Abstract

Abstract A dissimilar metal weld joint (DMWJ) between low alloy steel and casted duplex stainless steel (CDSS) prepared by automatic multi-pass gas tungsten arc welding (GTAW) with 309L and 52M filler metals is studied by optical microscopy, scanning electron microscopy (with electron back scattering diffraction and energy dispersive X-ray spectroscopy systems), scanning probe microscope techniques and micro-hardness testing. Carbon-depleted zones and microstructure transitions are found in the SA508 heat affected zone (HAZ). Type-I and type-II boundaries exist in 52Mb at some places near the SA508-52Mb interface. The ferrite at the unmixed zone and the zone adjacent to the 309L-CF8A interface (within ~300 μm) changes to a lamellar structure with intermixed ferrite and austenite strips during the buttering process. Epitaxial growth and higher residual strain level are found at the 52Mw-52Mb, 52Mw-309L and 309L-CF8A interface areas. The micro-hardness distribution across the dissimilar metal weld joint is related to the complex chemical composition distribution and the microstructure transition, which in turn made it non-uniform and complicated.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Thermal aging effect on Z3CN20.09M cast duplex stainless steel10.1016/j.nucengdes.2009.06.009 ↗
2. Microstructural changes and fracture behavior of CF8M duplex stainless steels after long-term aging10.1016/S0029-5493(97)00126-X ↗
3. Local mechanical properties of a dissimilar metal welded joint in nuclear power systems10.1016/j.msea.2013.01.037 ↗
4. Experimental evaluation of temper aging embrittlement of cast austenitic stainless steel from PWR10.1016/j.engfailanal.2010.09.022 ↗
5. Effect of long-term thermal aging on the mechanical properties of casting duplex stainless steels10.1016/j.msea.2012.04.105 ↗
6. Localized corrosion of thermally aged cast duplex stainless steel for primary coolant pipes of nuclear power plant10.1016/j.proeng.2012.03.015 ↗
7. Effect of sigma phase precipitation on the mechanical and wear properties of Z3CN20.09M cast duplex stainless steel10.1016/j.nucengdes.2013.02.037 ↗
8. Microstructure evolution and impact fracture behaviors of Z3CN20-09M stainless steels after long-term thermal aging10.1016/j.jnucmat.2012.09.004 ↗
9. Microstructural characterization of an SA508–309L/308L–316L domestic dissimilar metal welded safe-end joint10.1016/j.matchar.2014.08.023 ↗
10. Microstructure, local mechanical properties and stress corrosion cracking susceptibility of an SA508-52M-316LN safe-end dissimilar metal weld joint by GTAW10.1016/j.msea.2016.05.101 ↗
11. Local mechanical properties of alloy 82/182 dissimilar weld joint between SA508 Gr.1a and F316 SS at RT and 320 °C10.1016/j.jnucmat.2008.11.019 ↗
12. Microstructure of a safe-end dissimilar metal weld joint (SA508-52-316L) prepared by narrow-gap GTAW10.1016/j.matchar.2016.11.029 ↗
13. Mechanical property variation within Inconel 82/182 dissimilar metal weld between low alloy steel and 316 stainless steel10.1016/j.ijpvp.2007.08.004 ↗
14. Comparative study of microstructure and properties of low-alloy-steel/nickel-based-alloy interfaces in dissimilar metal weld joints prepared by different GTAW methods10.1016/j.matchar.2018.02.044 ↗
15. Stress corrosion cracking of a low alloy steel to stainless steel transition weld in PWR primary waters at 292 °C10.1016/S0010-938X(99)00131-6 ↗
16. Characterization of low alloy ferritic steel–Ni base alloy dissimilar metal weld interface by SPM techniques, SEM/EDS, TEM/EDS and SVET10.1016/j.matchar.2014.12.007 ↗
17. Microstructure and mechanical property of the fusion boundary region in an alloy 182-low alloy steel dissimilar weld joint10.1007/s10853-010-4581-6 ↗
18. Characterization of a Ni-Base NG-DMW weld of modern PWR
19. Fracture mechanical and microstructural characterization of narrow-gap safe-end dissimilar metal weld
20. Kou · 2003
21. Transition metal joints for steam generators—an overview10.1016/0308-0161(94)90061-2 ↗
22. Dissimilar metal welds—transition joints literature review
23. Microstructure and stress corrosion cracking of the fusion boundary region in an alloy 182-A533B low alloy steel dissimilar weld joint10.1016/j.corsci.2010.08.002 ↗
24. Nature and evolution of the fusion boundary in ferritic-austenitic dissimilar weld metals, part 1 - nucleation and growth
25. Correlation of the microstructure and fracture toughness of the heat-affected zones of an SA 508 steel10.1007/s11661-000-0106-2 ↗
26. The mechanism of hydrogen-induced pitting corrosion in duplex stainless steel studied by SKPFM10.1016/j.corsci.2012.04.010 ↗
27. Depletion effects at phase boundaries in 2205 duplex stainless steel characterized with SKPFM and TEM/EDS10.1016/j.corsci.2009.05.012 ↗
28. Characterization of phases in duplex stainless steel by magnetic force microscopy/scanning Kelvin probe force microscopy10.1149/1.2912601 ↗
29. Microstructure characterization of the fusion zone of an alloy 600-82 weld joint10.1016/j.jmst.2015.08.013 ↗
30. Microstructure, residual strain and stress corrosion cracking behavior in 316L heat-affected zone10.1007/s40195-016-0461-7 ↗
31. Effect of dissolved oxygen content on stress corrosion cracking of a cold worked 316L stainless steel in simulated pressurized water reactor primary water environment10.1016/j.jnucmat.2013.11.027 ↗
32. On a more restrictive geometric criterion for “special” CSL grain boundaries10.1016/S1359-6462(98)00077-3 ↗
33. Grain boundary engineering for structure materials of nuclear reactors10.1016/j.jnucmat.2013.03.050 ↗
34. Effects of cold working degrees on grain boundary characters and strain concentration at grain boundaries in alloy 60010.1016/j.corsci.2010.11.022 ↗
35. Microstructure and local properties of a domestic safe-end dissimilar metal weld joint by using hot-wire GTAW