Determining the heat treatment behaviour of metal injection moulded and wrought alloy 718 using differential scanning calorimetry
Source abstract
Abstract
Abstract The heat treatment behaviour of metal injection moulded (MIM) and wrought alloy 718 was investigated using DSC, microscopy and hardness measurements. Reheating solutionized samples in the DSC resulted in a distinct exothermic peak around 725 °C, which was attributed to γ" precipitation. This was followed by a broad endothermic region (~750-900 °C), which was attributed to the dissolution of γ' and γ" precipitates. No DSC peak was observed corresponding to γ' precipitation upon reheat. The endothermic dissolution region (750–900 °C) ended with an abrupt exothermic shoulder around 900 °C, which was attributed to the solvus of the γ'/γ" precipitates and an acceleration of δ phase precipitation. Ageing the samples at progressively higher temperatures and for longer times resulted in a decrease in the 725 °C exothermic γ" precipitation peak and a deepening of the 750–900 °C endothermic dissolution region. Also, samples with higher Al content exhibited a deeper dissolution trough and a small bump in the exothermic shoulder at the end of this trough (~880 °C), which were attributed to the higher levels of γ' observed in the FESEM for these samples. A shallow endothermic trough peaking between 1000 and 1045 °C was observed in samples treated below the δ phase solvus and was attributed to dissolution of the δ phase. Hardness measurements showed an increase in hardness with the amount of γ' and γ" precipitated as expected. Differences in heat treatment behaviour appeared to be driven largely by differences in chemical composition rather than by processing route (wrought vs. MIM). However, the MIM material had smaller, more evenly distributed carbides and additional oxides not present in the wrought material which acted to restrict grain growth in samples solutionized up to 1232 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Injection Molding Process and Properties · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Superalloys, the most successful alloy system of modern times - past, present and future
2. Alloy 718 at Pratt and Whitney - historical perspective and future challenges
3. Application of alloy 718 in GE aircraft engines: Past, present and next five years
4. Donachie · 2002
5. Metallurgical factors influencing the machinability of Inconel 718
6. Status and prospects of alloy 718
7. Microstructure and mechanical properties of Inconel 625 and 718 alloys processed by powder injection molding
8. Metal injection molding of alloy 718 for aerospace applications10.1007/s11837-012-0246-z ↗
9. Effect of solution treatment temperature on the microstructure and tensile properties of P/M (HIP) processed superalloy Inconel 718
10. Effect of standard heat treatment on the microstructure and mechanical properties of hot isostatically pressed superalloy Inconel 71810.1016/S0921-5093(03)00079-0 ↗
11. Influence of modified processing on structure and properties of hot isostatically pressed superalloy Inconel 71810.1016/j.msea.2005.11.031 ↗
12. Effect of heat treatment on microstructure and mechanical properties of the hot-isostatic-pressed Inconel 718 powder compact10.1016/j.jallcom.2013.12.107 ↗
13. Differential thermal analysis of nickel-base superalloys
14. Metallography of alloy 718
15. The physical metallurgy of cast and wrought alloy 718
16. Loomis · 1969
17. Étude du comportement structural de l’alliage NC 19 Fe Nb (Inconel 718)
18. Some features of anisothermal solid-state transformations in alloy 71810.1016/j.matchar.2010.02.011 ↗
19. Effects of cold rolling on the precipitation kinetics and the morphology evolution of intermediate phases in Inconel 718 alloy10.1016/j.jallcom.2015.07.149 ↗
20. Determination of the γ’-solvus temperature of two commercial wrought Ni-base superalloys by thermal expansion measurements
21. 2007
22. ASTM · 2012
23. ASTM · 2013
24. Aging of the Inconel 718 alloy between 500 and 750 °C10.1557/JMR.1997.0306 ↗
25. Morphology of γ' and γ'' precipitates and thermal stability of Inconel 718 type alloys10.1007/BF02649604 ↗
26. The effect of varying Al, Ti, and Nb content on the phase stability of Inconel 71810.1007/BF02645133 ↗
27. The heat capacity of Inconel 718 from 313 to 1053 K10.1016/0022-3115(78)90463-4 ↗
28. The specific heat from 50 to 700° C of a nominal Ni (16 wt % Mo, 7 wt % Cr, 5 wt % Fe) alloy10.1016/0022-3115(66)90047-X ↗
29. Specific-heat anomalies in solid solutions of chromium and molybdenum in nickel: evidence for short-range order
30. Thermal property measurements of metal injection moulded Inconel 625 and Inconel 718 using combined thermal analysis techniques10.1080/00325899.2020.1805547 ↗
31. Short term precipitation kinetics of delta phase in strain free Inconel 718 alloy10.1179/026708304225019830 ↗
32. Delta phase precipitation in Inconel 71810.1016/j.matchar.2004.07.004 ↗