journal article·2010-11

Effect of solidification parameters on the microstructure of Sn-3.7Ag-0.9Zn solder

U. Böyük, S. Engin, H. Kaya, N. Maraşlı

Materials Characterization· Volume 61· Issue 11
Publisher page

Abstract

Abstract In this work, Sn–Ag–Zn alloy of eutectic composition (Sn-3.7wt.%Ag-0.9wt.%Zn) was directionally solidified upward at a constant temperature gradient ( G = 4.33 K/mm) in a wide range of growth rates ( V = 3.38–220.12 μm/s) and a constant growth rate ( V = 11.52 μm/s) with different temperature gradients ( G = 4.33–12.41 K/mm) using a Bridgman type directional solidification furnace. The microstructure was observed to be a rod Ag 3 Sn structure in the matrix of β–Sn from the directionally solidified Sn-3.7wt.%Ag-0.9wt.%Zn samples. The values of eutectic spacing ( λ ) were measured from transverse section of samples. The dependency of eutectic spacing on the growth rate ( V ) and temperature gradient ( G ) were determined with linear regression analysis. The dependency of λ on the values of V and G were found to be λ = 10.42 V − 0.53 and λ = 0.27 G − 0.48 , respectively. The values of bulk growth were also determined to be λ 2 V = 86.39 μm 3 /s by using the measured values of λ and V . The results obtained in present work were compared with the previous similar experimental results obtained for binary and ternary alloys.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloy Microstructure Properties · Solidification and crystal growth phenomena

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Tin increases its cost-effectiveness
2. A viable tin–lead solder substitute – Sn–Ag–Cu10.1007/BF02653344 ↗
3. Research update: lead-free solder alternatives
4. The current status of lead-free solder alloys10.1109/6104.980031 ↗
5. Microstructural modifications and properties of Sn–Ag–Cu solder joints induced by alloying10.1007/s11664-002-0006-x ↗
6. Alloying effects in near-eutectic Sn–Ag–Cu solder alloys for improved microstructural stability10.1007/s11664-001-0129-5 ↗
7. Lead (Pb)-free solders for electronic packaging10.1007/BF02651362 ↗
8. Effect of cooling rate on growth of the intermetallic compound and fracture mode of near-eutectic Sn–Ag–Cu/Cu pad: Before and after aging10.1007/s11664-004-0095-9 ↗
9. Demonstration and characterization of Sn-3.0Ag-0.5Cu/Sn-57Bi-1Ag combination solder for 3-D multistack packaging10.1007/s11664-007-0296-0 ↗
10. Ag3Sn plate formation in the solidification of near-ternary eutectic Sn–Ag–Cu10.1007/s11837-003-0143-6 ↗
11. Choi · Mater Trans · 2001 · 42 · 78310.2320/matertrans.42.783 ↗
12. Comparison of Sn2.8Ag20In and Sn10Bi10In solders for intermediate-step soldering10.1007/s11664-006-0302-y ↗
13. Effects of Co Addition on Bulk Properties of Sn-3.5Ag Solder and Interfacial Reactions with Ni-P UBM10.1007/s11664-008-0529-x ↗
14. Effects of minor additions of Zn on interfacial reactions of Sn–Ag–Cu and Sn–Cu solders with various Cu substrates during thermal aging10.1007/s11664-007-0254-x ↗
15. Kang · 2008 · 478
16. Thermodynamic assessment of the Ni–Bi binary system and phase equilibria of the Sn–Bi–Ni ternary system10.1007/s11664-007-0256-8 ↗
17. Lead-free solders in microelectronics10.1016/S0927-796X(00)00010-3 ↗
18. Properties of lead-free solder alloys with rare earth element additions10.1016/j.mser.2004.01.001 ↗
19. Six cases of reliability study of Pb-free solder joints in electronic packaging technology10.1016/S0927-796X(02)00007-4 ↗
20. Calorimetric investigations of the two ternary systems Al–Sn–Zn and Ag–Sn–Zn10.3139/146.018073 ↗
21. The dependence of lamellar spacing on growth rate and temperature gradient in the lead-tin eutectic alloy10.1016/S0924-0136(99)00344-1 ↗
22. The effect of growth rate on microstructure and microindentation hardness in the In–Bi–Sn ternary alloy at low melting point10.1016/j.jallcom.2008.02.056 ↗
23. Directional solidification of Al–Cu–Ag alloy10.1007/s00339-009-5130-5 ↗
24. Hansen · 1958 · 52
25. Microstructures of eutectic Sn–Ag–Zn solder solidified with different cooling rates10.1016/j.jallcom.2007.09.103 ↗
26. Thermodynamic study of phase equilibria in the Sn–Ag–Zn system10.2320/jinstmet1952.63.6_685 ↗
27. Phase equilibria and thermodynamic properties of Sn–Ag based Pb-free solder alloys10.1109/TEPM.2003.813003 ↗
28. Formation of bulk Ag3Sn intermetallic compounds in Sn–Ag lead-free solders in solidification10.1007/s11664-005-0170-x ↗
29. The microstructure parameters and microhardness of directionally solidified Sn–Ag–Cu eutectic alloy10.1016/j.jallcom.2009.06.067 ↗
30. Eutectic Spacing selection in Al–Cu system10.1179/mst.1994.10.4.312 ↗
31. Permeability for flow parallel to primary dendrite arms10.1016/0921-5093(92)90186-5 ↗
32. Permeability for cross-flow through columnar-dendritic alloys10.1007/BF02654107 ↗
33. Lamellar and rod eutectic growth
34. Coupled two-phase [alpha(Al)+theta(Al2Cu)] planar growth and destabilisation along the univariant eutectic reaction in Al–Cu–Ag alloys10.1016/j.scriptamat.2004.05.040 ↗
35. In situ observation of microstructure evolution in low-melting Bi–In–Sn alloys by light microscopy10.1016/j.actamat.2005.04.015 ↗
36. Evaluation of the rodlike Cu6Sn5 phase in directionally solidified tin – 0.9wt.% copper eutectic alloys10.1016/S1044-5803(97)00036-3 ↗
37. Two-phase planar and regular lamellar coupled growth along the univariant eutectic reaction in ternary alloys: an analytical approach and application to the Al–Cu–Ag system10.1063/1.1906286 ↗
38. El Mahallawy · 1979
39. Moore · 1968
40. Growth and characterization of Al2O3/Y3Al5O12/ZrO2 ternary eutectic fibers10.1016/S0022-0248(01)01375-6 ↗
41. Experimental investigation of the effect of solidification processing parameters on rod spacings in the Sn-1.2 wt. Cu alloy10.1016/j.jallcom.2009.07.027 ↗
42. Dependency of microstructural parameters and microindentation hardness on the temperature gradient in the In–Bi–Sn ternary alloy with a low melting point10.3365/met.mat.2008.10.575 ↗
43. Dependency of eutectic spacings and microhardness on the temperature gradient for directionally solidified Sn–Ag–Cu lead free solder10.1016/j.matchemphys.2009.09.022 ↗
44. Phase separation and undercooling in Al-Si eutectic alloy–the influence of freezing rate and temperature gradient10.1016/0001-6160(76)90102-4 ↗
45. Directional solidification of the aluminium-copper eutectic alloy10.2320/matertrans1989.40.989 ↗
46. Effect of growth rates and temperature gradients on the spacing and undercooling in the broken-lamellar eutectic growth (Sn–Zn eutectic system)10.1361/105994903770343024 ↗