High-temperature tensile and creep deformation of cross-weld specimens of weld joint between T92 martensitic and Super304H austenitic steels
Source abstract
Abstract
The high-temperature mechanical behavior of cross-weld specimens prepared from a dissimilar weld joint between T92 martensitic and Super304H austenitic heat-resistant steels incorporating Ni-based weld metal was evaluated at temperatures up to 650 degrees C. For both high temperature tensile and creep tests, failure took place in T92 due to its faster degradation with temperature increase. The heat-affected zone of T92 played a critical role during creep deformation, resulting in type IV failure under the long-term creep condition. For the creep specimens, the location of failure shifted from the base metal region to the fine-grained heat-affected zone as the creep duration time increased from the short-term to the long-term condition. The massive precipitation of Laves phase on the grain boundaries of the fine-grained heat-affected zone during creep deformation was observed and found to be responsible for the accelerated void formation in the area leading to the premature failure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Creep strength of high chromium steels welded parts under multiaxial stress conditions10.1016/j.ijpvp.2010.03.018 ↗
2. Factors affecting type IV creep damage in grade 91 steel welds10.1016/j.msea.2013.04.045 ↗
3. Suppression of type IV fracture and improvement of creep strength of 9Cr steel welded joints by boron addition10.1016/j.ijpvp.2006.09.013 ↗
4. Z-phase formation in welded joints of high chromium ferritic steels after long-term creep10.1016/j.matchar.2007.09.009 ↗
5. Type IV cracking in ferritic power plant steels10.1179/174328406X148778 ↗
6. Creep crack growth behavior in the HAZ of weldments of W containing high Cr steel10.1016/S0308-0161(01)00090-4 ↗
7. Microstructural analysis on creep properties of dissimilar materials joints between T92 martensitic and HR3C austenitic steels10.1016/j.msea.2011.04.057 ↗
8. Creep fracture behavior of dissimilar weld joints between T92 martensitic and HR3C austenitic steels10.1016/j.ijpvp.2011.01.003 ↗
9. Microstructure and creep characteristics of dissimilar T91/TP316H martensitic/austenitic welded joint with Ni-based weld metal10.1016/j.matchar.2012.06.014 ↗
10. Abe · 2008
11. A trigger of type IV damage and a new heat treatment procedure to suppress it. Microstructural investigations of long-term ex-service Cr–Mo steel pipe elbows10.1016/j.ijpvp.2004.09.001 ↗
12. Creep damage and expected creep life for welded 9–11% Cr steels10.1016/j.ijpvp.2006.09.011 ↗
13. Elevated temperature intergranular cracking in heat-resistant steels10.1016/j.msea.2012.09.007 ↗
14. Anomalies in segregation kinetics of solutes under tensile stress in heat resistant steel10.1016/j.msea.2012.07.023 ↗
15. Mechanical and microstructural stability of P92 steel under uniaxial tension at high temperature10.1016/j.msea.2010.03.001 ↗
16. MatNavi, MatNavi, NIMS Materials Database (online).
17. Effect of thermo-mechanical treatment on microstructure and mechanical properties of P92 heat resistant steel10.1016/j.msea.2012.09.040 ↗
18. Effect of fine precipitation and subsequent coarsening of Fe2W Laves phase on the creep deformation behavior of tempered martensitic 9Cr–W steels10.1007/s11661-005-0305-y ↗
19. Strain localization in creep testing of samples with heterogeneous microstructures10.1016/0308-0161(94)00046-8 ↗