Abstract

PURPOSE: To investigate the surface roughness (Ra), shear bond strength (SBS), and Vickers hardness number (VHN) of additive manufactured interim resins manufactured through different vat polymerization techniques. METHODS: Samples were divided into four groups; additive manufacturing technology (Stereolithography:S-FL; Digital light processing:D-AS; Liquid crystal display:L-PH) and subtractive manufacturing technology (Polymethylmethacrylate: MP) (n = 10). After polishing, the Ra values were measured and resin material was then applied. Following thermocycling, SBS tests and VHN tests were carried out. The obtained data were evaluated using one-way analysis of variance (ANOVA) (a = 0.05). RESULTS: Significant differences were observed between the groups for SBS (P = 0.02) and VHN (P < 0.001), whereas the Ra values were not statistically significant (P = 0.148). D-AS and L-PH had higher and similar SBS (P = 1.000) while MP had statistically lower SBS. D-AS demonstrated higher VHN than all groups (P < 0.001) with the exception of S-FL (P = 0.831). MP had lower VHN than all groups (P < 0.01) other than L-PH (P = 0.143). CONCLUSION: All fabrication methods had clinically acceptable SBS values, L-PH and D-AS had higher results. D-AS demonstrated superiority in terms of VHN, all groups exhibited comparable Ra values.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Anatomy and Medical Technology · Orthodontics and Dentofacial Orthopedics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Prosthodontics, Biruni University, Faculty of Dentistry

Funding

Research Fund of the Biruni University Research and Development Coordination Office Directorate

References (34)

Show source-provided references
1. 1. Kim D, Shim JS, Lee D, Shin SH, Nam NE, Park KH et al. (2020) Effects of post-curing time on the mechanical and color properties of three-dimensional printed crown and bridge materials. Polymers 12, 2762. doi: 10.3390/polym1211276210.3390/polym12112762 ↗
2. 2. Diken Turksayar AA, Donmez MB, Olcay EO, Demirel M, Demir E (2022) Effect of printing orientation on the fracture strength of additively manufactured 3-unit interim fixed dental prostheses after aging. J Dent 124, 104155. doi: 10.1016/j.jdent.2022.10415510.1016/j.jdent.2022.104155 ↗
3. 3. Alammar A, Kois JC, Revilla‐León M, Att W (2022) Additive manufacturing technologies: current status and future perspectives. J Prosthodont 31, 4-12. doi: 10.1111/jopr.1347710.1111/jopr.13477 ↗
4. 4. Piedra-Cascón W, Krishnamurthy VR, Att W, Revilla-León M (2021) 3D printing parameters, supporting structures, slicing, and post-processing procedures of vat-polymerization additive manufacturing technologies: a narrative review. J Dent 109, 103630. doi: 10.1016/j.jdent.2021.10363010.1016/j.jdent.2021.103630 ↗
5. 5. Quan H, Zhang T, Xu H, Luo S, Nie J, Zhu X (2020) Photo-curing 3D printing technique and its challenges. Bioact Mater 5, 110-115. doi: 10.1016/j.bioactmat.2019.12.00310.1016/j.bioactmat.2019.12.003 ↗
6. 6. Schweiger J, Edelhoff D, Güth JF (2021) 3D printing in digital prosthetic dentistry: an overview of recent developments in additive manufacturing. J Clin Med 10, 2010. doi: 10.3390/jcm1009201010.3390/jcm10092010 ↗
7. 7. Lee HE, Alauddin MS, Mohd Ghazali MI, Said Z, Mohamad Zol S (2023) Effect of different vat polymerization techniques on mechanical and biological properties of 3D-printed denture base. Polymers 15, 1463.8. doi: 10.3390/polym1506146310.3390/polym15061463 ↗
8. 8. Ellakany P, Fouda SM, Mahrous AA, AlGhamdi MA, Aly NM (2022) Influence of CAD/CAM milling and 3D-printing fabrication methods on the mechanical properties of 3-unit interim fixed dental prosthesis after thermo-mechanical aging process. Polymers 14, 4103. doi: 10.3390/polym1419410310.3390/polym14194103 ↗
9. 9. Zhang J, Hu Q, Wang S, Tao J, Gou M (2019) Digital light processing based three-dimensional printing for medical applications. Int J Bioprinting 6, 242. doi: 10.18063/ijb.v6i1.24210.18063/ijb.v6i1.242 ↗
10. 10. Mai HN, Lee KB, Lee DH (2017) Fit of interim crowns fabricated using photopolymer-jetting 3D printing. J Prosthet Dent 118, 208-215. doi: 10.1016/j.prosdent.2016.10.03010.1016/j.prosdent.2016.10.030 ↗
11. 11. Abdullah AO, Pollington S, Liu Y (2018) Comparison between direct chairside and digitally fabricated temporary crowns. Dent Mater J 37, 957-963. doi: 10.4012/dmj.2017-31510.4012/dmj.2017-315 ↗
12. 12. Alageel O, Alhijji S, Alsadon O, Alsarani M, Gomawi AA, Alhotan A (2023) Trueness, flexural strength, and surface properties of various three-dimensional (3D) printed interim restorative materials after accelerated aging. Polymers 15, 3040. doi: 10.3390/polym1514304010.3390/polym15143040 ↗
13. 13. de Souza FA, Blois MC, Collares K, Dos Santos MBF (2024) 3D-printed and conventional provisional single crown fabrication on anterior implants: a randomized clinical trial. Dent Mater 40, 340-347. doi: 10.1016/j.dental.2023.12.00410.1016/j.dental.2023.12.004 ↗
14. 14. Pituru SM, Greabu M, Totan A, Imre M, Pantea M, Spinu T et al. (2020) A review on the biocompatibility of PMMA-based dental materials for interim prosthetic restorations with a glimpse into their modern manufacturing techniques. Materials 13, 2894. doi: 10.3390/ma1313289410.3390/ma13132894 ↗
15. 15. Sampaio CS, Niemann KD, Schweitzer DD, Hirata R, Atria PJ (2021) Microcomputed tomography evaluation of cement film thickness of veneers and crowns made with conventional and 3D printed provisional materials. J Esthet Restor Dent 33, 487-495. doi: 10.1111/jerd.1265110.1111/jerd.12651 ↗
16. 16. Lankes V, Reymus M, Liebermann A, Stawarczyk B (2023) Bond strength between temporary 3D printable resin and conventional resin composite: influence of cleaning methods and air-abrasion parameters. Clin Oral Investig 27, 31-43. doi: 10.1007/s00784-022-04800-710.1007/s00784-022-04800-7 ↗
17. 17. Dewan H, Sayed ME, Jundus A, Gharawi M, Baeshen S, Alali M et al. (2023) Shear strength of repaired 3D-printed and milled provisional materials using different resin materials with and without chemical and mechanical surface treatment. Polymers 15, 4284. doi: 10.3390/polym1521428410.3390/polym15214284 ↗
18. 18. Lad PP, Kamath M, Tarale K, Kusugal PB (2014) Practical clinical considerations of luting cements: a review. J Int Oral Health 6, 116-120.
19. 19. Albahri R, Yoon HI, Lee JD, Yoon S, Lee SJ (2021) Shear bond strength of provisional repair materials bonded to 3D printed resin. J Dent Sci 16, 261-267. doi: 10.1016/j.jds.2020.05.00310.1016/j.jds.2020.05.003 ↗
20. 20. Holmer L, Othman A, Lührs AK, von See C (2019) Comparison of the shear bond strength of 3D printed temporary bridges materials, on different types of resin cements and surface treatment. J Clin Exp Dent 11, e367-e372. doi: 10.4317/jced.5561710.4317/jced.55617 ↗
21. 21. Su N, Yue L, Liao Y, Liu W, Zhang H, Li X et al. (2015) The effect of various sandblasting conditions on surface changes of dental zirconia and shear bond strength between zirconia core and indirect composite resin. J Adv Prosthodont 7, 214-223. doi: 10.4047/jap.2015.7.3.21410.4047/jap.2015.7.3.214 ↗
22. 22. Zhou L, Qian Y, Zhu Y, Liu H, Gan K, Guo J (2014) The effect of different surface treatments on the bond strength of PEEK composite materials. Dent Mater 30, e209-e215 doi: 10.1016/j.dental.2014.03.01110.1016/j.dental.2014.03.011 ↗
23. 23. Alp G, Johnston WM, Yilmaz B (2019) Optical properties and surface roughness of prepolymerized poly (methyl methacrylate) denture base materials. J Prosthet Dent 121, 347-352. doi: 10.1016/j.prosdent.2018.03.00110.1016/j.prosdent.2018.03.001 ↗
24. 24. de Castro EF, Nima G, Rueggeberg FA, Araújo-Neto VG, Faraoni JJ, Palma-Dibb et al. (2023) Effect of build orientation in gloss, roughness and color of 3D-printed resins for provisional indirect restorations. Dent Mater 39, e1-e11. doi: 10.1016/j.dental.2023.05.00210.1016/j.dental.2023.05.002 ↗
25. 25. Wadhwani V, Sivaswamy V, Rajaraman V (2022) Surface roughness and marginal adaptation of stereolithography versus digital light processing threedimensional printed resins: An: in-vitro: study. J Indian Prosthodont Soc 22, 377-381. doi: 10.4103/jips.jips_8_2210.4103/jips.jips_8_22 ↗
26. 26. International Organization for Standardization (2020) Dentistry--Polymer-based crown and bridge materials. ISO 10477:2020, Geneve.
27. 27. Ersöz B, Aydın N, Ezmek B, Karaoglanoğlu S, Çal IK (2024) Effect of surface treatments applied to 3D printed permanent resins on shear bond strength. J Clin Exp Dent 16, e1059-e1066. doi: 10.4317/jced.6188410.4317/jced.61884 ↗
28. 28. Khanlar LN, Revilla-León M, Barmak AB, Ikeda M, Alsandi Q, Tagami J et al. (2023) Surface roughness and shear bond strength to composite resin of additively manufactured interim restorative material with different printing orientations. J Prosthet Dent 129, 788-795. doi: 10.1016/j.prosdent.2021.08.01010.1016/j.prosdent.2021.08.010 ↗
29. 29. Reymus M, Lümkemann N, Stawarczyk B (2019) 3D-printed material for temporaryrestorations: impact of print layer thickness and post-curing method on degree of conversion. Int J Comput Dent 22, 231-237. doi: 10.1007/s00784-019-02952-710.1007/s00784-019-02952-7 ↗
30. 30. Al-Qahtani AS, Tulbah HI, Binhasan M, Abbasi MS, Ahmed N, Shabib S et al. (2021) Surface properties of polymer resins fabricated with subtractive and additive manufacturing techniques. Polymers 13, 4077. doi: 10.3390/polym1323407710.3390/polym13234077 ↗
31. 31. Alshamrani AA, Raju R, Ellakwa A (2022). Effect of printing layer thickness and postprinting conditions on the flexural strength and hardness of a 3D-printed resin. Biomed Res Int 2022, 8353137. doi:10.1155/2022/835313710.1155/2022/8353137 ↗
32. 32. Katheng A, Prawatvatchara W, Chaiamornsup P, Sornsuwan T, Lekatana H, Palasuk J (2025) Comparison of mechanical properties of different 3D printing technologies. Sci Rep 15, 18998. doi: 10.1038/s41598-025-03632-110.1038/s41598-025-03632-1 ↗
33. 33. Tsolakis IA, Papaioannou W, Papadopoulou E, Dalampira M, Tsolakis AI (2022) Comparison in terms of accuracy between DLP and LCD printing technology for dental model printing. Dent J 10, 181. doi: 10.3390/dj1010018110.3390/dj10100181 ↗
34. 34. Sağlam G, Cengiz S, Köroğlu A, Şahin O, Velioğlu N (2023). Comparison of the micro-shear bond strength of resin cements to CAD/CAM glass ceramics with various surface treatments. Materials (Basel) 16, 2635. doi: 10.3390/ma1607263510.3390/ma16072635 ↗