journal article·2020-05-03Open access

Review of Growth Defects in Thin Films Prepared by PVD Techniques

Peter Panjan, Aljaž Drnovšek, Peter Gselman, Miha Čekada, Matjaž Panjan

Coatings· Volume 10· Issue 5

Abstract

The paper summarizes current knowledge of growth defects in physical vapor deposition (PVD) coatings. A detailed historical overview is followed by a description of the types and evolution of growth defects. Growth defects are microscopic imperfections in the coating microstructure. They are most commonly formed by overgrowing of the topographical imperfections (pits, asperities) on the substrate surface or the foreign particles of different origins (dust, debris, flakes). Such foreign particles are not only those that remain on the substrate surface after wet cleaning procedure, but also the ones that are generated during ion etching and deposition processes. Although the origin of seed particles from external pretreatment of substrate is similar to all PVD coatings, the influence of ion etching and deposition techniques is rather different. Therefore, special emphasis is given on the description of the processes that take place during ion etching of substrates and the deposition of coating. The effect of growth defects on the functional properties of PVD coatings is described in the last section. How defects affect the quality of optical coatings, thin layers for semiconductor devices, as well as wear, corrosion, and oxidation resistant coatings is explained. The effect of growth defects on the permeation and wettability of the coatings is also shortly described.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Semiconductor materials and devices · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Jožef Stefan Institute, Jamova 39, 1000 Ljubljana, Slovenia

Interkorn d.o.o, Gančani 94, 9231 Beltinci, Slovenia

Funding

Javna Agencija za Raziskovalno Dejavnost RS

References (99)

Show source-provided references
1. Interrelationships between process parameters, structure, and properties of CVD tungsten and tungsten–rhenium alloys10.1116/1.1312739 ↗
2. Growth of nodular defects during film deposition10.1063/1.359958 ↗
3. Nodular defects growth and structure in vapor deposited Films10.1007/BF02652964 ↗
4. Dendritic Growth During Electrodeposition
5. Ultrasmooth plasma polymerized coatings for laser fusion targets10.1116/1.571142 ↗
6. Investigation of the structure and properties of thick vacuum condensates of nickel, titanium, tungsten and aluminum oxide
7. Structure modification by ion bombardment during deposition10.1116/1.1316677 ↗
8. The influence of surface topography and angle of adatom incidence on growth structure in sputtered chromium10.1016/0040-6090(79)90112-3 ↗
9. Characterization of defect growth structrures in ion-plated films by scanning electron microscopy10.1016/0040-6090(79)90553-4 ↗
10. Nodular growth in thick-sputtered metallic coatings10.1116/1.1318706 ↗
11. Nodular defects in dielectric multilayers and thick single layers10.1364/AO.20.001034 ↗
12. Characterization of defect geometries in multilayer optical coatings10.1116/1.578948 ↗
13. Modeling of nodular defects in thin films for various deposition techniques10.1117/12.941849 ↗
14. Columnar microstructure in vapor-deposited thin films10.1016/0040-6090(77)90037-2 ↗
15. Thin film microstructure modelling10.1117/12.976106 ↗
16. Computer simulation of hillock growth10.1016/0042-207X(91)90090-6 ↗
17. Localized defects in multilayer coating10.1016/S0040-6090(03)01285-9 ↗
18. The role of defects in laser damage of multilayer coatings10.1117/12.180876 ↗
19. The advantages of evaporation of Hafnium in a reactive environment to manufacture high damage threshold multilayer coatings by electron-beam deposition10.1117/12.360095 ↗
20. Laser damage study of nodules in electron-beam evaporated HfO2/SiO2 high reflectors10.1364/AO.50.00C357 ↗
21. Characteristics of nodular defect in HfO2/SiO2 multilayer optical coatings10.1364/AO.49.001774 ↗
22. SEM study of defects in PVD hard coatings using focused ion beam milling10.1016/j.surfcoat.2007.09.033 ↗
23. Nodular defect growth in thin films10.1007/BF00701096 ↗
24. New approach for the critical size of the nodular defects: The mechanical connection10.1117/12.344397 ↗
25. Influence of composition and seed dimension on the structure and laser damage of nodular defects in HfO2/SiO2 high reflectors10.1364/AO.51.006781 ↗
26. Investigating the growth of localized defects in thin films using gold nanospheres10.1063/1.1314291 ↗
27. Defect-related properties of optical coatings10.1515/aot-2013-0063 ↗
28. In Situ Plasma Contamination Measurements by HeNe Laser Light Scattering: A Case Study10.1116/1.576838 ↗
29. Observation and evaluation of flaked particle behavior in magnetically enhanced reactive ion etching equipment using a dipole ring magnet10.1116/1.1763592 ↗
30. Corrosion of thin hard PVD coatings10.1016/0042-207X(94)90015-9 ↗
31. Corrosion protection with hard coatings on steel: Past approaches and current research efforts10.1016/j.surfcoat.2014.08.069 ↗
32. Identification of the growth defects responsible for pitting corrosion on sputter-coated steel samples by Large Area High Resolution mapping10.1016/j.tsf.2014.12.014 ↗
33. Corrosion protection of steel substrates by magnetron sputtered TiMgN hard coatings: Structure, mechanical properties and growth defect related salt spray test results10.1016/j.surfcoat.2018.05.037 ↗
34. The corrosion behaviour of macroparticle defects in arc bond-sputtered CrN/NbN superlattice coatings10.1016/S0257-8972(00)00554-5 ↗
35. Improvement of the corrosion resistance of PVD hard coating–substrate systems10.1016/S0257-8972(99)00551-4 ↗
36. Localized corrosion mechanisms of the multilayered coatings related to growth defects10.1016/S0257-8972(03)00939-3 ↗
37. Accelerated thermal degradation of DLC-coatings via growth defects10.1016/j.surfcoat.2018.05.063 ↗
38. Oxygen diffusion barrier properties of transparent oxide coatings on polymeric substrates10.1016/0257-8972(95)02420-4 ↗
39. Origin of friction in running-in sliding wear of nitride coatings10.1007/s11249-009-9548-x ↗
40. The influence of surface defects on the mechanical and tribological properties of VN-based arc-evaporated coatings10.1016/j.wear.2012.11.012 ↗
41. The effect of droplets in arc evaporated TiAlTaN hard coatings on the wear behavior10.1016/j.surfcoat.2014.01.010 ↗
42. The influence of growth defects in sputter-deposited TiAlN hard coatings on their tribological behavior10.1016/j.surfcoat.2016.01.021 ↗
43. Tribological aspects related to the morphology of PVD hard coatings10.1016/j.surfcoat.2017.09.084 ↗
44. (2018). Grinding of Uddeholm Tool Steels, [8th ed.]. Available online: https://www.uddeholm.com/app/uploads/sites/44/2018/11/Tech-Uddeholm-Grinding-EN.pdf.
45. (2016). Polishing of Uddeholm Mould Steel, [6th ed.]. Available online: https://www.uddeholm.com/app/uploads/sites/45/2018/02/Uddeholm_polishing-eng_t_1609_e6.pdf.
46. Panjan, P., Drnovšek, A., Gselman, P., Čekada, M., Panjan, M., Boncina, T., and Merl, D.K. (2019). Influence of Growth Defects on the Corrosion Resistance of Sputter-Deposited TiAlN Hard Coatings. Coatings, 9.10.3390/coatings9080511 ↗
47. Mattox, D.M. (2010). Handbook of Physical Vapor Deposition (PVD) Processing, Elsevier.10.1016/B978-0-8155-2037-5.00008-3 ↗
48. Six strategies to produce application tailored nanoscale multilayer structured PVD coatings by conventional and High Power Impulse Magnetron Sputtering (HIPIMS)10.1016/j.tsf.2019.137409 ↗
49. Growth characteristics of multilayered physical vapour deposited TiNTaN on high speed steel substrate10.1016/S0040-6090(00)01880-0 ↗
50. Formation of nodular defects as revealed by simulation of a modified ballistic model of depositional growth10.1023/A:1004399725862 ↗
51. Ion-assisted growth of Ti1−xAlxN/Ti1−yNbyN multilayers by combined cathodic-arc/magnetron-sputter deposition10.1016/S0040-6090(96)09524-7 ↗
52. The role of the growth defects on the corrosion resistance of CrN/NbN superlattice coatings deposited at low temperatures10.1016/j.tsf.2005.08.375 ↗
53. Mattox, D.M. (2009). Atomistic Film Growth and Resulting Film Properties. SVC Bull. Spring, 30–31.
54. Reid, F.H., and Goldie, W. (1974). Measurement of Porosity. Gold Plating Technology, Electrochemical Publications Ltd.
55. Growth defect density in PVD hard coatings prepared by different deposition techniques10.1016/j.surfcoat.2013.09.020 ↗
56. Sarkar, J. (2014). Troubleshooting in Sputter Deposition. Sputtering Materials for VLSI and Thin Film Devices, Elsevier. [2nd ed.].10.1016/B978-0-8155-1593-7.00008-4 ↗
57. In situ laser diagnostic studies of plasma-generated particulate contamination10.1116/1.576175 ↗
58. Cone formation on metal targets during sputtering10.1063/1.1660158 ↗
59. Nodule formation on sputtering targets: Causes and their control by MF power supplies10.1016/j.surfcoat.2017.09.009 ↗
60. Particle contamination formation in magnetron sputtering processes10.1116/1.580674 ↗
61. In-situ analysis of particle contamination in magnetron sputtering10.1016/S0040-6090(97)00603-2 ↗
62. Physics of arcing, and implications to sputter deposition10.1016/j.tsf.2005.07.228 ↗
63. Correlation between aluminium alloy sputtering target metalurgical characteristics, arc initiation, and in-film defect intensity
64. Materials processing using radio-frequency ion-sources: Ion-beam sputter-deposition and surface treatment10.1063/1.5063976 ↗
65. Factors affecting growth defect formation in cathodic arc evaporated coatings10.1016/0257-8972(95)02773-4 ↗
66. A Formation Mechanism for the Macroparticles in Arc Ion-Plated TiN Films10.1016/S0040-6090(00)01918-0 ↗
67. Defects in TiN and TiAIN coatings grown by combined cathodic arc/unbalanced magnetron technology10.1016/0042-207X(94)E0029-X ↗
68. Improvement of structure and quality of nanoscale multilayered composite coatings, deposited by filtered cathodic vacuum arc deposition method10.1177/1847980416680805 ↗
69. Effect of cathode composition and nitrogen pressure on macroparticle generation and type of arc discharge in a DC arc source with Ti–Al compound cathodes10.1016/j.surfcoat.2015.09.030 ↗
70. What is laser conditioning? A review focused on dielectric multilayers10.1117/12.344463 ↗
71. Mirkarimi, B., Baker, S.L., and Stearns, D.G. (2005). Planarization of Substrate Pits and Scratches. (2005/0118533A1), U.S. Patent.
72. Developing a viable multilayer coating process for extreme ultraviolet lithography reticles
73. Growth defects in carbon coatings deposited by magnetron sputtering10.1016/S0257-8972(03)00010-0 ↗
74. Influence of CVD and PVD coating micro topography on the initial material transfer of 316L stainless steel in sliding contacts—A laboratory study10.1016/j.wear.2016.12.003 ↗
75. Influence of surface roughness and coating type on the galling properties of coated forming tool steel10.1016/j.surfcoat.2003.11.002 ↗
76. Design and evaluation of tribological coatings10.1016/S0043-1648(00)00505-6 ↗
77. Holmberg, K., and Matthews, A. (2009). Coating Tribology, Elsevier. [2nd ed.].
78. Influence of surface topography of arc-deposited TiN and sputter-deposited WC/C coatings on the initial material transfer tendency and friction characteristics under dry sliding contact conditions10.1016/j.surfcoat.2008.12.011 ↗
79. On the influence from micro topography of PVD coatings on friction behaviour, material transfer and tribofilm formation10.1016/j.wear.2010.12.036 ↗
80. Surface topography effect on galling resistance of coated and uncoated tool steel10.1016/j.surfcoat.2011.11.041 ↗
81. The influence of surrounding atmosphere on tribological properties of hard protective coating10.1016/j.surfcoat.2014.11.068 ↗
82. Wear associated with growth defects in combined cathodic arcrunbalanced magnetron sputtered CrNrNbN superlattice coatings during erosion in alkaline slurry10.1016/S0257-8972(00)00913-0 ↗
83. The role of droplets on the cavitation erosion damage of TiN coatings produced with cathodic arc physical vapor deposition10.1016/j.surfcoat.2017.05.050 ↗
84. An approach to evaluate the resistance of hard coatings to shock loading10.1016/j.surfcoat.2010.10.033 ↗
85. Effect of chamber pressure on defect generation and their influence on corrosion and tribological properties of HIPIMS deposited CrN/NbN coatings10.1016/j.surfcoat.2017.08.021 ↗
86. The role of surface defects density on corrosion resistance of PVD hard coatings10.1002/ppap.200731416 ↗
87. Tribological and corrosion behavior of CrN coatings: Roles of substrate and deposition defects10.1016/j.surfcoat.2014.07.063 ↗
88. Oxidation of metastable single-phase polycrystalline Ti0.5Al0.5N films: Kinetics and mechanisms10.1063/1.345664 ↗
89. Localised oxidation defects in TiAlN/CrN superlattice structured hard coatings grown by cathodic arc/unbalanced magnetron deposition on various substrate materials10.1016/S0257-8972(99)00571-X ↗
90. High temperature behavior of nanolayered CrAlTiN coating: Thermal stability, oxidation, and tribological properties10.1016/j.surfcoat.2014.07.053 ↗
91. Performance of HIPIMS deposited CrN/NbN nanostructured coatings exposed to 650 C in pure steam environment10.1016/j.matchemphys.2016.05.017 ↗
92. Oxidation and diffusion processes during annealing of TiSi(V)N films10.1016/j.surfcoat.2015.05.031 ↗
93. Oxidation resistance of CrN/(Cr,V)N hard coatings deposited by DC magnetron sputtering10.1016/j.tsf.2015.05.010 ↗
94. Food Packaging Permeability behaviour10.1155/2012/302029 ↗
95. The Role of Defects in Single- and Multi-Layer Barriers for Flexible Electronics
96. Ultra barrier flexibe substrates for flat panel displays10.1016/S0141-9382(00)00064-0 ↗
97. Permeation barrier properties of thin oxide films on flexible polymer substrates10.1016/j.tsf.2008.11.089 ↗
98. Characterization of reactively sputtered permeation barrier materials on polymer substrates10.1016/j.surfcoat.2011.01.045 ↗
99. A combined experimental and theoretical study on the side ingress of water into barrier adhesives for organic electronics