Control of cracking in full-scaled columns made of ultra-high-strength concrete
Source abstract
Abstract
Experiments have shown that autogenous shrinkage and elevated temperature due to hydration in reinforced concrete members composed of ultra-high-strength concrete, such as concrete that has a design strength of over 120 MPa cause surface cracks, internal cracks, and cracks around rebar. Since ultra-high-strength concrete is generally used in Japan as cast-in-place concrete or precast concrete, the mitigation of these cracks is a crucial issue because the concrete is expected to have high durability. In the present study, expansive additive, shrinkage reducing agent, combined use of expansive additive and shrinkage reducing agent, thermal insulation to control temperature differences within a member, and combined use of thermal insulation and expansive additive were evaluated by placing full-scale columns and cutting out specimens in order to observe the crack patterns in the columns. Ways to mitigate the cracks were found and characterized. Although thermal insulation generally suppressed surface cracks, the peak temperature increased and consequently so did the risk of internal cracks due to the higher peak temperature and the resultant increase in autogenous shrinkage. Partial replacement of binder with expansive additive reduced cracks around rebar and surface cracks, but the soundness of the bond increased the risk of internal cracks. Addition of shrinkage reducing agent reduced surface cracks and internal cracks. Combined use of expansive additive and shrinkage reducing agent appeared to give a combination of these advantages. The best way to mitigate cracking was combined use of thermal insulation and expansive additive. This method reduced all types of cracks.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete Properties and Behavior · Innovative concrete reinforcement materials · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Collins MP, Mitchell D, MacGregor JG (1993) Structural design considerations for high-strength concrete. Concr Int 15:27–34
2. Folliard KJ, Berke NS (1997) Properties of high-performance concrete containing shrinkage-reducing additive. Cem Concr Res 27:1357–136410.1016/S0008-8846(97)00135-X ↗
3. Gajda J, Vangeem M (2002) Controlling temperatures in mass concrete. Concr Int 24:59–62
4. Goto Y (1971) Cracks formed in concrete around deformed tension bars. ACI J 68:244–251
5. Hori A, Morioka M, Sakai E, Daimon M (1999) Influence of expansive additives on autogenous shrinkage. In: Tazawa E (ed) Autogenous shrinkage of concrete. E&FN Spon, London, pp 93–104
6. Ito H, Maruyama I, Tanimura M, Sato R (2004) Early age deformation and resultant induced stress in expansive high strength concrete. J Adv Concr Technol 2(2):155–17410.3151/jact.2.155 ↗
7. Japan Concrete Institute (1999) Terminology. In: Tazawa E (ed) Autogenous shrinkage of concrete. E&FN Spon, London
8. Jensen OM, Hansen PF (1996) Autogenous deformation and change of the relative humidity in silica fume-modified cement paste. ACI Mater J 93(6):539–543
9. Kovler K, Jensen OM (2005) Novel techniques for concrete curing. Concr Int 27:39–42
10. Maltese C, Pistolesi C, Lolli A, Bravo A, Cerulli T, Salvioni D (2005) Combined effect of expansive and shrinkage reducing admixtures to obtain stable and durable mortars. Cem Concr Res 35:2244–225510.1016/j.cemconres.2004.11.021 ↗
11. Maruyama I, Kameta S, Suzuki M, Sato R (2006) Cracking of high strength concrete around deformed reinforcing bar due to shrinkage. In: Kovler K (ed) International RILEM-JCI seminar on concrete durability and service life planning. RILEM Publications S.A.R.L., Ein-Bokek, Israel, pp 104–11110.1617/291214390X.012 ↗
12. Maruyama I, Teramoto A (2011) Impact of time-dependant thermal expansion coefficient on the early-age volume change in cement pastes. Cem Concr Res 41:380–39110.1016/j.cemconres.2011.01.003 ↗
13. Maruyama I, Teramoto A (2013) Temperature dependence of autogenous shrinkage of silica fume cement pastes with a very low water-binder ratio. Cem Concr Res 50:41–5010.1016/j.cemconres.2013.03.017 ↗
14. Maruyama I, Suzuki M, Sato R (2013) Stress distribution and crack formation in full-scaled ultra-high strength concrete columns. Mater Struct. doi: 10.1617/s11527-012-9873-710.1617/s11527-012-9873-7 ↗
15. Meddah MS, Suzuki M, Sato R (2011) Influence of a combination of expansive and shrinkage-reducing admixture on autogenous deformation and self-stress of silica fume high-performance concrete. Cem Concr Res 25:239–250
16. Mitani Y, Maehori S, Tanimura M (2013) Reduction of autogenous shrinkage of ultra-high-strength concrete containing silica fume-premix cement. In: Third international conference on sustainable construction materials and technologies-SCMT3, Kyoto, Japan, p e325
17. Ohno T, Uomoto T (2000) Prediction of occurrence of cracks due to autogenous shrinkage and drying shrinkage. Trans Jpn Soc Civ Eng 49(662):29–44
18. Paillere AM, Buil M, Serrano JJ (1989) Effect of fiber addition on the autogenous shrinkage of silica fume concrete. ACI Mater J 86(2):139–144
19. Powers TC (1958) Structure and physical properties of hardened Portland cement paste. J Am Ceram Soc 4(1):1–510.1111/j.1151-2916.1958.tb13494.x ↗
20. Sato R, Tanaka S, Hayakawa T, Tanimura M (1999) Experimental studies on reduction of autogenous shrinkage and its induced stress in high-strength concrete. In: Proceedings of the second international research seminar on self-desiccation and its importance in concrete technology, Lund, Sweden, pp 163–171
21. Sellevold EJ, Bjøntegaad Ø (2006) Coefficient of thermal expansion of cement paste and concrete: mechanisms of moisture interaction. Mater Struct 39:809–81510.1617/s11527-006-9086-z ↗
22. Suzuki M, Maruyama I, Nakase H, Sato R (2009) Reduction of self-induced stress and resultant cracks in reinforced ultra high-strength concrete column by dosage of expansive additive and shrinkage reducing agent. J Struct Constr Eng 635:1–10 (in Japanese)10.3130/aijs.74.1 ↗
23. Suzuki M, Meddah MS, Sato R (2009) Use of porous ceramic waste aggregates for internal curing of high-performance concrete. Cem Concr Res 39:373–38110.1016/j.cemconres.2009.01.007 ↗
24. Tanimura M, Hyodo H, Nakamura H, Sato R (2002) Effectiveness of expansive additive on reduction of autogenous shrinkage stress in high-strength concrete. In: Proceedings of the third international research seminar on self-desiccation and its importance in concrete technology, Lund, Sweden, pp 205–216
25. Tanimura M, Kwak D, Fujita H, Mitani Y, Hyodo H (2009) Applicability of expansive additive on reducing shrinkage in ultra-high-strength concrete. In: 4th international conference on construction materials: performance, innovation and structural implications, Nagoya, Japan, pp 485–490
26. Tazawa E, Miyazawa S (1992) Autogenous shrinkage of cement paste with condensed silica fume. In: Fourth CANMET/ACI international conference on fly ash, silica fume, slag, and natural pozzolans in concrete, Istanbul, Turkey, pp 875–894
27. Tazawa E, Miyazawa S (1995) Influence of cement and admixture on autogenous shrinkage of cement paste. Cem Concr Res 25(2):281–28710.1016/0008-8846(95)00010-0 ↗
28. Tazawa E, Miyazawa S (1997) Influence of constituent and composition on autogenous shrinkage of cementitious materials. Mag Concr Res 49:15–2210.1680/macr.1997.49.178.15 ↗
29. Weber S, Reinhardt HW (1997) A new generation of high performance concrete: concrete with autogenous curing. Adv Cem Based Mater 6(2):59–6810.1016/S1065-7355(97)00009-6 ↗
30. Wyrzykowski M, Lura P (2013) Moisture dependence of thermal expansion in cement-based materials at early ages. Cem Concr Res 53:25–3510.1016/j.cemconres.2013.05.016 ↗