journal article·2026-10

Microstructural evolution and cryogenic toughness degradation in the heat-affected zone of Fe–28Mn–7Al–0.7C austenitic lightweight steel welded joints

Lei Yang, Shaoxian Zheng, Tongbang An, Zhilong Cao, Yue Zuo, Chengyong Ma

Publisher page

Abstract

In this study, Fe–28Mn–7Al–0.7C austenitic lightweight steel joints were fabricated by gas metal arc welding (GMAW) to clarify the origin of cryogenic toughness degradation in the heat-affected zone (HAZ). The microstructure, liquation cracking behavior, and cryogenic fracture mechanisms of the coarse-grained heat-affected zone (CGHAZ), fine-grained heat-affected zone (FGHAZ), and base metal (BM) were comparatively investigated. The results showed that both the BM and HAZ were dominated by austenite, and no additional phase transformation was detected after the welding thermal cycle. Abnormal grain growth occurred in the CGHAZ, where the average grain size reached 35.28 μm. Liquation cracks were mainly distributed along CGHAZ grain boundaries and initiated and propagated along Mn-segregation bands parallel to the rolling direction. At -196 °C, the impact absorbed energy of the BM was 228 J, whereas those of the CGHAZ and FGHAZ decreased sharply to 20 J and 34 J, respectively, indicating severe deterioration of cryogenic toughness in the HAZ. This degradation was mainly attributed to grain coarsening, which reduced crack propagation resistance; Mn-segregation bands, which induced local liquation and promoted grain-boundary liquation cracking; and κ-carbide precipitation, which further weakened grain-boundary cohesion. In addition, the superposition of tensile stress induced by molten pool shrinkage and welding restraint stress accelerated crack initiation. Strong texture and a reduced fraction of high-angle grain boundaries further limited crack deflection, enabling continuous crack propagation along low-resistance paths. This study provides a theoretical basis for evaluating the cryogenic service safety of Fe–Mn–Al–C austenitic lightweight steel welded joints.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Welding Techniques and Residual Stresses · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Excellent combination of strength and ductility in austenitic lightweight steel achieved by warm rolling process10.1016/j.msea.2024.147066 ↗
2. Current state of Fe-Mn-Al-C low density steels10.1016/j.pmatsci.2017.05.002 ↗
3. Research status and development prospect of Fe–Mn–C–Al system low-density steels10.1016/j.jmrt.2023.06.037 ↗
4. Effect of Mo and Cr additions on the microstructure, mechanical properties and pitting corrosion resistance of austenitic Fe-30Mn-10.5Al-1.1C lightweight steels10.1016/j.jallcom.2018.10.253 ↗
5. Effects of local-brittle-zone (LBZ) microstructures on crack initiation and propagation in three Mo-added high-strength low-alloy (HSLA) steels10.1016/j.msea.2019.05.120 ↗
6. Heat affected zone microstructures and their influence on toughness in two microalloyed HSLA steels10.1016/j.actamat.2015.05.055 ↗
7. Cleavage fracture micromechanisms in simulated heat affected zones of S690 high strength steels10.1016/j.msea.2023.144762 ↗
8. Effects of heat input on microstructure and fracture toughness of simulated coarse-grained heat affected zone for HSLA steels10.1016/j.matchar.2019.109818 ↗
9. Design of a low density Fe-Mn-Al-C steel with high strength-high ductility combination involving TRIP effect and dynamic carbon partitioning10.1016/j.msea.2018.11.044 ↗
10. γ decomposition in Fe–Mn–Al–C lightweight steels10.1016/j.jmrt.2020.02.088 ↗
11. Heat treatment and thermal stability of FeMnAlC alloys10.1016/S0924-0136(02)00937-8 ↗
12. Phase transformation and the mechanical characteristics of heat-affected zones in austenitic Fe–Mn–Al–Cr–C lightweight steel during post-weld heat treatment10.1016/j.matchar.2021.111150 ↗
13. Local brittle cracking in the heat-affected zone of lightweight steels10.1016/j.matchemphys.2019.121904 ↗
14. Effect of grain size and segregation on the cryogenic toughness mechanism in heat-affected zone of high manganese steel10.1016/j.matchar.2024.114030 ↗
15. Effect of welding thermal cycle on microstructural characteristics and low-temperature toughness in simulated heat affected zone of high-Mn steel for LNG tanks10.1007/s11665-025-12505-7 ↗
16. Evaluation of cryogenic toughness variation in multi-pass HAZ of high Mn austenitic steel for LNG cryogenic application10.1007/s12540-025-02023-5 ↗
17. The annealing twins of Fe-20Mn-4Al-0.3C austenitic steels during symmetric and asymmetric hot rolling10.3390/met8110882 ↗
18. A scale-up study on chemical segregation and the effects on tensile properties in two medium Mn steel castings10.1007/s11661-021-06533-w ↗
19. Microstructural evolution in AISI 304 stainless steel during directional solidification and subsequent solid-state transformation10.1016/j.msea.2006.08.039 ↗
20. A comparative study of methods for calculating the dislocation density in GaN-on-Si epitaxial wafers10.3390/mi15080954 ↗
21. Lu · 2016 · 525
22. Influence of microalloying on precipitation behavior and notch impact toughness of welded high-strength structural steels, weld
23. Nonlinear impact damage evolution of Charpy type and analysis of its key influencing factors10.1186/s10033-023-00986-3 ↗
24. The size dependence of micro-toughness in ductile fracture10.1016/j.jmps.2008.02.006 ↗
25. The superior low temperature toughness in a low-carbon microalloyed Q500 steel by finish rolling in dual-phase region10.1016/j.jmrt.2025.12.247 ↗
26. Relationship of the microstructure and toughness of the coarse grain heat-affected zone of TiNbV microalloyed steels based on Electron backscatter diffraction analysis10.1007/s11665-021-06140-1 ↗
27. Cleavage cracking resistance of high angle grain boundaries in Fe–3%Si alloy10.1016/S0167-6636(02)00284-3 ↗
28. Grain boundary embrittlement by Mn and eutectoid reaction in binary Fe–12Mn steel10.1016/j.actamat.2013.03.016 ↗
29. The influence of manganese content on the stacking fault and austenite/ε-martensite interfacial energies in Fe–Mn–(Al–Si) steels investigated by experiment and theory10.1016/j.actamat.2014.01.001 ↗
30. Effects of chemical segregation on ductility-anisotropy in high strength Fe-Mn-Al-C lightweight austenitic steels10.1016/j.actamat.2022.118589 ↗
31. Investigation of panel crack formation in steel ingots: part I. Mathematical analysis and mid face panel cracks10.1007/BF02654213 ↗
32. Characterization of heat affected zone liquation cracking in laser additive manufacturing of Inconel 71810.1016/j.matdes.2015.10.155 ↗
33. Investigating crack formation in IN738LC Ni-based superalloy fabricated by laser powder-bed fusion process10.1016/j.jmrt.2024.01.264 ↗
34. Overcoming liquation cracking in AA7075 welds via friction stir processing pre-weld treatment: a microstructural approach10.1007/s11661-024-07485-7 ↗
35. Segregation assisted grain boundary precipitation in a model Al-Zn-Mg-cu alloy10.1016/j.actamat.2018.07.003 ↗
36. Heat-affected zone characteristics with post-weld heat treatments in austenitic Fe–Mn–Al–C lightweight steels10.1007/s12540-021-01133-0 ↗
37. Microstructural influence on mechanical properties of a lightweight ultrahigh strength Fe-18Mn-10Al-0.9C-5Ni (wt%) steel10.3390/met10101305 ↗
38. Influence of grain boundary carbides on mechanical properties of high nitrogen austenitic stainless steel10.1016/j.matdes.2012.01.024 ↗
39. Effect of dislocation structure evolution on low-angle grain boundary formation in 7050 aluminum alloy during aging10.1007/s12613-015-1127-6 ↗
40. Experimental and modelling study of the grain refinement of Fe-30wt%Ni-Nb austenite model alloy subjected to severe plastic deformation process10.1007/s43452-021-00178-7 ↗