In-situ observation on the growth of Widmanstätten sideplates in an Fe–C–Mn steel
Source abstract
Abstract
Abstract The growth behavior of Widmanstatten plates as well as their lengthening rate in an Fe–0.09C–1.48Mn (weight percent) alloy were examined in-situ on the specimen surface and in bulk specimen by the traditional quench-arrest experiments. Widmanstatten plates directly emanated from austenite grain boundaries and/or from the existing ferrite allotriomorphs, i.e. through the mechanism of edge-to-face sympathetic nucleation. Simultaneously, face-to-face sympathetic nucleation could also occur on the broad face of pre-formed plates. The growth of Widmanstatten plates on the free surface did not occur at a constant lengthening rate but was accompanied by acceleration and deceleration. The average plate lengthening rate measured on the free surface was about one order of magnitude larger than that measured in bulk specimen. The former was close to the plate lengthening rate predicted by the modified Zener–Hillert model assuming paraequilibrium, while, the latter was close to the one that assumes negligible partition local equilibrium.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metallurgy and Material Forming · Magnetic Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. The mechanism of phase transformation in metals
2. Widmanstätten ferrite formation in iron-carbon alloys
3. Sympathetic nucleation of ferrite
4. Sympathetic nucleation: an overview10.1016/0921-5107(95)80022-0 ↗
5. Computer simulation of morphological change of grain boundary precipitates growing by the ledge mechanism10.1007/BF02660655 ↗
6. The evolution and growth kinetics of precipitate plates growing by the ledge mechanism10.1016/0956-7151(94)90193-7 ↗
7. The formation mechanism(s), morphology, crystallography of ferrite plates and crystallography of ferrite plates10.1007/BF02649812 ↗
8. New insights into the Widmanstätten proeutectoid ferrite transformation: integration of crystallographic and three-dimensional morphological observations10.1007/s11661-005-0213-1 ↗
9. In situ observation of Widmanstätten ferrite formation in a low-carbon steel10.1016/j.msea.2005.07.015 ↗
10. Widmanstätten ferrite plate formation in low-carbon steels10.1007/s11661-004-0276-4 ↗
11. Diffusion controlled precipitate growth in ternary systems10.1007/BF02642453 ↗
12. Hillert · 1969 · 231
13. Thermo-Calc Software
14. Growth kinetics of proeutectoid ferrite in Fe–0.1C–1.5Mn–1Si quaternary and Fe–0.1C–1.5Mn–1Si–0.2Al quinary alloys10.1007/s11661-011-1000-9 ↗
15. Thermionic emission microscope study of the formation of ferrite plates10.1016/0001-6160(64)90116-6 ↗
16. An in situ hot stage transmission electron microscopy study of the decomposition of Fe–C austenite10.1007/BF00369670 ↗
17. Ferrite formation in Fe–C alloys during austenite decomposition under non-equilibrium interface conditions10.1016/S0921-5093(97)00365-1 ↗
18. Diffusion in growth of bainite10.1007/BF02649044 ↗
19. Diffusion and interface control of reactions in alloys10.1007/BF02673664 ↗
20. Lengthening kinetics of ferrite and bainite plate10.1007/BF02644517 ↗
21. Effect of concentration-dependent diffusion coefficient on the migration of interphase boundaries10.1063/1.1710174 ↗
22. Enomoto · 2000
23. Thermodynamics of the bainite reaction
24. A revised expression for the diffusivity of carbon in binary Fe–C austenite10.1016/0036-9748(86)90384-4 ↗
25. Diffusion coefficient of carbon in austenite
26. Application of cyclic partial phase transformations for identifying kinetics transitions during solid-state phase transformations: experiments and modeling10.1016/j.actamat.2011.07.033 ↗
27. Analysis of ferrite growth retardation induced by local Mn enrichment in austenite created by prior interface passages10.1016/j.actamat.2012.11.011 ↗
28. Experimental kinetics of bainite formation
29. Phase-field simulation of austenite to ferrite transformation and Widmanstätten ferrite formation in Fe–C alloy10.2320/matertrans.47.2725 ↗