Implementing the effect of geopolymer concrete pore solution pH in the standard rapid migration test NT Build 492 protocol
Source abstract
Abstract
Abstract This research investigates the impact of the pore solution pH values on chloride content at the colour change boundary determined according to the standard rapid migration test (NT Build 492), with a focus on alkali-activated materials, so-called geopolymer. The study investigates a range of geopolymer formulations using various proportions of ground granulated blast furnace slag (GGBFS), fly ash, and calcined clay, alongside different activator concentrations, to examine their influence on the pH value of the pore solution. Findings from this study suggest that the pH value of the pore solution greatly influence in the chloride ion concentration at the colour change boundary, which should be accounted for in the calculation of the non-steady-state migration coefficients (Dnssm). It is noted that mixtures with higher GGBFS content exhibit higher pH values than mixtures containing fly ash or calcined clay, impacting the Dnssm. The results advocate for modifications to the standard NT Build 492 protocol to enhance its applicability and accuracy for geopolymer materials, emphasizing the importance of using revised Dnssm values calculated considering the unique properties of geopolymer concrete for more durability assessment.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Corrosion and Durability · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Barcelo L, Kline J, Walenta G, Gartner E (2013) Cement and carbon emissions. Mater Struct 47:1055–106510.1617/s11527-013-0114-5 ↗
2. van Deventer JSJ, White CE, Myers RJ (2020) A roadmap for production of cement and concrete with low-CO2 emissions. Waste Biomass Valoriz 12:4745–477510.1007/s12649-020-01180-5 ↗
3. Miller SA, Van Roijen E, Cunningham P, Kim A (2021) Opportunities and challenges for engineering construction materials as carbon sinks. RILEM Techn Lett 6:105–11810.21809/rilemtechlett.2021.146 ↗
4. Angst UM (2023) Steel corrosion in concrete—Achilles’ heel for sustainable concrete? Cement Concr Res 172:10723910.1016/j.cemconres.2023.107239 ↗
5. Li K, Li L (2019) Crack-altered durability properties and performance of structural concretes. Cement Concr Res 124:10581110.1016/j.cemconres.2019.105811 ↗
6. Douglas Hooton R (2019) Future directions for design, specification, testing, and construction of durable concrete structures. Cement Concr Res 124:10582710.1016/j.cemconres.2019.105827 ↗
7. Vaysburd AM, Emmons PH (2000) How to make today’s repairs durable for tomorrow—corrosion protection in concrete repair. Constr Build Mater 14:189–19710.1016/S0950-0618(00)00022-2 ↗
8. Tuutti K (1982) Corrosion of steel in concrete
9. Angst UM, Geiker MR, Alonso MC, Polder R, Isgor OB, Elsener B, Wong H, Michel A, Hornbostel K, Gehlen C, François R, Sanchez M, Criado M, Sørensen H, Hansson C, Pillai R, Mundra S, Gulikers J, Raupach M, Pacheco J, Sagüés A (2019) The effect of the steel–concrete interface on chloride-induced corrosion initiation in concrete: a critical review by RILEM TC 262-SCI. Mater Struct 52:8810.1617/s11527-019-1387-0 ↗
10. Angst U, Elsener B, Larsen CK, Vennesland Ø (2009) Critical chloride content in reinforced concrete—a review. Cement Concr Res 39:1122–113810.1016/j.cemconres.2009.08.006 ↗
11. Rodriguez J, Ortega L, Casal J, Diez J (2018) Corrosion of reinforcement and service life of concrete structures. In: Durability of Building Materials and Components 7. Routledge, pp 117–12610.4324/9781315025025-13 ↗
12. Li K (2017) Durability design of concrete structures: Phenomena, modeling, and practice. John Wiley and Sons, Hoboken
13. Nguyen QD, Castel A (2023) Long-term durability of underground reinforced concrete pipes in natural chloride and carbonation environments. Constr Build Mater 394:13223010.1016/j.conbuildmat.2023.132230 ↗
14. Glass G, Buenfeld N (2000) Chloride-induced corrosion of steel in concrete. Prog Struct Eng Mater 2:448–45810.1002/pse.54 ↗
15. Bertolini L, Elsener B, Pedeferri P, Redaelli E, Polder RB (2013) Corrosion of steel in concrete: prevention, diagnosis, repair. John Wiley and Sons, Hoboken10.1002/9783527651696 ↗
16. NT Build 492 (1999-11) (1999) Concrete, mortar and cement-based repair materials: chloride migration coefficient from non-steady-state migration experiments, Nordtest, Espoo, Finland
17. Pontes J, Bogas JA, Real S, Silva A (2021) The rapid chloride migration test in assessing the chloride penetration resistance of normal and lightweight concrete. Appl Sci 11:725110.3390/app11167251 ↗
18. Maes M, Gruyaert E, De Belie N (2013) Resistance of concrete with blast-furnace slag against chlorides, investigated by comparing chloride profiles after migration and diffusion. Mater Struct 46:89–10310.1617/s11527-012-9885-3 ↗
19. Yuan Q, Shi C, He F, De Schutter G, Audenaert K, Zheng K (2008) Effect of hydroxyl ions on chloride penetration depth measurement using the colorimetric method. Cement Concr Res 38:1177–118010.1016/j.cemconres.2008.04.003 ↗
20. Grant Norton M, Provis JL (2020) 1000 at 1000: geopolymer technology—the current state of the art. J Mater Sci 55:13487–1348910.1007/s10853-020-04990-z ↗
21. Noushini A, Nguyen QD, Castel A (2021) Assessing alkali-activated concrete performance in chloride environments using NT Build 492. Mater Struct 54:5710.1617/s11527-021-01652-7 ↗
22. Gomes SDC, Nguyen QD, Li W, Castel A (2023) Carbonation resistance of calcined clay-ground granulated blast furnace slag alkali-activated mortar. Constr Build Mater 393:13181110.1016/j.conbuildmat.2023.131811 ↗
23. Noushini A, Castel A, Aldred J, Rawal A (2020) Chloride diffusion resistance and chloride binding capacity of fly ash-based geopolymer concrete. Cement Concr Compos 105:10329010.1016/j.cemconcomp.2019.04.006 ↗
24. Lloyd RR, Provis JL, van Deventer JSJ (2010) Pore solution composition and alkali diffusion in inorganic polymer cement. Cement Concr Res 40:1386–139210.1016/j.cemconres.2010.04.008 ↗
25. Bernal SA, Provis JL, Brice DG, Kilcullen A, Duxson P, van Deventer JSJ (2012) Accelerated carbonation testing of alkali-activated binders significantly underestimates service life: the role of pore solution chemistry. Cement Concr Res 42:1317–132610.1016/j.cemconres.2012.07.002 ↗
26. Noushini A, Castel A (2018) Performance-based criteria to assess the suitability of geopolymer concrete in marine environments using modified ASTM C1202 and ASTM C1556 methods. Mater Struct 51:14610.1617/s11527-018-1267-z ↗
27. Vollpracht A, Lothenbach B, Snellings R, Haufe J (2016) The pore solution of blended cements: a review. Mater Struct 49:3341–336710.1617/s11527-015-0724-1 ↗
28. ASTM C39/C39M-18 (2018) Standard test method for compressive strength of cylindrical concrete specimens. ASTM International, West Conshohocken
29. Nguyen QD, Khan MSH, Castel A (2020) Chloride diffusion in limestone flash calcined clay cement concrete. ACI Mater J 117:165
30. ASTM C1152/C1152M Standard Test Method for Acid-Soluble Chloride in Mortar and Concrete. ASTM International, West Conshohocken
31. ASTM C1218/C1218M-20 Standard Test Method for Water-Soluble Chloride in Mortar and Concrete. ASTM International, West Conshohocken
32. Tang J, Wei S, Li W, Ma S, Ji P, Shen X (2019) Synergistic effect of metakaolin and limestone on the hydration properties of Portland cement. Constr Build Mater 223:177–18410.1016/j.conbuildmat.2019.06.059 ↗
33. Tennakoon C, Shayan A, Sanjayan JG, Xu A (2017) Chloride ingress and steel corrosion in geopolymer concrete based on long term tests. Mater Des 116:287–29910.1016/j.matdes.2016.12.030 ↗
34. AS 3600 (2018) Concrete structures. Standards Australia, Sydney
35. Alventosa KML, White CE (2021) The effects of calcium hydroxide and activator chemistry on alkali-activated metakaolin pastes. Cement Concr Res 145:10645310.1016/j.cemconres.2021.106453 ↗
36. Zuo Y, Nedeljković M, Ye G (2019) Pore solution composition of alkali-activated slag/fly ash pastes. Cement Concr Res 115:230–25010.1016/j.cemconres.2018.10.010 ↗
37. Nobuaki O, Shigeyoshi N, Kenji N (1992) Evaluation of AgNO 3 solution spray method for measurement of chloride penetration into hardened cementitious matrix materials. ACI Mater J 89:587
38. He F, Shi C, Yuan Q, Chen C, Zheng K (2012) AgNO3-based colorimetric methods for measurement of chloride penetration in concrete. Constr Build Mater 26:1–810.1016/j.conbuildmat.2011.06.003 ↗
39. Elfmarkova V, Spiesz P, Brouwers HJH (2015) Determination of the chloride diffusion coefficient in blended cement mortars. Cement Concr Res 78:190–19910.1016/j.cemconres.2015.06.014 ↗
40. Meck E, Sirivivatnanon V (2003) Field indicator of chloride penetration depth. Cement Concr Res 33:1113–111710.1016/S0008-8846(03)00012-7 ↗
41. Andrade C, Castellote M, Alonso C, González C (1999) Relation between colourimetric chloride penetration depth and charge passed in migration tests of the type of standard ASTM C1202–91. Cement Concr Res 29:417–42110.1016/S0008-8846(98)00226-9 ↗
42. He F, Shi C, Yuan Q, An X, Tong B (2011) Calculation of chloride concentration at color change boundary of AgNO3 colorimetric measurement. Cement Concr Res 41:1095–110310.1016/j.cemconres.2011.06.008 ↗
43. Song S, Jennings HM (1999) Pore solution chemistry of alkali-activated ground granulated blast-furnace slag. Cement Concr Res 29:159–17010.1016/S0008-8846(98)00212-9 ↗
44. Babaee M, Castel A (2018) Water vapor sorption isotherms, pore structure, and moisture transport characteristics of alkali-activated and Portland cement-based binders. Cement Concr Res 113:99–12010.1016/j.cemconres.2018.07.006 ↗
45. ASTM C642-06 Standard Test Method for Density, Absorption, and Voids in Hardened Concrete. ASTM International, West Conshohocken
46. Tang L (1996) Electrically accelerated methods for determining chloride diffusivity in concrete—current development. Mag Concr Res 48:173–17910.1680/macr.1996.48.176.173 ↗