Abstract
Abstract In the current work, the influences of both traverse and rotational speeds of friction stir processing (FSP) on the microstructural evolution, crystallographic texture, and mechanical properties of AZ91 alloy were investigated. The tool traverse and rotational speeds used in the present study were 20, 40, 60 mm/min, and 400, 800, 1200 rpm, respectively. The average grain size significantly decreased from 61.6 μm in the as-cast condition to below 10 μm in the FSP-processed samples owing to the occurrence of dynamic recrystallization (DRX). By increasing the tool traverse speed and decreasing the rotational speed, the grain size reduced. The grain boundaries pinned by fine β-Mg17Al12 particles, retarding the grain growth. The fraction of the β-Mg17Al12 remarkably decreased after the FSP owing to fragmentation and dissolution. The high strain rate of the 800–40 and 1200–40 samples coupled with their higher peak temperatures increased the dissolution of β-Mg17Al12 during FSP. It was found that a texture transition from (10.1) pyramidal to (00.2) basal occurred by decreasing the traverse speed and increasing the rotational speed. The highest microhardness, which was equal to 104.4 HV, belongs to the 800–20 sample due to its very fine grains. When the rotational speed increased from 400 to 1200 rpm, the ultimate tensile strength (UTS) improved from 236.8 to 267.1 MPa, the total elongation (TE) decreased from 7.5% to 6.6%, and the energy absorption (EA) improved from 13.1 to 14.2 J/cm3. These results were due to the higher accumulated strain, the larger solid solution strengthening, the lower aspect ratio of β-Mg17Al12, stronger {0002} texture, and the lower content of β-Mg17Al12 of the 1200–400 sample. The UTS and TE of the 1200–40 sample showed an enhancement of 96.4% in UTS, 26.9% in TE, and 132.8% in EA as compared to the as-cast AZ91. Up to the true strain of 0.05, with increasing the rotational speed, the strain hardening rate increased owing to decreasing the fraction of grain boundaries. After the true strain of 0.05, the strain hardening rate reduced by increasing the rotational speed due to strengthening the {0002} texture. The fractured surface of the 800–20 sample had the largest number and smallest size of dimples as compared to the other FSP-processed samples owing to its lowest grain size. Finally, the strong {0002} basal texture in the 800–40, 1200–40, and 800–20 samples led to tear ridges aligning with the normal direction of fractured surfaces.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Microstructure evolution during high strain rate tensile deformation of a fine-grained AZ91 magnesium alloy10.1016/j.msea.2013.10.029 ↗
2. Effect of β–Mg17Al12 phase on microstructure, texture and mechanical properties of AZ91 alloy processed by asymmetric hot rolling10.1016/j.msea.2018.09.086 ↗
3. Fatigue properties of magnesium alloy AZ91 processed by severe plastic deformation10.1016/j.jmbbm.2014.11.019 ↗
4. Microstructural modification and its effect on strengthening mechanism and yield asymmetry of in-situ TiC-TiB2/AZ91 magnesium matrix composite10.1016/j.msea.2018.03.060 ↗
5. Asymmetric cold rolling: a technique for achieving non-basal textures in AZ91 alloy10.1016/j.matlet.2019.04.087 ↗
6. Thermal stability of bimodal microstructure in magnesium alloy AZ91 processed by ECAP10.1016/j.matchar.2015.07.009 ↗
7. Tensile anisotropy of AZ91 magnesium alloy by equal channel angular processing10.1016/j.jallcom.2014.11.046 ↗
8. Effect of asymmetric cold rolling on the microstructure, texture, and mechanical properties of the AZ91 alloy
9. Developing an industrial-scale ECAP Mg-Al-Zn alloy with multi-heterostructure for synchronously high strength and good ductility10.1016/j.matchar.2020.110341 ↗
10. Achieving single-pass high-reduction rolling and enhanced mechanical properties of AZ91 alloy by RD-ECAP pre-processing10.1016/j.msea.2020.140717 ↗
11. Managing strength and ductility in AZ91 magnesium alloy through ECAP combined with prior and post aging treatment10.1016/j.matchar.2019.04.022 ↗
12. Microstructure evolution of AZ91 alloy processed by a combination method of equal channel angular pressing and rolling10.1016/j.jma.2019.05.012 ↗
13. Superplastic behaviour of AZ91 magnesium alloy processed by high-pressure torsion10.1016/j.msea.2015.04.004 ↗
14. Effect of large thickness-reduction on microstructure evolution and tensile properties of Mg-9Al-1Zn alloy processed by hard-plate rolling10.4028/b-NdD003 ↗
15. Achieving bimodal microstructure and enhanced tensile properties of Mg–9Al–1Zn alloy by tailoring deformation temperature during hard plate rolling10.1016/j.jallcom.2018.04.328 ↗
16. Superplastic tensile behavior of a fine-grained AZ91 magnesium alloy prepared by friction stir processing10.1016/j.msea.2012.06.063 ↗
17. Microstructures and tensile properties of submerged friction stir processed AZ91 magnesium alloy10.1016/j.jma.2015.08.001 ↗
18. Machining characteristics of fine grained AZ91 Mg alloy processed by friction stir processing10.1016/S1003-6326(17)60092-X ↗
19. Strengthening and ductilization mechanisms of friction stir processed cast Mg–Al–Zn alloy10.1016/j.msea.2020.139249 ↗
20. Development of titanium particulate reinforced AZ31 magnesium matrix composites via friction stir processing10.1016/j.jallcom.2019.153071 ↗
21. Formations of AZ91/Al2O3 nano-composite layer by friction stir processing10.1016/j.jma.2016.11.002 ↗
22. The effect of process parameters on microstructural characteristics of AZ91/SiO2 composite fabricated by FSP10.1016/j.msea.2012.08.084 ↗
23. Enhancing corrosion resistance and mechanical properties of AZ31 magnesium alloy by friction stir processing with the same speed ratio10.1016/j.jallcom.2020.154452 ↗
24. Effect of process parameters on microstructure and micro-hardness of AZ91/Al2O3 surface composite produced by FSP10.1007/s11665-010-9812-0 ↗
25. Arbegast · 1988
26. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
27. Friction stir welding of AZ31 magnesium alloy rolled sheets: influence of processing parameters10.1016/j.actamat.2008.09.011 ↗
28. Effect of post-weld heat treatment on mechanical properties of local weld-affected zones in friction stir welded AZ31 plates10.1016/j.msea.2021.140809 ↗
29. Microstructure evolution and mechanical properties of a submerged friction-stir-processed AZ91 magnesium alloy10.1007/s10853-015-8887-2 ↗
30. Achieving ultrafine grain size in mg–Al–Zn alloy by friction stir processing10.1016/j.scriptamat.2007.04.007 ↗
31. Relationship between grain size and Zener-Holloman parameter during friction stir processing in AZ31 mg alloys10.1016/j.scriptamat.2004.05.043 ↗
32. Enhancing mechanical properties of AZ61 magnesium alloy via friction stir processing: effect of processing parameters10.1016/j.msea.2020.139945 ↗
33. Enhanced corrosion resistance of AZ91 magnesium alloy through refinement and homogenization of surface microstructure by friction stir processing10.1016/j.corsci.2018.04.028 ↗
34. Aging behavior of nano SiC particles reinforced AZ91D composite fabricated via friction stir processing10.1016/j.jallcom.2019.04.280 ↗
35. Cullity · 2014
36. Microstructure evolution and mechanical properties of hot deformed Mg9Al1Zn samples containing a friction stir processed zone10.1016/j.jma.2017.11.003 ↗
37. Machining characteristics and corrosion behavior of grain refined AZ91 mg alloy produced by friction stir processing: role of tool pin profile10.1007/s12666-017-1250-3 ↗
38. The significance of texture parameters in phase analysis by X-ray diffraction10.1107/S0021889869006881 ↗
39. Deformation behavior of as-cast and as-extruded Mg97Zn1Y2 alloys during compression, as tracked by in situ neutron diffraction10.1016/j.ijplas.2018.08.001 ↗
40. Effect of gradient microstructure on the mechanical properties of aluminum alloy10.1016/j.matchar.2021.111023 ↗
41. Simultaneous enhancement of strength and ductility in ferrite-martensite steel via increasing the martensite fraction10.1016/j.matchemphys.2020.124204 ↗
42. A new method to produce dual-phase steel10.1016/j.msea.2020.140695 ↗
43. Effect of post-annealing on the microstructure and mechanical properties of nanostructured copper10.1016/j.msea.2020.140666 ↗
44. A new 1.2 GPa-strength plain low carbon steel with high ductility obtained by SRDR of martensite and intercritical annealing10.1016/j.msea.2020.139584 ↗
45. A novel technique to form gradient microstructure in AA5052 alloy10.1016/j.msea.2020.139075 ↗
46. Improving microstructural and tensile properties of AZ31B magnesium alloy joints by stationary shoulder friction stir welding10.1016/j.jmapro.2018.11.014 ↗
47. Enhanced mechanical properties of tungsten inert gas welded AZ31 magnesium alloy joint using two-pass friction stir processing with rapid cooling10.1016/j.msea.2016.01.009 ↗
48. Effects of heat input on tensile properties and fracture behavior of friction stir welded Mg–3Al–1Zn10.1016/j.msea.2009.09.044 ↗
49. Effect of micro-texture on fracture location in friction stir weld of Mg alloy AZ61 during tensile test10.1016/S1359-6462(03)00210-0 ↗