journal article·2019-10Open access

Waste glass as binder in alkali activated slag–fly ash mortars

G. Liu, M. V. A. Florea, H. J. H. Brouwers

Materials and Structures· Volume 52· Issue 5

Abstract

Abstract This paper illustrates the application of waste glass powder as part of the binder in slag–fly ash systems activated by NaOH and NaOH/Na2CO3 activators. To evaluate the reaction kinetics, reaction products, mechanical properties, and durability performance of glass powder modified alkali activated slag–fly ash systems, calorimetry test, X-ray diffraction, FTIR, strength test, drying shrinkage tests, and carbonation test were conducted. From the isothermal calorimeter results, glass powder shows a higher reactivity compared to fly ash but still lower than slag. The reaction products of glass power modified samples exhibit an enhancement of polymerization degree of Si–O–T, observed in FTIR. As a consequence, higher drying shrinkage exists in glass modified mortars. The mechanical performance of different samples is mostly controlled by the Ca/Si of dry mixtures and activator type. After the slag–fly ash binder system was modified by the waste glass, a significant enhancement of resistance to carbonation was identified, especially for NaOH/Na2CO3 activated mortars, which show an increase of 300% on the carbonation resistance ability compared to the reference sample. The Na/(Si + Al) ratio of dry mixtures exhibits a positive correlation with carbonation resistance.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Feiz R, Ammenberg J, Eklund M, Helgstrand A, Marshall R (2015) Improving the CO2 performance of cement, part I: utilizing life-cycle assessment and key performance indicators to assess development within the cement industry. J Clean Prod 98:272–28110.1016/j.jclepro.2014.01.083 ↗
2. Yang K-H, Jung Y-B, Cho M-S, Tae S-H (2015) Effect of supplementary cementitious materials on reduction of CO2 emissions from concrete. J Clean Prod 103:774–78310.1016/j.jclepro.2014.03.018 ↗
3. Torres-Carrasco M, Puertas F (2015) Waste glass in the geopolymer preparation. Mechanical and microstructural characterisation. J Clean Prod 90:397–40810.1016/j.jclepro.2014.11.074 ↗
4. Crossin E (2015) The greenhouse gas implications of using ground granulated blast furnace slag as a cement substitute. J Clean Prod 95:101–10810.1016/j.jclepro.2015.02.082 ↗
5. Liu G, Florea MVA, Brouwers HJH (2019) Performance evaluation of sustainable high strength mortars incorporating high volume waste glass as binder. Constr Build Mater 202:574–58810.1016/j.conbuildmat.2018.12.110 ↗
6. Liu G, Florea MVA, Brouwers HJH (2018) The hydration and microstructure characteristics of cement pastes with high volume organic-contaminated waste glass powder. Constr Build Mater 187:1177–118910.1016/j.conbuildmat.2018.07.162 ↗
7. Zeng Q, Li K, Fen-chong T, Dangla P (2012) Pore structure characterization of cement pastes blended with high-volume fly-ash. Cem Concr Res 42(1):194–20410.1016/j.cemconres.2011.09.012 ↗
8. Kayali O, Sharfuddin Ahmed M (2013) Assessment of high volume replacement fly ash concrete—concept of performance index. Constr Build Mater 39:71–7610.1016/j.conbuildmat.2012.05.009 ↗
9. Brough A, Atkinson A (2002) Sodium silicate-based, alkali-activated slag mortars: part I. Strength, hydration and microstructure. Cem Concr Res 32(6):865–87910.1016/S0008-8846(02)00717-2 ↗
10. Jeon D, Jun Y, Jeong Y, Oh JE (2015) Microstructural and strength improvements through the use of Na2CO3 in a cementless Ca(OH)2-activated Class F fly ash system. Cem Concr Res 67:215–22510.1016/j.cemconres.2014.10.001 ↗
11. Škvára F, Kopecký L, Šmilauer V, Bittnar Z (2009) Material and structural characterization of alkali activated low-calcium brown coal fly ash. J Hazard Mater 168(2–3):711–72010.1016/j.jhazmat.2009.02.089 ↗
12. Ye H, Cartwright C, Rajabipour F, Radlińska A (2017) Understanding the drying shrinkage performance of alkali-activated slag mortars. Cem Concr Compos 76:13–2410.1016/j.cemconcomp.2016.11.010 ↗
13. Ma Y, Ye G (2015) The shrinkage of alkali activated fly ash. Cem Concr Res 68:75–8210.1016/j.cemconres.2014.10.024 ↗
14. Lee NK, Jang JG, Lee HK (2014) Shrinkage characteristics of alkali-activated fly ash/slag paste and mortar at early ages. Cem Concr Compos 53:239–24810.1016/j.cemconcomp.2014.07.007 ↗
15. Gao X, Yu QL, Brouwers HJH (2016) Assessing the porosity and shrinkage of alkali activated slag–fly ash composites designed applying a packing model. Constr Build Mater 119:175–18410.1016/j.conbuildmat.2016.05.026 ↗
16. Ballekere Kumarappa D, Peethamparan S, Ngami M (2018) Autogenous shrinkage of alkali activated slag mortars: basic mechanisms and mitigation methods. Cem Concr Res 109:1–910.1016/j.cemconres.2018.04.004 ↗
17. Sugama T, Brothers LE, Van de Putte TR (2005) Acid-resistant cements for geothermal wells: sodium silicate activated slag/fly ash blends. Adv Cem Res 17(2):65–7510.1680/adcr.2005.17.2.65 ↗
18. Shayan A, Xu A (2006) Performance of glass powder as a pozzolanic material in concrete: a field trial on concrete slabs. Cem Concr Res 36(3):457–46810.1016/j.cemconres.2005.12.012 ↗
19. Spiesz P, Rouvas S, Brouwers HJH (2016) Utilization of waste glass in translucent and photocatalytic concrete. Constr Build Mater 128:436–44810.1016/j.conbuildmat.2016.10.063 ↗
20. Torres-Carrasco M, Puertas F (2017) Waste glass as a precursor in alkaline activation: chemical process and hydration products. Constr Build Mater 139:342–35410.1016/j.conbuildmat.2017.02.071 ↗
21. Vafaei M, Allahverdi A (2017) High strength geopolymer binder based on waste-glass powder. Adv Powder Technol 28(1):215–22210.1016/j.apt.2016.09.034 ↗
22. Puertas F, Torres-Carrasco M (2014) Use of glass waste as an activator in the preparation of alkali-activated slag. Mechanical strength and paste characterisation. Cem Concr Res 57:95–10410.1016/j.cemconres.2013.12.005 ↗
23. Martinez-Lopez R, Ivan Escalante-Garcia J (2016) Alkali activated composite binders of waste silica soda lime glass and blast furnace slag: strength as a function of the composition. Constr Build Mater 119:119–12910.1016/j.conbuildmat.2016.05.064 ↗
24. Shi Z, Shi C, Wan S, Li N, Zhang Z (2018) Effect of alkali dosage and silicate modulus on carbonation of alkali-activated slag mortars. Cem Concr Res 113:55–6410.1016/j.cemconres.2018.07.005 ↗
25. D EN (2009) Methods of testing cement—part 3: determination of setting times and soundness
26. BS EN (2005) Methods of testing cement—part 1: determination of strength, vol 3
27. Leemann A, Moro F (2017) Carbonation of concrete: the role of CO2 concentration, relative humidity and CO2 buffer capacity. Mater Struct Constr 50(1):1–1410.1617/s11527-016-0917-2 ↗
28. Gao X, Yu QL, Brouwers HJH (2015) Reaction kinetics, gel character and strength of ambient temperature cured alkali activated slag–fly ash blends. Constr Build Mater 80:105–11510.1016/j.conbuildmat.2015.01.065 ↗
29. Puertas F et al (2018) Alkali-activated slag concrete: fresh and hardened behaviour. Cem Concr Compos 85:22–3110.1016/j.cemconcomp.2017.10.003 ↗
30. Fang G, Bahrami H, Zhang M (2018) Mechanisms of autogenous shrinkage of alkali-activated fly ash–slag pastes cured at ambient temperature within 24 h. Constr Build Mater 171:377–38710.1016/j.conbuildmat.2018.03.155 ↗
31. Song S, Jennings HM (1999) Pore solution chemistry of alkali-activated ground granulated blast-furnace slag. Cem Concr Res 29(2):159–17010.1016/S0008-8846(98)00212-9 ↗
32. Yuan B, Yu QL, Brouwers HJH (2017) Assessing the chemical involvement of limestone powder in sodium carbonate activated slag. Mater Struct 50(2):13610.1617/s11527-017-1003-0 ↗
33. Bernal SA, Provis JL, Myers RJ, San Nicolas R, van Deventer JSJ (2015) Role of carbonates in the chemical evolution of sodium carbonate-activated slag binders. Mater Struct 48(3):517–52910.1617/s11527-014-0412-6 ↗
34. Garbev K, Beuchle G, Bornefeld M, Black L, Stemmermann P (2008) Cell dimensions and composition of nanocrystalline calcium silicate hydrate solid solutions. Part 1: synchrotron-based X-ray diffraction. J Am Ceram Soc 91(9):3005–301410.1111/j.1551-2916.2008.02484.x ↗
35. Garbev K, Bornefeld M, Beuchle G, Stemmermann P (2008) Cell dimensions and composition of nanocrystalline calcium silicate hydrate solid solutions. Part 2: X-ray and thermogravimetry study. J Am Ceram Soc 91(9):3015–302310.1111/j.1551-2916.2008.02601.x ↗
36. Kumar A et al (2017) The atomic-level structure of cementitious calcium silicate hydrate. J Phys Chem C 121(32):17188–1719610.1021/acs.jpcc.7b02439 ↗
37. Toniolo N, Rincón A, Roether JA, Ercole P, Bernardo E, Boccaccini AR (2018) Extensive reuse of soda-lime waste glass in fly ash-based geopolymers. Constr Build Mater 188:1077–108410.1016/j.conbuildmat.2018.08.096 ↗
38. Ismail I, Bernal SA, Provis JL, San Nicolas R, Hamdan S, van Deventer JSJ (2014) Modification of phase evolution in alkali-activated blast furnace slag by the incorporation of fly ash. Cem Concr Compos 45:125–13510.1016/j.cemconcomp.2013.09.006 ↗
39. Bernal SA, Provis JL, Rose V, Mejía de Gutierrez R (2011) Evolution of binder structure in sodium silicate-activated slag–metakaolin blends. Cem Concr Compos 33(1):46–5410.1016/j.cemconcomp.2010.09.004 ↗
40. Zhang S, Keulen A, Arbi K, Ye G (2017) Waste glass as partial mineral precursor in alkali-activated slag/fly ash system. Cem Concr Res 102:29–4010.1016/j.cemconres.2017.08.012 ↗
41. Marjanović N, Komljenović M, Baščarević Z, Nikolić V, Petrović R (2015) Physical–mechanical and microstructural properties of alkali-activated fly ash–blast furnace slag blends. Ceram Int 41(1):1421–143510.1016/j.ceramint.2014.09.075 ↗
42. Fernández-Jiménez A, Palomo JG, Puertas F (1999) Alkali-activated slag mortars: mechanical strength behaviour. Cem Concr Res 29(8):1313–132110.1016/S0008-8846(99)00154-4 ↗
43. Fernández-Jiménez A, Puertas F, Sobrados I, Sanz J (2003) Structure of calcium silicate hydrates formed in alkaline-activated slag: influence of the type of alkaline activator. J Am Ceram Soc 86(8):1389–139410.1111/j.1151-2916.2003.tb03481.x ↗
44. Gonen T, Yazicioglu S (2007) The influence of compaction pores on sorptivity and carbonation of concrete. Constr Build Mater 21(5):1040–104510.1016/j.conbuildmat.2006.02.010 ↗
45. Bakharev T, Sanjayan J, Cheng Y-B (2003) Resistance of alkali-activated slag concrete to acid attack. Cem Concr Res 33(10):1607–161110.1016/S0008-8846(03)00125-X ↗
46. Costa DG, Rocha AB, Souza WF, Chiaro SSX, Leitão AA (2012) Comparative structural, thermodynamic and electronic analyses of ZnAlAn− hydrotalcite-like compounds (An− Cl−, F−, Br−, OH−, CO3 2− or NO3 −): an ab initio study. Appl Clay Sci 56:16–2210.1016/j.clay.2011.11.014 ↗
47. Chen Y, Shui Z, Chen W, Chen G (2015) Chloride binding of synthetic Ca–Al–NO3 LDHs in hardened cement paste. Constr Build Mater 93:1051–105810.1016/j.conbuildmat.2015.05.047 ↗
48. Chen-Tan NW, van Riessen A, Ly CV, Southam DC (2009) Determining the reactivity of a fly ash for production of geopolymer. J Am Ceram Soc 92(4):881–88710.1111/j.1551-2916.2009.02948.x ↗
49. Puertas F, Martínez-Ramírez S, Alonso S, Vázquez T (2000) Alkali-activated fly ash/slag cements: strength behaviour and hydration products. Cem Concr Res 30(10):1625–163210.1016/S0008-8846(00)00298-2 ↗
50. Oh JE, Monteiro PJM, Jun SS, Choi S, Clark SM (2010) The evolution of strength and crystalline phases for alkali-activated ground blast furnace slag and fly ash-based geopolymers. Cem Concr Res 40(2):189–19610.1016/j.cemconres.2009.10.010 ↗
51. Torres-Carrasco M, Palomo JG, Puertas F, Puertas F (2014) Sodium silicate solutions from dissolution of glasswastes. Statistical analysis. Mater Constr 64(314):e01410.3989/mc.2014.05213 ↗
52. Li N, Farzadnia N, Shi C (2017) Microstructural changes in alkali-activated slag mortars induced by accelerated carbonation. Cem Concr Res 100:214–22610.1016/j.cemconres.2017.07.008 ↗