Carbide formation accompanying internal nitridation of austenitic stainless steel
Source abstract
Abstract
Internal oxidation, carburization, and nitridation are three forms of internal corrosion commonly experienced by high-temperature alloy components in industrial plants. They are characterized by ingress of an oxidizing species (oxygen, carbon or nitrogen) into the sub-surface region of the affected material, often accompanied by formation of precipitate phases. These microstructural changes can have a significant impact on mechanical performance. Management of such threats to equipment integrity therefore requires a comprehensive understanding of microstructural evolution, including rate information. In this work, we use optical, scanning electron, transmission electron, and atomic force microscopy to study precipitate phases and quantify internal corrosion rates in the austenitic stainless steel Alloy 800H subjected to nitriding in a 95% N2 + 5% H2 atmosphere at service-relevant temperatures (800–1000 °C). We identify and characterize carbide and carbonitride precipitates formed alongside the expected nitrides, and use the thermodynamic software Thermo-Calc to show that formation of carbides during nitridation is thermodynamically possible in this alloy. This work ultimately demonstrates that a wide-ranging analytical approach may be crucial to gaining a full picture of the effects of internal corrosion in complex industrial alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · High-Temperature Coating Behaviors · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Oxidation
2. Oxidation of alloys II: Internal oxidation
3. Creep fracture
4. Plastic deformation in crystalline materials
5. Time–temperature–precipitation relations for nitrides and evaluation of internal oxidation theory for nitridation of austenitic stainless steel10.1007/s11661-020-05868-0 ↗
6. Oxidation and nitridation of alloy 800 H at a growing creep crack and for unstressed samples10.1007/BF02665510 ↗
7. Precipitate morphologies and growth kinetics in the internal carburisation and nitridation of Fe–Ni–Cr alloys10.1016/S0010-938X(99)00095-5 ↗
8. Comparison of internal nitridation reactions in ammonia and in nitrogen10.1007/BF01058247 ↗
9. Investigations of nitridation behaviour of high temperature materials10.1002/maco.19970480806 ↗
10. Effect of addition of 4% Al on the high temperature oxidation and nitridation of a 20Cr–25Ni austenitic stainless steel10.1007/s11085-014-9503-6 ↗
11. Nitride-hardening of an austenitic stainless steel containing titanium10.1179/msc.1974.8.1.209 ↗
12. Thermo-Calc and DICTRA, computational tools for materials science10.1016/S0364-5916(02)00037-8 ↗
13. Investigations on the influence of internal nitridation on creep crack growth in alloy 800 H10.1007/BF02665511 ↗
14. Reaction types in the oxidation of alloys
15. 2019
16. 2010
17. Gwyddion: an open-source software for SPM data analysis10.2478/s11534-011-0096-2 ↗
18. Fiji: an open-source platform for biological-image analysis10.1038/nmeth.2019 ↗
19. Precipitation of intragranular M23C6 particles and their effect on the high temperature creep of austenite10.1016/0025-5416(81)90181-6 ↗
20. Microstructural evolution during creep of alloy 800HT in the temperature range 600 °C to 1000 °C10.1007/s11661-008-9751-7 ↗
21. Interstitial nitrides: properties and general characteristics
22. Carbides of group IV: Titanium, zirconium, and hafnium carbides
23. Failures of pigtails: Why they happen and how to avoid them
24. Mechanical and microstructural properties of alloy 80010.1007/BF02652243 ↗
25. Kinetics of the internal nitridation of austenitic Fe-Cr-Ni-Ti alloys10.1007/BF02819257 ↗
26. An experimental and thermodynamic study of the Fe-Cr-C-N system at 1273 K10.1007/BF02646207 ↗
27. Analysis of the solubility of carbides, nitrides, and carbonitrides in steels using methods of computer thermodynamics: III. Solubility of carbides, nitrides, and carbonitrides in the Fe-Ti-C, Fe-Ti-N, and Fe-Ti-C-N systems10.1134/S0031918X09110088 ↗
28. Kinetics, microstructures and mechanism of internal oxidation - its effect and prevention in high temperature alloy oxidation10.5006/0010-9312-21.12.382 ↗
29. A model to predict carburization profiles in high temperature alloys10.1007/BF02655105 ↗
30. Appendix C: Standard gibbs energies of formation and evaporation
31. Influence of the thermal treatment and alloy composition on the internal oxidation of iron alloys10.1002/srin.196003128 ↗
32. The transport of oxygen to the advancing internal oxide front during internal oxidation of nickel-base alloys at high temperature10.1016/0167-2738(84)90166-8 ↗
33. Failure mechanisms of alloy 800H in steam reformer furnace pigtails
34. Metallurgical evaluation of alloy 800HT pigtails
35. Qualification of stationary creep of the carbide precipitating alloy 800H
36. Influence on high temperature mechanical strength by high temperature corrosion
37. Beardsley · 2018