journal article·2013-10

Optimization of chemical compositions in low-carbon Al-killed enamel steel produced by ultra-fast continuous annealing

Futao Dong, Linxiu Du, Xianghua Liu, Fei Xue

Publisher page

Abstract

The influence of Mn,S and B contents on microstructural characteristics, mechanical properties and hydrogen trapping ability of low-carbon Al-killed enamel steel was investigated. The materials were produced and processed in a laboratory and the ultra-fast continuous annealing processing was performed using a continuous annealing simulator. It was found that increasing Mn,S contents in steel can improve its hydrogen trapping ability which is attributed by refined ferrite grains, more dispersed cementite and added MnS inclusions. Nevertheless, it deteriorates mechanical properties of steel sheet. Addition of trace boron results in both good mechanical properties and significantly improved hydrogen trapping ability. The boron combined with nitrogen segregating at grain boundaries, cementite and MnS inclusions, provides higher amount of attractive hydrogen trapping sites and raises the activation energy for hydrogen desorption from them.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Continuously cast steel sheet for enamelling and technical properties of hot and cold rolled sheet
2. New type cold rolled steel sheet for enamelling produced by the continuous casting method
3. A quantitative analysis of hydrogen trapping10.1007/BF02661939 ↗
4. A classification of hydrogen traps10.1007/BF02812023 ↗
5. Thermal analysis of trapped hydrogen in pure iron10.1007/BF02642424 ↗
6. Effect of cold working on the hydrogen trapping phenomena in pure iron10.1007/BF02664812 ↗
7. The influence of microstructure on hydrogen transport in carbon steels10.1016/0010-938X(96)00109-6 ↗
8. A critical-strain criterion for hydrogen embrittlement of cold-drawn ultrafine pearlitic steel10.1007/s11661-002-0217-z ↗
9. Effects of sulfide inclusion on hydrogen transport in steels10.1016/0167-577X(95)00068-2 ↗
10. Hydrogen diffusion and trapping process around MnS precipitates in α-Fe examined by tritium autoradiography10.1016/j.jallcom.2007.02.005 ↗
11. Influences of Mn on recrystallization behavior and annealing texture formation in ultralow-carbon and low-carbon steels10.2355/isijinternational.34.85 ↗
12. Microstructural evolution during batch annealing of boron containing aluminum-killed steel10.1007/s10853-009-3499-3 ↗
13. Influence of boron on strain hardening behaviour and ductility of low carbon hot rolled steel10.1016/j.msea.2011.06.030 ↗
14. The absorption and diffusion of hydrogen in palladium10.1098/rspa.1962.0205 ↗
15. The development of a ceramic sensor for the prediction of hydrogen attack10.1016/0010-938X(95)00150-I ↗
16. Effect of manganese on aging in low carbon sheet steels10.2355/isijinternational.37.74 ↗
17. Effect of morphological change of carbide on elongation of boron-bearing Al-killed steel sheets10.2355/isijinternational.41.900 ↗
18. The effect of the microscale distribution of boron on the yield strength of C–Mn steels subjected to neutron irradiation10.1016/S1359-6454(02)00277-X ↗
19. Hydrogen solubility, diffusivity and trapping in a tempered Fe–C–Cr martensitic steel under various mechanical stress states10.1016/j.msea.2011.11.084 ↗