Microstructure formation in partially melted zone during gas tungsten arc welding of AZ91 Mg cast alloy
Source abstract
Abstract
During gas tungsten arc (GTA) welding of AZ91 Mg cast alloy, constitutional liquid forms locally in the original interdendritic regions in the partially melted zone (PMZ). The PMZ re-solidification behaviour has not been well understood. In this study, the gradual change of the re-solidification microstructure within PMZ from base metal side to weld metal side was characterised. High cooling rate experiments using Gleeble thermal simulator were also conducted to understand the morphological change of the α-Mg/β-Mg17Al12 phase interface formed during re-solidification after partial melting. It was found that the original partially divorced eutectic structure has become a more regular eutectic phase in most of the PMZ, although close to the fusion boundary the re-solidified eutectic is again a divorced one. Proceeding the eutectic re-solidification, if the degree of partial melting is sufficiently high, α-Mg re-solidified with a cellular growth, resulting in a serrated interface between α-Mg and α-Mg/β-Mg17Al12 in the weld sample and between α-Mg and β-Mg17Al12 (fully divorced eutectic) in Gleeble samples. The morphological changes affected by the peak temperature and cooling rate are also explained.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Advanced Welding Techniques Analysis · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Magnesium: commodity or exotic?10.1179/174328407X154374 ↗
2. Mechanical properties and microstructures of a magnesium alloy gas tungsten arc welded with a cadmium chloride flux10.1016/j.matchar.2006.10.012 ↗
3. Chloride contributions in flux-assisted GTA welding of magnesium alloys
4. Magnesium–lithium alloy weldability: a microstructural characterization
5. Influence of laser beam variables on AZ91D weld fusion zone microstructure10.1080/174329313X13789830157627 ↗
6. Factors controlling the magnesium weld morphology in deep penetration welding by a CO2 laser10.1361/105994901770344854 ↗
7. Fundamentals in the fusion welding of magnesium and its alloys
8. Fundamental aspects in the joining of magnesium alloys by the GTAW [TIG welding] and LBW [laser beam welding] processes
9. Electron beam welding of magnesium AZ91D plates
10. An investigation on the effects of gases in GTA welding of a wrought AZ80 magnesium alloy
11. Laser-weld heat-affected zone liquation and cracking in a high-strength Mg-based alloy10.1007/BF01729281 ↗
12. Continuous wave nd:yag laser welding of sand-cast ze41a-t5 magnesium alloys10.1081/AMP-200060436 ↗
13. Electron-beam welding behavior in Mg–Al-based alloys10.1007/s11661-002-0069-6 ↗
14. CO2 laser beam welding of magnesium-based alloys
15. Partially melted zone microstructural characterization from gas tungsten-arc bead on plate welds of magnesium AZ91 alloy10.1023/A:1006640008914 ↗
16. Effects of constitutional liquation in 18-Ni maraging steel weldments
17. Kou · 2002
18. Mechanical properties and microstructure of gas tungsten arc welded magnesium AZ91D plates10.1016/S0921-5093(00)01356-3 ↗
19. A review of laser welding techniques for magnesium alloys10.1016/j.jmatprotec.2005.06.068 ↗
20. Incipient melting in partially melted zone during arc welding of AZ91D magnesium alloy10.1016/j.msea.2005.10.032 ↗
21. Thermal analytical investigations of the magnesium alloys AM 60 and AZ 91 including the melting range10.1016/S0040-6031(01)00752-3 ↗
22. Development of the as-cast microstructure in magnesium–aluminium alloys10.1016/S1471-5317(00)00007-9 ↗
23. Divorced eutectic in a HPDC magnesium–aluminum alloy10.1016/j.jallcom.2003.11.174 ↗
24. Eutectic growth morphologies in magnesium–aluminium alloys
25. The effect of solidification rate on the structure of magnesium–aluminium eutectic grains10.1080/13640461.2000.11819383 ↗