10.1002/adem.201200113 ↗
28. Effect of boron addition on tensile ductility in lamellar TiAl alloys10.1016/S0966-9795(02)00087-0 ↗
29. The effect of boron and alpha grain size on the massive transformation in Ti-46Al-8Nb-xB alloys10.1016/j.intermet.2005.12.003 ↗
30. Characterization of the variant selection occurring during the alpha ->beta ->alpha phase transformations of a cold rolled titanium sheet10.1016/S1359-6454(01)00351-2 ↗
31. Structure of TiB precipitates in laser deposited in situ, Ti-6Al-4V-TiB composites10.1016/j.matlet.2005.10.033 ↗
32. Nanoscale TiB precipitates in laser deposited Ti-matrix composites10.1016/j.scriptamat.2005.08.014 ↗
33. Formation of equiaxed alpha in TiB reinforced Ti alloy composites10.1016/j.scriptamat.2004.10.019 ↗
34. The role of ordered domains and slip mode of α2 phase in the plastic behaviour of TiAl crystals containing oriented lamellae10.1016/0956-7151(93)90163-M ↗
35. Dimensionless parameters controlling fluid flow in electromagnetic cold crucible10.1016/j.jmatprotec.2017.12.020 ↗
36. Effect of beam oscillating behavior on pore inhibition and microstructure evolution mechanisms of laser welded Q235 steel10.1016/j.jmrt.2021.02.033 ↗
37. Surface tension and viscosity of industrial Ti-alloys measured by the oscillating drop method on board parabolic flights10.1515/HTMP.2008.27.6.401 ↗