Durability of self-consolidating concrete to different exposure regimes of sodium sulfate attack
Source abstract
Abstract
This study investigates the durability of a wide scope of self-consolidating concrete (SCC) mixture designs to sodium sulfate attack. The mixture design variables included the type of binder (single, binary, ternary and quaternary), air-entrainment, sand-to-aggregate ratio and hybrid fibre reinforcement. Since current standard test methods (e.g. ASTM C 1012) generally do not address various sulfate attack exposure scenarios that may exist under field conditions, three different sulfate attack exposure regimes (full immersion, wetting-drying and partial immersion) were investigated in the current study. In the wetting-drying and partial immersion exposure regimes, results of the physico-mechanical properties revealed performance risks associated with some SCC mixture designs. Such risks were not captured by the full immersion exposure. Thermal, mineralogical and microscopy studies elucidated the complexity of degradation mechanisms, which in some cases varied at different locations of the same specimen. Findings from this study emphasize the need for performance standard tests that can better simulate various realistic field exposure regimes in order to achieve a more reliable and comprehensive evaluation of the resistance of concrete to sulfate attack.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Building materials and conservation · Concrete and Cement Materials Research · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. BIBM, CEMBUREAU, ERMCO, EFCA, EFNARC (2005) The European guidelines for self-compacting concrete. www.efnarc.org , p 63
2. ACI Committee 237 (ACI 237R-07) (2007) Self-consolidating concrete. American Concrete Institute, Farmington Hills, p 30
3. Khayat K, Ghezal A (2002) Optimizing self-consolidating concrete with limestone filler by using statistical factorial design methods. ACI Mater J 99(3):264–272
4. Lachemi M, Hossain KMA, Patel R, Shehata M, Bouzoubaa N (2007) Influence of paste/mortar rheology on the flow characteristics of high-volume fly ash self-consolidating concrete. Mag Concr Res 59(7):517–52810.1680/macr.2007.59.7.517 ↗
5. Zhu W, Bartos J (2003) Permeation properties of self-compacting concrete. Cem Concr Res 33(6):921–92610.1016/S0008-8846(02)01090-6 ↗
6. De Schutter G, Audenaert K (eds) (2007) Durability of self-compacting concrete, State-of-the-art report of RILEM Technical Committee 205-DSC, RILEM Report 38, RILEM Publications S.A.R.L., p 185
7. Boel V, Audenaert K, De Schutter G, Heirman G, Vandewalle L, Desmet B, Vantomme J (2007) Transport properties of self compacting concrete with limestone filler and fly ash. Mater Struct 40(5):507–51610.1617/s11527-006-9159-z ↗
8. Skalny J, Marchand J, Odler I (2002) Sulfate attack on concrete. Spon Press, London
9. Mehta PK (2000) Sulfate attack on concrete: separating myths from reality. Concr Int 22(8):57–61
10. Neville A (2004) The confused world of sulfate attack on concrete. Cem Concr Res 34(8):1275–129610.1016/j.cemconres.2004.04.004 ↗
11. Hewlett PC (ed) (1998) Lea’s chemistry of cement and concrete. Arnold, London
12. Crammond NJ (2003) The thaumasite form of sulfate attack in the UK. Cem Concr Comp 25(8):809–81810.1016/S0958-9465(03)00106-9 ↗
13. Haynes H, O’Neill R, Mehta PK (1996) Concrete deterioration from physical attack by salts. Concr Int 18(1):63–68
14. Hime W, Martinek R, Backus L, Marusin S (2001) Salt hydration distress. Concr Int 23(10):43–50
15. Persson B (2003) Sulphate resistance of self-compacting concrete. Cem Concr Res 33(12):1933–193810.1016/S0008-8846(03)00184-4 ↗
16. Nehdi M, Pardhan M, Koshowski S (2004) Durability of self-consolidating concrete incorporating high-volume replacement composite cements. Cem Concr Res 34(11):2103–211210.1016/j.cemconres.2004.03.018 ↗
17. American Society for Testing and Materials (2007) ASTM C 1012: Standard test method for length change of hydraulic-cement mortar exposed to a sulfate solution, Philadelphia, PA
18. American Society for Testing and Materials (2007) ASTM C 496: Standard test method for splitting tensile strength of cylindrical concrete specimens, Philadelphia, PA
19. American Society for Testing and Materials (2007) ASTM C 215: Standard test method for fundamental transverse, longitudinal, and torsional resonant frequencies of concrete specimens, Philadelphia, PA
20. American Society for Testing and Materials (2007) ASTM C 78: Standard test method for flexural strength of concrete using simple beam with third-point loading, Philadelphia, PA
21. Cohen D, Mather B (1991) Sulfate attack on concrete-research needs. ACI Mater J 88(1):62–69
22. Santhanam M (2001) Studies on sulfate attack: mechanisms, test methods, and modeling. PhD Dissertation, Purdue University, USA
23. Frearson J (1986) The sulfate resistance of combinations of portland cement and ground granulated blast furnace slag. In: Malhotra VM (ed) Proceedings of the second CANMET/ACI international conference on fly ash, silica fume, slag, and natural pozzolans in concrete, Madrid, Spain, ACI SP-91, vol II, pp 1495–1524
24. ACI Committee 201 (201.2R-01) (2001) Guide to durable concrete. American Concrete Institute, Farmington Hills, p 40
25. Montgomery D (2001) Design and analysis of experiments. Wiley, New York
26. Flatt R (2002) Salt damage in porous materials: how high supersaturates are generated. J Crystal Growth 242(3–4):435–45410.1016/S0022-0248(02)01429-X ↗
27. Thaulow N, Sahu S (2004) Mechanism of concrete deterioration due to salt crystallization. Mater Charact 53(2–4):123–12710.1016/j.matchar.2004.08.013 ↗
28. Rodriguez-Navarro C, Doehne E, Sebastian E (2000) How does sodium sulfate crystallize? Implications for the decay and testing of building materials. Cem Concr Res 30(10):1527–153410.1016/S0008-8846(00)00381-1 ↗
29. Folliard K, Sandberg P (1994) Mechanism of concrete deterioration by sodium sulfate crystallization. In: Malhotra VM (ed) Proceedings of the third CANMET/ACI international conference on durability of concrete, Nice, France, ACI SP-145, pp 933–945
30. Haynes H (2006) A mechanism of distress of concrete during crystallization of mirabilite. In: Malhotra VM (ed) Proceedings of the seventh CANMET/ACI international conference on durability of concrete, Montreal, Canada, ACI Supplementary Volume, pp 1–16
31. Rodriguez-Navarro C, Doehne E (1999) Salt weathering: influence of evaporation rate, supersaturation and crystallization pattern. Earth Surf Process Landf 24(2–3):191–20910.1002/(SICI)1096-9837(199903)24:3<191::AID-ESP942>3.0.CO;2-G ↗
32. Sahu S, Badger S, Thaulow N (2003) Evidence of thaumasite in Southern California concrete. Cem Concr Comp 24(3–4):379–384
33. Bassuoni MT, Nehdi M (2005) The case for air-entrainment in high performance concrete. ICE Struct Build 158(5):311–31910.1680/stbu.2005.158.5.311 ↗
34. Johnston C (2001) Fiber-reinforced cements and concretes. Gordon and Breach Science Publications, The Netherlands
35. Correns C (1949) Growth and dissolution of crystals under linear pressure. Faraday Society-Discussions 5:267–27110.1039/df9490500267 ↗