journal article·2021-04

Modifications on solidification thermal parameters, microstructure and hardness induced by Cu additions to a hypereutectic Zn 8Al alloy

Múcio Dantas de Medeiros, Rudimylla Septímio, Cássio Augusto Pinto da Silva, José Eduardo Spinelli, Noé Cheung, Amauri Garcia, Bismarck Luiz Silva

Publisher page

Abstract

Abstract Binary Zn Al alloys are interesting alternatives when tensile strength and hardness performances are required. However, such alloys exhibit limitations on lubrication, ductility at room temperature and mechanical strength at high temperatures. It is known that small alloying additions of Cu to Zn Al alloys can modify the microstructure and properties such as creep and wear resistances, hardness, fluidity, and lubrication. In this sense, this work aims to study the effects of Cu additions on the solidification thermal parameters such as cooling and growth rates (ṪL/VL-liquidus isotherm and ṪE/VE-eutectic front), microstructure (dendritic and eutectic arrangements), and hardness of a hypereutectic Zn-8wt.%Al alloy. Techniques such as X-Ray Diffraction (XRD), X-Ray Fluorescence (XRF), Optical Microscopy (OM) and Scanning Electron Microscopy (SEM) were used to characterize the as cast samples. The results show that the resulting microstructures consist of a eutectic matrix [(Zn) + (Al + Zn)] with lamellar and fibrous morphologies and τ’-Al4Cu3Zn intermetallic particles disseminated within the (Zn) phase; pro-eutectic Al-rich (Al') dendrites containing alternating lamellae of Al and Zn phases, which resulted from the eutectoid transformation [(Al')↔(Al) + (Zn)]. The Cu additions have coarsened the fibrous and lamellar eutectic of the binary Zn-8wt%Al alloy, with exception of the Zn-8 wt% Al-1.3 wt% Cu alloy, which showed a refinement of the fibrous eutectic for VE > 0.30 mm/s. Increase in hardness has been observed for both Cu-modified alloys due to the solid-solution strengthening mechanism and presence of the τ’-Al4Cu3Zn intermetallics. An expressive increase of about 73.4% has been observed due to the addition of 1.3% Cu, which is also related to lower eutectic fibrous spacings.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Magnesium Alloys: Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Barnhurst · 1990
2. Smith · 1993
3. Correlation between unsteady-state solidification thermal parameters and microstructural growth of Zn–8 mass% Al and Zn–8 mass% Al–XBi tribological alloys10.1007/s10973-019-08600-2 ↗
4. Effects of Al addition on the structure and mechanical properties of Zn alloys10.1016/j.jallcom.2016.06.196 ↗
5. Design of mechanical properties of a Zn27Al alloy based on microstructure dendritic array spacing10.1016/j.matdes.2006.09.009 ↗
6. Osório · 2005 · 397 · 179
7. Near-eutectic Zn-Mg alloys: interrelations of solidification thermal parameters, microstructure length scale and tensile/corrosion properties10.1016/j.cap.2019.02.013 ↗
8. Thermal parameters and microstructural development in directionally solidified Zn-rich Zn-Mg alloys10.1007/s11661-016-3494-7 ↗
9. Microstructural development of hypoeutectic Zn-(10-40)wt%Sn solder alloys and impacts of interphase spacing and macrosegregation pattern on hardness10.1016/j.jallcom.2015.05.195 ↗
10. Interconnection of thermal parameters, microstructure, macrosegregation and microhardness of unidirectionally solidified Zn-rich Zn-Ag peritectic alloys10.1016/j.matdes.2014.07.002 ↗
11. Meyers · 2009
12. Comparison of the wear properties of modified ZA-8 alloys and conventional bearing bronze10.1016/j.matdes.2006.04.010 ↗
13. Effect of different Al contents on the microstructure, tensile and wear properties of Zn-based alloy10.1016/j.matlet.2003.10.058 ↗
14. Yılmazer · 2020
15. Study of the influence of copper and magnesium additions on the microstructure formation of Zn-Al hypoeutectic alloys10.1016/j.jallcom.2009.08.125 ↗
16. Microstructure and mechanical properties of Zn-15Al-based ternary and quaternary alloys10.1016/j.msea.2014.02.047 ↗
17. Relationships between cooling rate, copper content and mechanical properties of monotectoid based Zn-Al-Cu alloys10.1016/j.matchar.2003.12.003 ↗
18. Precipitation of metastable ϵ-phase in a hypereutectic zinc-aluminium alloy containing copper10.1016/0956-7151(91)90005-L ↗
19. Review of microstructures and properties of zinc alloys10.3390/met10020253 ↗
20. Image processing with imageJ
21. Directional solidification of aluminium-copper alloys10.1016/S0921-5093(01)01649-5 ↗
22. ASTM · 2016
23. Characterization of the Al-3wt.%Si alloy in unsteady-state horizontal directional solidification10.1590/S1516-14392013005000072 ↗
24. Kurz · 1990
25. Characteristics of Zn-Al-cu alloys for high temperature solder application10.2320/matertrans.MF200809 ↗
26. Hekimoğlu · 2016 · 13
27. Dry sliding friction and wear properties of zinc-based alloys10.1016/S0043-1648(02)00050-9 ↗
28. Effect of phase transformations on hardness in Zn-Al-Cu alloys
29. Experimental study of the Al–Cu–Zn ternary phase diagram10.1007/s10853-020-04686-4 ↗
30. Dendritic solidification microstructure affecting mechanical and corrosion properties of a Zn4Al alloy10.1007/s10853-005-0852-z ↗
31. Plate-like cell growth during directional solidification of a Zn-20wt%Sn high-temperature lead-free solder alloy10.1016/j.mseb.2013.11.016 ↗
32. Effects of cell morphology and macrosegregation of directionally solidified Zn-rich Zn-Cu alloys on the resulting microhardness10.1016/j.matlet.2012.04.095 ↗