Insight into the effect of weld pitch on the microstructure-properties relationships of St 37/AISI 316 steels dissimilar welds processed by friction stir welding
Source abstract
Abstract
Abstract This research aims to evaluate the effect of weld pitch on the microstructure and properties of St 37/AISI 316 steels friction stir welds. The microstructure and microtexture of the samples were studied by means of electron backscatter diffraction analysis. The mechanical behaviors of the weldments were also investigated by microhardness, shear punch testing, and uniaxial tensile testing. In addition, the corrosion behavior of the welds was also evaluated. It was observed that the weld pitch of 0.0830 or 0.0625 mm/rotation resulted in producing defect-free welds with acceptable tensile strength level. Moreover, hardness and shear strength of the weld zone were improved up to 57% and 74%, respectively as compared to the base metals. It was due to the grain refinement which occurred within the stir zones by activating the dynamic recrystallization mechanism. Initial texture components of the base metals were replaced by recrystallized texture components in the stir zones. Orientation of grains in the stir zones was found to be highly dependent on the weld pitch. Regarding the corrosion resistance, the obtained results revealed that stir zone of St 37 steel was the weakest part of the weldments. Overall, the weldment employing the weld pitch of 0.0625 mm/rotation was found to achieve superior microstructural features and optimum properties.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Optimization of laser welding process parameters in dissimilar joint of stainless steel AISI316/AISI1018 low carbon steel to attain the maximum level of mechanical properties through PWHT10.1016/j.optlastec.2018.11.035 ↗
2. Microstructure and mechanical properties of dissimilar friction stir spot welding between St37 steel and 304 stainless steel10.1007/s11665-017-2703-x ↗
3. Effect of pulse width in pulsed Nd:YAG dissimilar laser welding of austenitic stainless steel (304 L) and carbon steel (st37)10.1007/s40516-018-0069-z ↗
4. Pivotal microstructural characteristics to determine the cryogenic impact toughness of dissimilar joint between SA645 and AISI304L made by autogenous fiber laser welding10.1016/j.matchar.2020.110399 ↗
5. Microstructural characterization and mechanical properties of TIG-welded API 5L X60 HSLA steel and AISI 310S stainless steel dissimilar joints10.1007/s11661-018-4890-y ↗
6. Microstructural characterization in dissimilar friction stir welding between 304 stainless steel and st37 steel10.1016/j.matchar.2012.09.004 ↗
7. Microstructure and failure behavior of dissimilar resistance spot welds between low carbon galvanized and austenitic stainless steels10.1016/j.msea.2007.07.007 ↗
8. Friction stir lap welding of stainless steel and plain carbon steel to enhance corrosion properties10.1016/j.jmatprotec.2018.04.048 ↗
9. Microstructure and mechanical properties of dissimilar friction stir welded type 304 austenitic stainless steel to Q235 low carbon steel10.1016/j.matchar.2019.109803 ↗
10. Effect of tool offset and rotational speed in dissimilar friction stir welding of AISI 304 stainless steel and mild steel10.1007/s11665-019-04362-y ↗
11. Kumar · 2015
12. Microstructure and mechanical properties of a dissimilar friction stir weld between austenitic stainless steel and low carbon steel10.1016/j.jmst.2013.02.008 ↗
13. Evaluation of mechanical properties using shear-punch testing10.1016/j.msea.2004.12.048 ↗
14. Semisolid joining of aluminum A356 alloy by partial remelting and mechanical stirring10.1016/S1003-6326(09)60376-9 ↗
15. A Local mechanical properties , microstructure , and microtexture in friction stir welded Ti-6Al-4V alloy10.1016/j.msea.2019.01.077 ↗
16. Corrosion studies using potentiodynamic and EIS electrochemical techniques of welded lean duplex stainless steel UNS S8244110.1016/j.apsusc.2016.01.260 ↗
17. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
18. Investigations on the effects of friction stir welding parameters on intermetallic and defect formation in joining aluminum alloy to mild steel10.1016/j.matdes.2013.01.013 ↗
19. Elimination of tunnel defect in ultrasonic vibration enhanced friction stir welding10.1016/j.matdes.2015.10.131 ↗
20. Microstructure and mechanical characterization of Incoloy 825 Ni-based alloy welded to 2507 super duplex stainless steel through dissimilar friction stir welding10.1016/S1003-6326(19)65074-0 ↗
21. Friction stir welding of mild steel to alloy 625 - development of welding parameters10.1179/1362171814Y.0000000198 ↗
22. Microstructural evolution during friction stir welding of mild steel and Ni-based alloy 62510.1007/s11661-016-3925-5 ↗
23. Interfacial microstructural and corrosion characterizations of friction stir welded AA6061-T6 and AISI304 materials10.1007/s12540-018-00222-x ↗
24. High speed friction stir welding of 5182-H111 alloy: temperature and microstructural insights into deformation mechanisms
25. Mechanical properties and microstructural evaluation of AA1100 to AZ31 dissimilar friction stir welds10.1016/j.matchemphys.2015.12.046 ↗
26. Friction stir welding studies on mild steel - process results, microstructures, and mechanical properties are reported
27. Microstructure and mechanical properties of friction stir welded lean duplex stainless steel10.1016/j.msea.2012.10.068 ↗
28. On the formation of grain structure during friction stir welding of duplex stainless steel10.1016/j.msea.2010.07.011 ↗
29. Evolution of grain boundary character distributions in alloy 825 tubes during high temperature annealing: is grain boundary engineering achieved through recrystallization or grain growth?10.1016/j.matchar.2016.11.016 ↗
30. Mechanism of grain structure development for pure cu and cu-30Zn with low stacking fault energy during FSW mechanism of grain structure development for pure cu and cu-30Zn with low
31. A comparative study on the microstructure development of friction stir welded 304 austenitic , 430 ferritic , and 2205 duplex stainless steels10.1016/j.matchemphys.2019.121833 ↗
32. Microstructural evolution and mechanical properties of the stir zone in friction stir processed AISI201 stainless steel10.1016/j.matdes.2016.05.106 ↗
33. Evolution of microstructure and crystallographic texture during dissimilar friction stir welding of duplex stainless steel to low carbon-manganese structural St10.1007/s11661-018-5023-3 ↗
34. Microstructural evolution of friction stir welded SAF 2205 duplex stainless steel10.1016/j.jallcom.2017.12.310 ↗
35. Friction-stir welding of ultrafine grained austenitic 304L stainless steel produced by martensitic thermomechanical processing10.1016/j.matdes.2015.03.052 ↗
36. Microstructure and mechanical properties of friction stir processed AISI 316L stainless steel10.1016/j.matdes.2014.10.082 ↗
37. Engineering tensile properties by controlling welding parameters and microstructure in a mild steel processed by friction stir welding10.1016/j.msea.2016.06.008 ↗
38. Characterization and mechanical behavior of AISI 316L / Incoloy 825 dissimilar welds processed by friction stir welding10.1016/j.jmapro.2020.03.045 ↗
39. Lippold · 2015
40. Structural refinement in austenitic stainless steel by submerged friction stir processing10.1016/j.matchemphys.2017.05.034 ↗
41. A metallurgical and mechanical study on dissimilar Friction Stir welding of aluminum 1050 to brass (CuZn30)10.1016/j.msea.2011.06.004 ↗
42. Microstructure evolution and mechanical properties of friction stir welding super-austenitic stainless steel S3265410.1016/j.matdes.2017.01.034 ↗
43. Microstructure, mechanical and corrosion properties of friction stir welded high nitrogen nickel-free austenitic stainless steel10.1016/j.matdes.2015.06.103 ↗
44. Correlation between weld nugget grain size , weld nugget hardness and tensile strength of friction stir welded commercial grade aluminium alloy joints10.1016/j.matdes.2011.07.054 ↗
45. Influence of friction stir welding parameters on grain size and formability in 5083 aluminum alloy10.1016/j.msea.2006.12.079 ↗
46. Corrosion studies of austenitic and duplex stainless steels in aqueous lithium bromide solution at different temperatures10.1016/j.corsci.2004.05.025 ↗
47. Laser beam welding of Waspaloy : characterization and corrosion behavior evaluation10.1016/j.optlastec.2016.03.011 ↗
48. Dissimilar welding between AISI 304 stainless steel and AISI 1020 carbon steel plates
49. Grain boundary engineering of titanium-stabilized 321 austenitic stainless steel10.1007/s10853-010-5244-3 ↗
50. Improving the intergranular corrosion resistance of 304 stainless steel by grain boundary network control10.1016/j.corsci.2011.02.005 ↗
51. Micro-texture and corrosion behavior of dissimilar joints of UNS S32750 stainless steel/UNS N08825 Ni-based superalloy10.1016/j.matchar.2019.109802 ↗
52. Influence of texture on corrosion rate of AZ31 Mg alloy in 3 . 5 wt .% NaCl10.1016/j.matdes.2011.04.031 ↗