Effect of 4wt.% Cr on microstructure, corrosion resistance and tribological properties of Fe3Al–20wt.%Al2O3 composites
Source abstract
Abstract
Abstract Fe 3 Al–20 wt.%Al 2 O 3 ultrafine grained composites with 4 wt.% Cr were prepared by mechanical alloying inducing self propagating high temperature synthesis with subsequent plasma activated sintering. Microstructures of the composites were studied by X-ray diffraction, scanning electron microscopy, energy dispersive spectrum and transmission electron microscope. Then the relative density, room temperature hardness, static corrosion resistance and dry sliding wear behavior at a temperature range of 25 °C–800 °C of the sintered samples were tested and analyzed. The results showed that the composites had high hardness and a good microstructure with fine grain size, high relative density. The composites with 4 wt.% Cr amount also exhibited excellent comprehensive tribological properties at medium–high temperatures especially at a temperature above 500 °C, although the wear resistance did not be improved at 25 °C–500 °C. 4 wt.% Cr element addition improved the corrosion resistance of the composites significantly with the corrosion loss decreasing by 19.48%.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced materials and composites · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Processing, properties, and applications of nickel and iron aluminides10.1016/S0079-6425(97)00014-5 ↗
2. The high-temperature corrosion of Fe–28Al and Fe–18Al–10Nb in a H2/H2S/H2O gas mixture10.1016/S0921-5093(98)00927-7 ↗
3. Mechanical properties of Fe–Al–M–C (MZTi, V, Nb, Ta) alloys with strengthening carbides and Laves phase10.1016/j.intermet.2004.05.010 ↗
4. Tribological properties of a Fe3Al material in sulfuric acid corrosive environment10.1016/j.wear.2009.07.018 ↗
5. Wear resistance of Fe–28Al–3Cr intermetallic alloy under wet conditions10.1016/j.matlet.2006.11.069 ↗
6. Wear deformation of ordered Fe–Al intermetallic alloys10.1016/0043-1648(93)90527-S ↗
7. Dry sliding wear behavior of Fe–28Al and Fe–28Al–10Ti alloys10.1016/j.msea.2003.09.049 ↗
8. Preparation and properties of Fe3Al-based friction materials10.1016/j.triboint.2004.07.024 ↗
9. Characterization of Fe3Al-based intermetallic alloys fabricated by mechanical alloying and HIP consolidation10.1016/S0921-5093(00)01025-X ↗
10. Tribological properties of Fe3Al–Fe3AlC0.5 composites under dry sliding10.1016/j.intermet.2005.03.005 ↗
11. The FeAl–30% TiC nanocomposite produced by mechanical alloying and hot-pressing consolidation10.1016/S0966-9795(02)00009-2 ↗
12. High strength TiC matrix Fe28Al toughened composites prepared by spontaneous melt infiltration10.1016/j.jeurceramsoc.2006.01.005 ↗
13. Sintering technology research of Fe3Al/Al2O3 ceramic composites10.1016/S0924-0136(01)00608-2 ↗
14. Microstructure and mechanical properties of Fe3Al-based alloys with strengthening boride precipitates10.1016/j.intermet.2007.02.005 ↗
15. Wear resistance of aluminium alloy and its composites reinforced by Al2O3 particles10.1016/j.jmatprotec.2006.10.021 ↗
16. Sliding wear behavior of plasma sprayed Fe3Al–Al2O3 graded coatings10.1016/j.tsf.2007.07.126 ↗
17. The influence of interfacial characteristics between SiCp and Mg/Al metal matrix on wear, coefficient of friction and microhardness10.1016/S0043-1648(00)00536-6 ↗
18. Long range order and vacancy properties in Al-rich Fe3Al and Fe3Al(Cr) alloys10.1016/S1359-6454(97)00464-3 ↗
19. Effect of chromium on properties of Fe3Al10.1557/JMR.1989.1156 ↗
20. Environmental effects on room-temperature ductility and fracture in Fe sub(3)Al10.1016/0956-716X(90)90496-4 ↗
21. On the role of chromium in minimizing room temperature hydrogen embrittlement in iron aluminides10.1016/1359-6462(95)00495-5 ↗
22. Sliding wear resistance of iron aluminides10.1007/BF02707452 ↗
23. Microstructures and mechanical properties of Fe–28Al–5Cr/TiC composites produced by hot-pressing sintering10.1016/j.msea.2011.05.063 ↗
24. Progresses in studies on Fe–Al intermetallic matrix composites
25. Mechanochemical behavior of Fe2O3–Al–Fe powder mixtures to produce Fe3Al–Al2O3 nanocomposite powder10.1007/s10853-007-2123-7 ↗
26. Mechanochemically synthesized Fe3Al–Al2O3 nanocomposite10.1016/j.jallcom.2007.11.123 ↗
27. Effect of fabrication methods on microstructure and mechanical properties of Fe3Al-based alloys10.1016/j.jallcom.2009.08.138 ↗
28. Study on preparation and mechanical properties of Fe3Al–20 wt.%Al2O3 composites10.1016/j.matdes.2012.02.044 ↗
29. Combustion synthesis of titanium carbide: theory and experiment10.1007/BF01144729 ↗
30. Synthesis of high temperature materials by self-propagating combustion methods
31. Experimental determination of phase equilibria in the Fe–Al–C system10.1016/0966-9795(95)00003-H ↗
32. Microstructure and properties of Fe3Al–Fe3AlC0.5 composites prepared by self-propagating high temperature synthesis casting10.1016/j.msea.2004.03.095 ↗
33. Reaction zone microstructure in a Ti3Al+Nb/SiC composite10.1007/BF02672571 ↗
34. Standard practice for the preparation of substitute ocean water
35. Hot hardness and creep of Fe3Al-based alloys10.1016/S0966-9795(99)00118-1 ↗
36. Vacancy formation and effects in FeAl10.1016/S0966-9795(03)00027-X ↗
37. Vacancies, vacancy aggregates and hardening in FeAl10.1016/S0921-5093(98)00922-8 ↗
38. The stress anomaly in FeAl–Fe3Al alloys10.1016/j.intermet.2004.08.012 ↗