Simultaneous improvement of corrosion and wear resistance of Fe–Mn–Al–C lightweight steels: The role of Cr/Mo
Source abstract
Abstract
Fe–Mn–Al–C lightweight steel has promising applications due to its low density and excellent mechanical properties. This study investigates the influence of Cr/Mo on the electrochemical corrosion and wear behavior of lightweight steel. The results showed that adding Cr/Mo significantly improved the corrosion resistance in NaCl/NaHSO 3 solution. This improvement was attributed to the presence of protective Cr/Mo oxides and the reduction of harmful Mn oxides, which increased the compactness and charge transfer resistance of the oxide film. The primary wear types of lightweight steels include abrasive, adhesive, fatigue and oxidative wear. The wear test results showed that adding Cr/Mo improved the wear resistance of lightweight steel, which can be attributed to the increased toughness and hardness gradient.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Improved corrosion and wear resistance of micro-arc oxidation coatings on the 2024 aluminum alloy by incorporation of quasi-two-dimensional sericite microplates10.1016/j.apsusc.2022.152693 ↗
2. Wear and corrosion of an additively-manufactured AlMgScZrMn alloy10.1016/j.matchar.2023.112829 ↗
3. Enhanced corrosion and wear resistances in a precipitate-hardened magnesium alloy by laser surface remelting10.1016/j.matchar.2022.112306 ↗
4. Effects of (Ti, Mo) C particles on the abrasive wear -corrosion of low alloy martensitic steel10.1016/j.wear.2022.204288 ↗
5. Cobalt-based bulk glassy alloy with ultrahigh strength and soft magnetic properties10.1038/nmat982 ↗
6. Microstructural characterization of Hadfield austenitic manganese steel10.1007/s10853-008-2759-y ↗
7. Rolling contact fatigue of Hadfield steel X120Mn1210.1016/j.wear.2010.07.001 ↗
8. Hot deformation characterization of duplex low-density steel through 3D processing map development10.1016/j.matchar.2015.07.028 ↗
9. Microstructure and mechanical properties of a Fe–30Mn–10Al–1.5C–xBe (x = 0, 0.5, 1.0, 1.5) Be low-density steels10.1016/j.matchar.2022.112643 ↗
10. The effect of Cr content on intragranular κ-carbide precipitation in Fe-Mn-Al-(Cr)-C low-density steels: a multiscale investigation10.1016/j.matchar.2022.111801 ↗
11. Tensile deformation behavior related with strain-induced martensitic transformation in a duplex Fe-Mn-Al-C low-density steel10.1016/j.matchar.2022.111954 ↗
12. The influence of silicon and aluminum alloying on the lattice parameter and stacking fault energy of austenitic steel10.1016/j.scriptamat.2014.07.019 ↗
13. Effect of alloying chemistry on the lattice constant of austenitic Fe-Mn-Al-C alloys10.1016/0956-716X(94)90611-4 ↗
14. Physical and mechanical properties of iron-aluminium-(Mn, Si) lightweight steels10.1051/metal:2000110 ↗
15. Current state of Fe-Mn-Al-C low density steels10.1016/j.pmatsci.2017.05.002 ↗
16. Supra-ductile and high-strength manganese-TRIP/TWIP steels for high energy absorption purposes10.2355/isijinternational.43.438 ↗
17. Effect of ferrite on corrosion of Fe-Mn-Al alloys in sodium chloride solution10.5006/1.3293550 ↗
18. Effect of Mn additions on the corrosion behaviour of TWIP Fe-Mn-Al-Si austenitic steel in chloride solution10.1016/j.corsci.2019.04.026 ↗
19. A novel high-strength, high-ductility and high-corrosion-resistance FeAlMnC low-density alloy10.1016/j.scriptamat.2012.10.034 ↗
20. The influence of aluminum on microstructure, mechanical properties and wear performance of Fe–14%Mn–1.05%C manganese steel10.1016/j.jmrt.2021.10.054 ↗
21. Microstructure and tribological property of selective laser melted Fe-Mn-Al-C alloy10.1016/j.matlet.2020.127699 ↗
22. Effect of normal load on abrasive wear resistance and wear micromechanisms in FeMnAlC alloy and other austenitic steels10.1016/j.wear.2015.11.019 ↗
23. Microstructure and wear behavior of a Cr-Mo-Nb alloyed manganese steel10.1016/j.jmrt.2020.08.048 ↗
24. Characterisation of wear behaviour of different microstructures in Ni–Cr–Mo–V steel10.1016/j.wear.2006.12.014 ↗
25. Influences of Mo on stress corrosion cracking susceptibility of newly developed FeCrMnNiNC-based lean austenitic stainless steels10.1016/j.matchar.2016.08.006 ↗
26. In vitro corrosion behaviour of Ti–Nb–Sn shape memory alloys in Ringer’s physiological solution10.1007/s10856-012-4560-3 ↗
27. Synergistic effects of fluoride and chloride on general corrosion behavior of AISI 316 stainless steel and pure titanium in H2SO4 solutions10.1016/j.corsci.2017.10.028 ↗
28. A comparative study of primary and secondary passive films formed on AM355 stainless steel in 0.1M NaOH10.1016/j.apsusc.2017.08.151 ↗
29. Effect of Al on the microstructure and corrosion resistance of high-Mn steel10.1016/j.matlet.2022.132286 ↗
30. Enhancing pitting corrosion resistance of severely cold-worked high nitrogen austenitic stainless steel by nitric acid passivation10.1149/2.0211913jes ↗
31. Effect of nitrogen alloying on the semiconducting properties of passive films and metastable pitting susceptibility of 316L and 316LN stainless steels10.1016/j.matchemphys.2010.02.033 ↗
32. High temperature oxidation of Fe–Al and Fe–Cr–Al alloys: the role of Cr as a chemically active element10.1016/j.corsci.2010.06.019 ↗
33. Element-resolved electrochemical analysis of the passivity of additively manufactured stainless steel 316L10.1016/j.corsci.2021.109576 ↗
34. Synthesis of titanium oxide nanotubes and their decoration by MnO nanoparticles for biomedical applications10.1016/j.ceramint.2019.06.177 ↗
35. Stability, reactivity and breakdown of passive films. Problems of recent and future research10.1016/S0013-4686(00)00347-9 ↗
36. Electrochemical properties of Fe-Cr-Mo alloys and Fe2O3-Cr2O3-MoO2 artificial passivation films in 1 M HCl
37. Growth of corrosion pits on stainless steel in chloride solution containing dilute sulphate10.1016/0010-938X(92)90191-5 ↗
38. The role of Mo in the chemical composition and semiconductive behaviour of oxide films formed on stainless steels10.1016/S0010-938X(98)00126-7 ↗
39. Effects of alloying concentration on the aqueous corrosion and passivation of aluminum-manganese-molybdenum concentrated alloys10.1016/j.corsci.2022.110137 ↗
40. Novel Mo-modified medium entropy alloys achieving enhanced corrosion resistance in acidic solution10.1016/j.corsci.2023.111094 ↗
41. New insight into the dry rolling-sliding wear mechanism of carbide-free bainitic and pearlitic steel10.1016/j.wear.2019.202943 ↗
42. Wear behavior and the corresponding work hardening characteristics of Hadfield steel10.1016/j.triboint.2018.01.044 ↗
43. Unraveling the significant role of retained austenite on the dry sliding wear behavior of medium manganese steel10.1016/j.wear.2021.203745 ↗
44. Effect of loading on microstructure and friction and wear behavior of an austenite lightweight steel10.1016/j.triboint.2022.108006 ↗
45. Nanoindentation studies of materials10.1016/S1369-7021(06)71495-X ↗
46. Oliver–Pharr indentation method in determining elastic moduli of shape memory alloys—a phase transformable material10.1016/j.jmps.2013.05.007 ↗
47. Contact and rubbing of flat surfaces10.1063/1.1721448 ↗
48. Effect of counterpart material on the tribological properties of Zr-based bulk metallic glass under relatively heavy loads10.1016/j.wear.2015.10.018 ↗
49. Effects of composition and microstructure on the abrasive wear performance of quenched wear resistant steels10.1016/j.wear.2014.06.003 ↗