Abstract Corrosion of the Fe-25Ni-15Cr under the combined effects of marine atmospheric exposure and the subsequent high-temperature oxidation was investigated in the present work. The results indicated that high-temperature oxidation rate of the superalloy after field exposure was significantly accelerated due to the deposited salts and corrosion products. The oxidation kinetic process of the superalloy was clearly divided into two stages, resulting in changes in morphology, structure and composition of the oxide film. And also, the spontaneous passive state of the superalloy was changed to active dissolution by high–temperature oxidation, indicating a substantial deterioration in corrosion resistance. A degradation model for superalloy under the combined effects of electrochemical corrosion and high temperature oxidation was proposed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Reed · 2008
2. Nickel-based superalloys for advanced turbine engines: chemistry, microstructure and properties10.2514/1.18239 ↗
3. Benefit of the corrosion product film formed on a new weathering steel containing 3% nickel under marine atmosphere in Maldives10.1016/j.corsci.2019.108416 ↗
4. Degradation of austenite stainless steel by atmospheric exposure in tropical marine environment10.1179/1743278212Y.0000000070 ↗
5. Long-term atmospheric corrosion behaviour of aluminium alloys 2024 and 7075 in urban, coastal and industrial environments10.1016/j.corsci.2009.01.016 ↗
6. Corrosion behaviour of Field-Exposed 7A04 aluminum alloy in the Xisha tropical marine atmosphere10.1007/s11665-015-1571-5 ↗
7. Hot corrosion behaviour of super alloys
8. Rust evolution and electrochemical properties of field-exposed carbon steel in a tropical marine environment10.20964/2018.08.02 ↗
9. Atmospheric corrosion of weathering steels. Overview for engineers. Part II: Testing, inspection, maintenance10.1016/j.conbuildmat.2019.06.155 ↗
10. Electrochemical behaviour of 304 stainless steel in marine atmosphere and its simulated solution10.1080/00032719.2012.706847 ↗
11. Atmospheric corrosion of field-exposed AZ31 magnesium in a tropical marine environment10.1016/j.corsci.2013.06.047 ↗
12. Corrosion behaviour of Field-Exposed zinc in a tropical marine atmosphere10.5006/1177 ↗
13. Morphological study of 16-year patinas formed on copper in a wide range of atmospheric exposures10.1016/j.corsci.2007.05.030 ↗
14. Accelerated oxidation rate of chromium induced by sodium chloride10.1007/BF00659274 ↗
15. Electrochemical impedance spectroscopy (EIS) studies of the corrosion of pure Fe and Cr at 600 °C under solid NaCl deposit in water vapor10.1016/j.electacta.2006.01.033 ↗
16. Evidence for the occurrence of electrochemical reactions and their interaction with chemical reactions during the corrosion of pure Fe with solid NaCl deposit in water vapor at 600 °C10.1016/j.elecom.2009.11.021 ↗
17. Influence of Cr content on the corrosion of Fe−Cr alloys: The synergistic effect of NaCl and water vapor10.1023/A:1023083309041 ↗
18. Studies on the corrosion behaviour of Fe–20Cr alloy in NaCl solution spray at 600 °C10.1016/j.corsci.2018.01.033 ↗
19. Corrosion behaviors and protective layer stabilization mechanism of 316 stainless steel in NaCl–KCl–NaF reciprocal salts at high temperatures10.1016/j.corsci.2022.110893 ↗
20. Alkali induced high-temperature corrosion of stainless steel: the influence of NaCl, KCl and CaCl210.1007/s11085-012-9293-7 ↗
21. Hot corrosion behaviour of superalloy IN718 at 550 and 650 °C10.1007/s11665-013-0532-0 ↗
22. Salt induced corrosion behaviour of superalloy IN718
23. Effects of processing on microstructures and properties of FGH4097 superalloy
24. NaCl induced corrosion of Ti-6Al-4V alloy at high temperature10.1016/j.corsci.2016.04.016 ↗
25. Effect of streaming water vapor on the corrosion behaviour of Ti60 alloy under a solid NaCl deposit in water vapor at 600 °C10.1016/j.corsci.2019.108177 ↗
26. Quantitative study of the corrosion evolution and stress corrosion cracking of high strength aluminum alloys in solution and thin electrolyte layer containing Cl−10.1016/j.corsci.2020.109076 ↗
27. Machining performance of high energy die-sinking electrical discharge machining on FE–25NI–15CR10.1080/10426914.2020.1758328 ↗
28. High-temperature fatigue properties of austenitic superalloys 718, A286 and 304L10.1016/j.ijfatigue.2008.01.004 ↗
29. Fatigue strength properties of precipitation strengthening stainless steel A286 focused attention on small fatigue10.1016/j.proeng.2011.04.327 ↗
30. ISO 9223 · 2012 · 2012
31. ASTM G-50 · 2015
32. Corrosion behaviour of Ni–Cr alloys in mixed oxidising gases at 650 °C10.1016/j.corsci.2020.108801 ↗
33. Corrosion behaviour of Ni-Cr alloys in wet CO2 atmosphere at 700 and 800 °C10.1016/j.corsci.2018.10.029 ↗
34. Water vapour effects on corrosion of Ni-Cr alloys in CO2 gas at 650°C10.1016/j.corsci.2018.03.023 ↗
35. Passivity of 316L stainless steel in borate buffer solution studied by Mott-Schottky analysis, atomic absorption spectrometry and X-ray photoelectron spectroscopy10.1016/j.corsci.2010.07.013 ↗
36. Active phase, catalytic activity, and induction period of Fe/zeolite material in nonoxidative aromatization of methane10.1016/j.jcat.2016.01.027 ↗
37. The analysis of electrode impedances complicated by the presence of a constant phase element10.1016/S0022-0728(84)80324-1 ↗
38. A comparative study of primary and secondary passive films formed on AM355 stainless steel in 0.1 M NaOH10.1016/j.apsusc.2017.08.151 ↗
39. Capacitance dispersion in electrochemical impedance spectroscopy measurements of iodide adsorption on Au (111)10.1016/j.apsusc.2006.02.010 ↗
40. In situ study of dew point corrosion by electrochemical measurement10.1016/j.corsci.2013.03.001 ↗
41. Comparison of the corrosion behavior of pure titanium and its alloys in fluoride-containing sulfuric acid10.1016/j.corsci.2015.11.003 ↗
42. Chloridation and oxidation of iron, chromium, nickel and their alloys in chloridizing and oxidizing atmospheres at 400–700 °C10.1016/S0010-938X(99)00142-0 ↗
43. Synergistic effect of NaCl and water vapor on the corrosion of 1Cr–11Ni–2W–2Mo–V steel at 500–700 °C10.1023/A:1018854202982 ↗
44. The hot corrosion of 310 stainless steel with pre-coated NaCl/Na2SO4 mixtures at 750 °C10.1016/j.matchemphys.2004.10.002 ↗
45. Mechanisms of Na2SO4-induced accelerated oxidation10.1016/0010-938X(75)90036-0 ↗
46. Hot corrosion behavior of friction welded AISI 4140 and AISI 304 in K2SO–60% NaCl mixture10.1016/S1005-0302(12)60148-0 ↗
47. The oxidation behavior of the new nickel-based superalloy Inconel 740 with and without Na2SO4 deposit10.1016/j.surfcoat.2003.12.003 ↗
48. An investigation of oxidation/hot corrosion-creep interaction at 800 °C in a Ni-base superalloy coated with salt mixture deposits of Na2SO4-NaCl-NaVO310.1016/j.corsci.2018.11.029 ↗
49. Metal dusting of Fe−Cr and Fe−Ni−Cr alloys under cyclic conditions10.1023/A:1016032722703 ↗