journal article·2014-12

High-temperature low cycle fatigue behavior of a gray cast iron

K.L. Fan, G.Q. He, M. She, X.S. Liu, Q. Lu, Y. Yang, D.D. Tian, Y. Shen

Publisher page

Abstract

Abstract The strain controlled low cycle fatigue properties of the studied gray cast iron for engine cylinder blocks were investigated. At the same total strain amplitude, the low cycle fatigue life of the studied material at 523 K was higher than that at 423 K. The fatigue behavior of the studied material was characterized as cyclic softening at any given total strain amplitude (0.12%–0.24%), which was attributed to fatigue crack initiation and propagation. Moreover, this material exhibited asymmetric hysteresis loops due to the presence of the graphite lamellas. Transmission electron microscopy analysis suggested that cyclic softening was also caused by the interactions of dislocations at 423 K, such as cell structure in ferrite, whereas cyclic softening was related to subgrain boundaries and dislocation climbing at 523 K. Micro-analysis of specimen fracture appearance was conducted in order to obtain the fracture characteristics and crack paths for different strain amplitudes. It showed that the higher the temperature, the rougher the crack face of the examined gray cast iron at the same total strain amplitude. Additionally, the microcracks were readily blunted during growth inside the pearlite matrix at 423 K, whereas the microcracks could easily pass through pearlite matrix along with deflection at 523 K. The results of fatigue experiments consistently showed that fatigue damage for the studied material at 423 K was lower than that at 523 K under any given total strain amplitude.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fatigue and fracture mechanics · High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Microstructure and mechanical properties of pearlitic gray cast iron10.1016/j.msea.2007.11.070 ↗
2. Fatigue crack growth in austempered ductile and grey cast irons—stress ratio effects in air and mine water10.1016/S0921-5093(98)01140-X ↗
3. Thermal conductivity–structure relationships in grey cast iron10.1179/136404605225023162 ↗
4. Surface hardening of a gray cast iron used for a diesel engine cylinder block using high-energy electron beam irradiation10.1007/s11661-999-0271-x ↗
5. Short fatigue crack growth in cast iron described using P-a curves10.1016/0142-1123(95)98940-5 ↗
6. Notch fatigue behaviour in cast irons explained using a fracture mechanics approach10.1016/0142-1123(96)00018-7 ↗
7. Prediction of fatigue life using modal analysis for grey and ductile cast iron10.1016/j.ijfatigue.2006.05.004 ↗
8. A methodology for the fatigue design of notched castings in gray cast iron10.1016/j.engfracmech.2006.04.018 ↗
9. Modeling microstructure development in gray cast irons10.1007/BF02652281 ↗
10. Fracture toughness and fatigue crack growth of grey cast irons10.1007/BF00552378 ↗
11. Near-threshold fatigue behavior of flake graphite cast irons microstructers10.1016/0167-8442(95)00032-A ↗
12. Fatigue damage accumulation in grey cast iron10.1016/0142-1123(87)90048-X ↗
13. Thermal fatigue characteristics of gray cast iron with non-smooth surface treated by laser alloying of Cr powder10.1016/j.surfcoat.2007.09.014 ↗
14. ASTM E 606–04 · 2012 · 636
15. The fracture and fatigue properties of cast irons used for trunk mains in the water industry10.1016/j.msea.2010.05.071 ↗
16. The effect of mean stress on the fatigue strength of gray cast iron was examined and its mechanism was investigated
17. Effects of surface shape on thermal fatigue resistance of biomimetic non-smooth cast iron10.1016/j.msea.2007.02.124 ↗
18. Effects of holding time on thermomechanical fatigue properties of compacted graphite iron through tests with notched specimens
19. Fatigue behaviour and mean effects in grey cast iron10.1016/0142-1123(82)90040-8 ↗
20. Definition of damage parameter in low-cycle fatigue of gray cast iron10.4028/www.scientific.net/KEM.345-346.367 ↗
21. 1990
22. Microstructural study of the parameters governing coarsening and cyclic softening in fatigued ultrafine-grained copper10.1080/01418610208235689 ↗
23. Influence of porosity on the fatigue limit of die cast magnesium and aluminium alloys10.1016/S0142-1123(02)00054-3 ↗
24. Low cycle fatigue behavior of Inconel 718 at 298K and 823K10.1007/BF02667395 ↗
25. Low cycle fatigue and cyclic softening behaviour of martensitic cast steel10.1016/j.engfailanal.2013.06.019 ↗
26. Low-cycle fatigue behaviors of an As-extruded Mg–12%Gd–3%Y–0.5%Zr alloy10.1016/j.jmst.2013.04.011 ↗
27. Developing dislocation subgrain structures and cyclic softening during high-temperature creep–fatigue of a nickel alloy10.1007/s11661-013-1737-4 ↗
28. Dependence of dynamic strain ageing on strain amplitudes during the low-cycle fatigue of TP347H austenitic stainless steel at 550°C10.1016/j.ijfatigue.2013.07.010 ↗
29. Development of high strength ductile hypereutectoid steel by cyclic heat treatment process10.1016/j.msea.2012.02.026 ↗
30. ASM International Handbook Committee · 1987 · vol. 12
31. Suresh · 1998
32. Fatigue crack propagation in dual phase steels: effects of ferrite–martensite microstructures on crack path morphology10.1007/BF02644714 ↗
33. Fatigue crack growth characteristics of a new Ni–Co-base superalloy TMW-4M3: effects of temperature and load ratio10.1007/s10853-011-5732-0 ↗
34. Dieter · 1986
35. The brittle fracture of gray cast iron