Ti particle-reinforced surface layers in Al: Effect of particle size on microstructure, hardness and wear

B.N. Mordyuk, V.V. Silberschmidt, G.I. Prokopenko, Yu.V. Nesterenko, M.O. Iefimov

Materials Characterization· Volume 61· Issue 11
Publisher page

Abstract

Abstract Two types of Ti particles are used in an ultrasonic impact peening (UIP) process to modify sub-surface layers of cp aluminium atomized, with an average size of approx. 20 μm and milled (0.3–0.5 μm). They are introduced into a zone of severe plastic deformation induced by UIP. The effect of Ti particles of different sizes on microstructure, phase composition, microhardness and wear resistance of sub-surface composite layers in aluminium is studied in this paper. The formed layers of a composite reinforced with smaller particles have a highly misoriented fine-grain microstructure of its matrix with a mean grain size of 200–400 nm, while reinforcement with larger particles results in relatively large Al grains (1–2 μm). XRD, SEM, EDX and TEM studies confirm significantly higher particle/matrix bonding in the former case due to formation of a Ti 3 Al interlayer around Ti particles with rough surface caused by milling. Different microstructures determine hardness and wear resistance of reinforced aluminium layers: while higher magnitudes of microhardness are observed for both composites (when compared with those of annealed and UIP-treated aluminium), the wear resistance is improved only in the case of reinforcement with small particles.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Surface Treatment and Residual Stress · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Clyne · 1993
2. Fatigue of particle and whisker-reinforced metal-matrix composites10.1016/S0079-6425(00)00006-2 ↗
3. Effects of nano-diamond particles on the structure and tribological property of Ni-matrix nanocomposite coatings10.1016/j.msea.2004.08.033 ↗
4. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
5. Friction stir processing: a novel technique for fabrication of surface composite10.1016/S0921-5093(02)00199-5 ↗
6. Microstructures and mechanical properties of Al/Al2O3 surface nano-composite layer produced by friction stir processing10.1016/j.msea.2008.09.064 ↗
7. XRD investigation of thermostability of TiB2/Al deformation layer introduced by shot peening10.1016/j.msea.2007.07.004 ↗
8. Fabrication of Ti–Al coatings by mechanical alloying method10.1016/j.surfcoat.2006.06.044 ↗
9. Investigation of physicomechanical characteristics of Al after saturation with Ti with the use of ultrasonic shock processing
10. Structural state of aluminium after ultrasonic-shock processing with a titanium powder
11. Structure, microhardness and damping characteristics of Al matrix composite reinforced with AlCuFe or Ti using ultrasonic impact peening10.1016/j.surfcoat.2009.10.009 ↗
12. Challenges and advances in nanocomposite processing techniques10.1016/j.mser.2006.11.002 ↗
13. Mechanical alloying and milling10.1016/S0079-6425(99)00010-9 ↗
14. Effect of in-situ TiC particulate on the wear resistance of spray-deposited 7075 Al matrix composite10.1016/j.matchar.2005.01.011 ↗
15. A study of microstructure and tribological behaviour of Al-4.5% Cu/Al3Ti composites10.1016/j.matchar.2009.01.012 ↗
16. Abrasive wear of aluminium composites — a review10.1016/S0043-1648(96)07228-6 ↗
17. Mordyuk · Mechanical alloying of powder materials by ultrasonic milling ultrasonics · 2004 · 42 · 43
18. Fatigue life improvement of α-titanium by novel ultrasonically assisted technique10.1016/j.msea.2006.07.119 ↗
19. Ultrasonic impact peening for surface properties' management10.1016/j.jsv.2007.03.054 ↗
20. Determination of residual stress in ceramics-metal composites by X-ray diffraction methods10.1016/0921-5093(89)90052-X ↗
21. State of residual stress in laser-deposited ceramic composite coatings on aluminium alloys10.1016/j.actamat.2006.07.049 ↗
22. Abrasive wear of 2124Al–SiC composites in the temperature range 20–200°C10.1016/j.jmatprotec.2006.01.010 ↗
23. Wear resistance of aluminium alloy and its composites reinforced by Al2O3 particles10.1016/j.jmatprotec.2006.10.021 ↗
24. Processing Ti3Al–SiC nanocomposites using high energy mechanical milling10.1016/j.msea.2003.10.231 ↗
25. Lattice imperfections in intermetallic Ti–Al alloys: an X-ray diffraction study of the microstructure by the Rietveld method10.1016/j.intermet.2005.05.004 ↗
26. Matrix grain refinement in Al–TiAl composites by severe plastic deformation: influence of particle size and processing route10.1016/j.msea.2006.03.027 ↗
27. Microstructural characterization of EN AW6061 alloy matrix composites with Ti3Al intermetallics reinforcement
28. Evolution of dislocation structure under shock-pulse loads at different frequencies
29. Amorphous, nanoquasicrystalline and nanocrystalline alloys in Al-based systems10.1016/S0079-6425(98)00005-X ↗
30. Formation of nanocrystalline surface layers in various metallic materials by near surface severe plastic deformation10.1016/j.stam.2003.10.015 ↗
31. Grain growth controlled by mobile particles on grain boundaries10.1016/j.scriptamat.2006.04.006 ↗
32. Hirsch · 1965
33. Plastic-strain cyclic response of SiC particulate reinforced aluminum composites10.1016/S0921-5093(02)00012-6 ↗
34. Internal friction behaviour in SiC particulate reinforced aluminum metal matrix composite in thermal cycling10.1016/j.jallcom.2005.12.121 ↗
35. Study on abrasive and erosive wear behaviour of Al 6063/TiB2 in situ composites10.1016/j.msea.2008.09.003 ↗
36. An analytical study on strengthening of particulate reinforced metal matrix composites10.1016/1359-6454(95)00150-9 ↗
37. Low and high temperature hardness of WC-6%Co alloys10.1016/S0263-4368(97)81231-0 ↗
38. Intermetallic coatings produced by TIG surface melting10.1016/S0924-0136(01)00609-4 ↗
39. Influence of in situ formed TiB2 particles on the abrasive wear behaviour of Al–4Cu alloy10.1016/j.msea.2007.02.117 ↗
40. Friction properties of Al-1.5 Pct Mg/SiC particulate metal-matrix composites10.1007/BF02665513 ↗
41. Abrasive wear of Al2O3-reinforced aluminium-based MMCs10.1016/S0266-3538(01)00131-2 ↗