Thermal behavior of AZ31 gradient microstructure after cold severe surface plastic deformation
Source abstract
Abstract
Abstract Surface severe plastic deformation such as severe shot peening has been proposed to manufacture a gradient microstructure with grains smaller than 5 μm near the surface. Subsequent annealing of the heavily cold deformed structure contributes to grain boundary recovery, dislocation rearrangement or annihilation, and consequently ductility enhancement due to the formation of defect-free grains. This structure would be unstable in thermal conditions due to incomplete recrystallization, high density of dislocations, and smaller grain size. In this work, microstructural evolution and thermal stability of a gradient microstructure created via the severe shot peening process in AZ31 is investigated through characterizing the microstructure during isothermal and isochronal heat treatment. In the end, thermal stability of the structure is demonstrated wherein recrystallization started at 150 ∘C from the surface and continued through the thickness until new defect-free grains appeared in all deformed layers. The newly-formed structure stays relatively stable with slow grain growth from temperature 300 ∘C to 450 ∘C that leads to the acceptable value of grain boundary activation energy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Surface Treatment and Residual Stress · Metal and Thin Film Mechanics · Magnesium Alloys: Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Analysis of superplastic deformation of az31 magnesium alloy10.1002/adem.200700155 ↗
2. Effects of nanofeatures induced by severe shot peening (ssp) on mechanical, corrosion and cytocompatibility properties of magnesium alloy az3110.1016/j.actbio.2017.11.032 ↗
3. Microstructure and texture evolution of magnesium alloy after shear assisted processing and extrusion (shapetm)
4. Study of the surface nanocrystallization induced by the esonix ultrasonic impact treatment on the near-surface of 2024-t351 aluminum alloy10.1361/105994906X108693 ↗
5. Research on friction and wear behavior of gradient nano-structured 40cr steel induced by high frequency impacting and rolling10.1016/j.engfailanal.2017.09.012 ↗
6. Microstructures and mechanical properties of pure copper deformed severely by equal-channel angular pressing and high pressure torsion10.1016/j.msea.2007.05.083 ↗
7. Surface severe plastic deformation of aisi 304 via conventional shot peening, severe shot peening and repeening10.1016/j.apsusc.2015.05.093 ↗
8. Effects of the strain rate and temperature on the microstructural evolution of twin-rolled cast wrought az31b alloys sheets10.1007/s11665-013-0598-8 ↗
9. Mechanical properties and deformation mechanism of mg-al-zn alloy with gradient microstructure in grain size and orientation10.1016/j.msea.2017.04.005 ↗
10. Strain hardening and tensile behaviors of gradient structure mg alloys with different orientation relationships10.1016/j.msea.2018.08.053 ↗
11. Fatigue behavior of a low-alloy steel with nanostructured surface obtained by severe shot peening10.1016/j.engfracmech.2011.06.011 ↗
12. Microstructure and thermal stability of nanocrystalline mg-gd-y-zr alloy processed by high pressure torsion10.1016/j.jallcom.2017.05.164 ↗
13. Strengthening and toughening of magnesium alloy by {1 0–1 2} extension twins10.1016/j.scriptamat.2011.09.033 ↗
14. The effect of pre-twinning on the mechanical behavior of free-end torsion for an extruded az31 magnesium alloy10.1016/j.msea.2018.11.051 ↗
15. Surface nanocrystallization by surface mechanical attrition treatment
16. Grain refinement and deformation mechanisms in room temperature severe plastic deformed mg-az3110.3390/met3030283 ↗
17. Thermal stability of nanogradient microstructure produced by surface mechanical rolling treatment in zircaloy-410.1007/s10853-019-04303-z ↗
18. Effect of gradient microstructures on strengthening and toughening of az3110.1016/j.msea.2019.138615 ↗
19. Increased structural stability in twin-roll cast az31 magnesium alloy processed by equal channel angular pressing10.1016/j.matchar.2019.05.006 ↗
20. Microstructure stability of a fine-grained az31 magnesium alloy processed by constrained groove pressing during isothermal annealing
21. Thermal stability and strength of deformation microstructures in pure copper10.1016/j.actamat.2012.04.022 ↗
22. Structural stability of ultra-fine grained magnesium alloys processed by equal channel angular pressing
23. Effects of shot peening parameters on gradient microstructure and mechanical properties of trc az3110.1016/j.matchar.2018.12.001 ↗
24. High tensile ductility in a nanostructured metal10.1038/nature01133 ↗
25. Effect of annealing on microstructure and mechanical properties of zk60 magnesium alloy sheets processed by twin-roll cast and differential speed rolling10.1016/j.matchar.2014.09.014 ↗
26. Annealing of a magnesium alloy az31 after interrupted cold deformation
27. Strength-ductility modulation via surface severe plastic deformation and annealing10.1016/j.msea.2019.06.033 ↗
28. Annealing behavior of a cast mg-gd-y-zr alloy with necklace fine grains developed under hot deformation10.1016/j.msea.2017.02.008 ↗
29. Heterogeneous and architectured materials: a possible strategy for design of structural materials10.1002/adem.200700289 ↗
30. Thermal microstructural stability of az31 magnesium after severe plastic deformation10.1016/j.matchar.2014.12.026 ↗
31. Recrystallization mechanism and activation energies of severely-deformed magnesium during annealing process10.1016/j.mtla.2018.100188 ↗
32. Microstructure stability of ultra-fine grained magnesium alloy az31 processed by extrusion and equal-channel angular pressing (ex–ecap)10.1016/j.matchar.2014.05.013 ↗
33. Mechanical behaviour and texture of annealed az31 mg alloy deformed by ecap10.1179/174328407X161132 ↗
34. Twinning and the ductility of magnesium alloys: part i:“tension” twins10.1016/j.msea.2006.12.037 ↗
35. Humphreys · 2012
36. On the time exponent in isothermal grain growth10.1007/BF03038435 ↗
37. Microstructural stability after severe plastic deformation of az31 magnesium10.1016/j.matchar.2014.12.026 ↗