journal article·2024-01

Co-construction of microstructure evolution and wear resistance of in-situ TiBw/TA15 composites with network structure

Yunbin Lu, Yangju Feng, Wei Wang, Wenke Wang, Jianlei Yang, Wenzhen Chen, Guorong Cui, Dongdong Zhuang, Hongyang Cao

Publisher page

Abstract

To further improve the wear resistance of titanium alloy, titanium matrix composites with network distributed TiBw were fabricated. Microstructure evolution and wear mechanism of TA15 alloy and 5 vol% TiBw/TA15 composites were investigated at the temperature of 25 °C and 600 °C. The wear rate of TiBw/TA15 composites at 600 °C was only 7.2 × 10 −5 mm 3 /(N·m). Compared to TA15 alloy, the wear rate of composites decreased by 17.2% at room temperature and 38.4% at high temperature. A novel approach was used to investigate the enhancement role of reinforcement on wear resistance of composites: co-construction of subsurface microstructure evolution and wear resistance through multi-angle observation. The results showed that the improvement of the wear resistance at room temperature was attributed to the TiBw, which enhanced work hardening and improved thermal conductivity. During high- temperature wear process, the TiBw effectively hindered dislocation movement and promoted the DRX, which decreased the stress concentration caused by severe plastic deformation.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Synergistically enhanced strength and ductility of TiB/(TA15-Si) composites: a two-step HIP strategy10.1016/j.compositesb.2023.110583 ↗
2. Improved tribocorrosion behavior on bio-functionalized β-type titanium alloy by the pillar effect given by TiN reinforcements10.1016/j.surfcoat.2021.127122 ↗
3. Effects of Y2O3 addition on the microstructure and wear-resistant performance of TiN/TiB-reinforced Ti-based laser-clad coatings on Ti-6Al-4V alloys
4. Fabrication of GO/RGO/TiC/TiB2 nanocomposite coating on Ti–6Al–4V alloy using electrical discharge coating and exploring its tribological properties10.1016/j.triboint.2021.106860 ↗
5. Microstructural characteristics and tribological behavior of an additively manufactured Ti-6Al-4V alloy under direct aging and solution-aging treatments10.1016/j.triboint.2022.107763 ↗
6. Reaction mechanism and friction behavior of an in-situ Ti/B4C composite synthesized by spark plasma sintering10.1016/j.ceramint.2022.07.358 ↗
7. Effect of Ti5Si3 on the wear properties of Ti–3Si-1.5 Fe–1Mo titanium alloy with ultrahigh hardness10.1016/j.jmrt.2022.07.042 ↗
8. Effect of microwave sintering on the microstructure and tribological behavior of Ti-3Al-2.5 V-xWC composite10.1016/j.triboint.2022.107714 ↗
9. Research on the inhomogeneity and joint interface of in situ oriented TiBw/TA15 composites fabricated by vacuum hot-pressing sintering and canned extrusion10.1016/j.jmapro.2020.09.047 ↗
10. Microstructure and tribological properties of microwave-sintered Ti0. 8Ni–0.3 Mo/TiB composites10.1016/j.ceramint.2022.11.085 ↗
11. In situ preparation of Ti/CaB6 composites via powder metallurgy: microstructure, mechanical and tribological properties improvement10.1007/s10853-022-08124-5 ↗
12. Room and high temperature dry sliding wear behavior of boron modified as-cast Ti-6Al-4V alloys against hardened steel10.1016/j.wear.2018.10.021 ↗
13. Fabrication and mechanical properties of network structured titanium alloy matrix composites reinforced with Ti2AlC particulates10.1016/j.msea.2020.139065 ↗
14. Microstructure characteristics and enhanced properties of network-structured TiB/(TA15-Si) composites via rolling deformation at different temperatures10.1016/j.msea.2021.142176 ↗
15. Grain refinement of cast titanium alloys via trace boron addition10.1016/j.scriptamat.2005.08.020 ↗
16. Research on the inhomogeneity and joint interface of in situ oriented TiBw/TA15 composites fabricated by vacuum hot-pressing sintering and canned extrusion10.1016/j.jmapro.2020.09.047 ↗
17. Effect of high pressure torsion process on the microhardness, microstructure and tribological property of Ti6Al4V alloy10.1016/j.jmst.2021.03.044 ↗
18. Microstructure and wear resistance behavior of Ti–C–B4C-reinforced composite coating10.1016/j.ceramint.2020.06.300 ↗
19. Sliding wear of MAX phase composites Ti3SiC2–TiC and Ti3AlC2–Ti2AlC at 400° C and the influence of counterface material (steel, Al2O3, and Si3N4) on wear behaviour
20. Influence of areal surface parameters on the tribological behavior of Ti6Al4V under lubricated condition
21. Evaluation of wear mechanism between TC4 titanium alloys and self-lubricating fabrics
22. Microstructure evolution and elevated temperature wear performance of in-situ laser-synthesized Ti-25Al-17Nb coating on Ti-6Al-4V10.1016/j.triboint.2022.107807 ↗
23. Nanoindentation study of mechanical and wear properties of spark plasma sintered Ti-6Ni-xTiCN composites10.1016/j.ceramint.2022.09.186 ↗
24. Structural evolution of contact parts of the friction stir processing heat-resistant nickel alloy tool used for multi-pass processing of Ti6Al4V/(Cu+ Al) system
25. Sliding wear performance of in-situ spark plasma sintered Ti-TiBw composite at temperatures up to 900 C10.1016/j.wear.2021.203663 ↗
26. Electrochemical depositing rGO-Ti-rGO heterogeneous substrates with higher thermal conductivity and heat transfer performance compared to pure Ti10.1088/1361-6528/aa538b ↗
27. Tribological properties and wear mechanisms of TixVNbTaWy RHEAs sliding against Si3N4 ceramic balls: the effects of Ti and W contents10.1016/j.triboint.2022.107801 ↗
28. Effect of temperature and sliding velocity on the dry sliding wear mechanisms of boron modified Ti-6Al-4V alloys10.3390/lubricants10110296 ↗
29. Thermal characterization of titanium–titanium boride composites10.1007/s10973-019-08014-0 ↗
30. Deformation behavior and microstructure evolution mechanism of 5 vol.% (TiBw + TiCp)/Ti composites during isothermal compression10.1016/j.matchar.2019.06.002 ↗
31. Influence of deformation parameters and network structure to the microstructure evolution and flow stress of TiBw/Ti64 composite10.1016/j.msea.2021.140997 ↗
32. Aligned TiB whiskers in TiB/Ti6Al4V composites manipulated by spark plasma sintering and hot extrusion: in-situ rotation and strengthening mechanism10.1016/j.msea.2022.144264 ↗
33. Microstructure evolution of TiBw/Ti composites during severe plastic deformation: spheroidization behavior10.1016/j.matchar.2020.110725 ↗
34. Isothermal deformation and spheroidization mechanism of (TiB+ La2O3)/Ti composites with different initial structures10.1016/j.matchar.2018.09.040 ↗
35. Room-temperature and high-temperature tensile mechanical properties of TA15 titanium alloy and TiB whisker-reinforced TA15 matrix composites fabricated by vacuum hot-pressing sintering10.3390/ma10040424 ↗
36. Mesoscale deformation mechanisms in relation with slip and grain boundary sliding in TA15 titanium alloy during tensile deformation10.1016/j.jmst.2021.05.008 ↗
37. Dynamic recrystallization and texture evolution of Ti-22Al-25Nb alloy during plane-strain compression10.1016/j.jallcom.2018.03.372 ↗
38. The effect of deformation parameters on the dynamic recrystallization and microstructure evolution of the quasi-continuous network reinforced TiAl/B4C composites10.1007/s10853-022-07396-1 ↗
39. Microstructure evolution and deformation mechanisms of β phase in TiBw/Ti60 composites studied by reconstructing grain during the hot deformation10.1016/j.jallcom.2020.153872 ↗