Abstract

PURPOSE: High-viscosity glass ionomer cements (HV-GICs) are reinforced with ultrafine, highly reactive glass particles, as well as a higher-molecular-weight polyalkenoic acid component. Silver diammine fluoride (SDF) is an agent with promising activity against active caries. The present study aimed to evaluate the shear bond strength (SBS) and interfacial morphology of a new HV-GIC bonded to dentin after treatment with various adhesive protocols including SDF. METHODS: HV-GIC cylinders were bonded to dentin after various surface treatments (6 groups, n = 22): water; polyalkenoic acid; SDF; SDF + potassium iodide (KI); SDF + KI + polyalkenoic acid; SDF + KI + two weeks of storage in water + polyalkenoic acid. For each group, 20 samples were tested for SBS after 48 h, and 2 samples were cut and subjected to environmental scanning electron microscopy (E-SEM) and energy-dispersive X-ray (EDX) analysis. RESULTS: No significant differences in SBS were found between any of the protocols tested. However, E-SEM and EDX images showed different interfaces when SDF was applied. CONCLUSION: SDF has no influence on the adhesion of HV-GIC to sound dentin and could potentially improve the cario-resistance of the dentin/HV-GIC interface.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Health and Care Utilization · Dental Erosion and Treatment

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Innovative Dental Materials and Interfaces Research Unit (URB2i, UR 4462), University of Paris

Department of Restorative Dentistry, Bretonneau Hospital (AP-HP)

Dental School, University of Manchester

CentraleSupélec, Paris-Saclay University

Department of Restorative Dentistry, Charles Foix Hospital (AP-HP)

Department of Pediatric Dentistry, Henri Mondor Hospital (AP-HP)

References (39)

Show source-provided references
1. 1. Wilson AD, Kent BE (1971) The glass-ionomer cement, a new translucent dental filling material. J Chem Technol Biotechnol 21, 313.
2. 2. Tay FR, Smales RJ, Ngo H, Wei SH, Pashley DH (2001) Effect of different conditioning protocols on adhesion of a GIC to dentin. J Adhes Dent 3, 153-167.
3. 3. Bahsi E, Sagmak S, Dayi B, Cellik O, Akkus Z (2019) The evaluation of microleakage and fluoride release of different types of glass ionomer cements. Niger J Clin Pract 22, 961-970.10.4103/njcp.njcp_644_18 ↗
4. 4. Sidhu SK (2011) Glass-ionomer cement restorative materials: a sticky subject? Aust Dent J 56, 23-30.10.1111/j.1834-7819.2010.01293.x ↗
5. 5. Hayacibara MF, Rosa OPS, Koo H, Torres SA, Costa B, Cury JA (2003) Effects of fluoride and aluminum from ionomeric materials on S. mutans biofilm. J Dent Res 82, 267-271.10.1177/154405910308200405 ↗
6. 6. Krämer N, Schmidt M, Lücker S, Domann E, Frankenberger R (2018) Glass ionomer cement inhibits secondary caries in an in vitro biofilm model. Clin Oral Investig 22, 1019-1031.10.1007/s00784-017-2184-1 ↗
7. 7. Yoshihara K, Nagaoka N, Maruo Y, Sano H, Yoshida Y, Van Meerbeek B (2017) Bacterial adhesion not inhibited by ion-releasing bioactive glass filler. Dent Mater 33, 723-734.10.1016/j.dental.2017.04.002 ↗
8. 8. Lagarde M, Francois P, Goff SL, Attal J-P, Dursun E (2018) Structural and long-term mechanical properties from a resin-modified glass ionomer cement after various delays of light-activation Dent Mater J 37, 874-879.10.4012/dmj.2017-342 ↗
9. 9. Dermata A, Papageorgiou SN, Fragkou S, Kotsanos N (2018) Comparison of resin modified glass ionomer cement and composite resin in class II primary molar restorations: a 2-year parallel randomized clinical trial Eur Arch Paediatr Dent 19, 393-401.10.1007/s40368-018-0371-7 ↗
10. 10. Cattani-Lorente MA, Dupuis V, Payan J, Moya F, Meyer JM (1999) Effect of water on the physical properties of resin-modified glass ionomer cements. Dent Mater 15, 71-78.10.1016/S0109-5641(99)00016-0 ↗
11. 11. Khoroushi M, Keshani F (2013) A review of glass-ionomers: from conventional glass-ionomer to bioactive glass-ionomer. Dent Res J (Isfahan) 10, 411-420.
12. 12. Gurgan S, Kutuk ZB, Ergin E, Oztas SS, Cakir FY (2015) Four-year randomized clinical trial to evaluate the clinical performance of a glass ionomer restorative system. Oper Dent 40, 134-143.10.2341/13-239-C ↗
13. 13. Francois P, Vennat E, Le Goff S, Ruscassier N, Attal J-P, Dursun E (2019) Shear bond strength and interface analysis between a resin composite and a recent high-viscous glass ionomer cement bonded with various adhesive systems Clin Oral Investig 23, 2599-2608.10.1007/s00784-018-2678-5 ↗
14. 14. Craig GG, Knight GM, McIntyre JM (2012) Clinical evaluation of diamine silver fluoride/potassium iodide as a dentine desensitizing agent. A pilot study Aust Dent J 57, 308-311.10.1111/j.1834-7819.2012.01700.x ↗
15. 15. Zhao IS, Gao SS, Hiraishi N, Burrow MF, Duangthip D (2018) Mechanisms of silver diamine fluoride on arresting caries: a literature review Int Dent J 68, 67-76.10.1111/idj.12320 ↗
16. 16. Yu OY, Zhao IS, Mei ML, Lo ECM, Chu CH (2018) Caries-arresting effects of silver diamine fluoride and sodium fluoride on dentine caries lesions J Dent 78, 65-71.10.1016/j.jdent.2018.08.007 ↗
17. 17. Ishiguro T, Mayanagi G, Azumi M, Otani H, Fukushima A, Sasaki K et al (2019) Sodium fluoride and silver diamine fluoride-coated tooth surfaces inhibit bacterial acid production at the bacteria/tooth interface. J Dent 84, 30-35.10.1016/j.jdent.2018.12.017 ↗
18. 18. Seifo N, Cassie H, Radford JR, Innes NPT (2019) Silver diamine fluoride for managing carious lesions: an umbrella review. BMC Oral Health 19, 145-154.10.1186/s12903-019-0830-5 ↗
19. 19. Patel J, Anthonappa RP, King NM (2018) Evaluation of the staining potential of silver diamine fluoride: in vitro. Int J Paediatr Dent, 28, 514-522.10.1111/ipd.12401 ↗
20. 20. Gurgan S, Kutuk ZB, Yalcin Cakir F, Ergin E (2019) A randomized controlled 10 years follow up of a glass ionomer restorative material in class I and class II cavities. J Dent, 94, 108-117.
21. 21. Wadenya R, Mante FK (2007) An in vitro comparison of marginal microleakage of alternative restorative treatment and conventional glass ionomer restorations in extracted permanent molars. Pediatr Dent 29, 303-307.
22. 22. Giray FE, Peker S, Durmus B, Kargül B (2014) Microleakage of new glass ionomer restorative materials in permanent teeth. Eur J Paediatr Dent 15, 122-126.
23. 23. Meral E, Baseren NM (2019) Shear bond strength and microleakage of novel glass-ionomer cements: an in vitro study. Niger J Clin Pract 22, 566-572.10.4103/njcp.njcp_543_18 ↗
24. 24. Knight GM, McIntyre JM, Craig GG, Mulyani, Zilm PS, Gully NJ (2009) Inability to form a biofilm of Streptococcus mutans on silver fluoride- and potassium iodide-treated demineralized dentin. Quintessence Int 40, 155-161.
25. 25. Mei ML, Li QL, Chu CH, Yiu CKY, Lo ECM (2012) The inhibitory effects of silver diamine fluoride at different concentrations on matrix metalloproteinases. Dent Mater 28, 903-908.10.1016/j.dental.2012.04.011 ↗
26. 26. Mei ML, Ito L, Cao Y, Li QL, Lo ECM, Chu CH (2013) Inhibitory effect of silver diamine fluoride on dentine demineralisation and collagen degradation. J Dent 41, 809-817.10.1016/j.jdent.2013.06.009 ↗
27. 27. Crystal YO, Niederman R (2019) Evidence-based dentistry update on silver diamine fluoride. Dent Clin North Am 63, 45-68.10.1016/j.cden.2018.08.011 ↗
28. 28. Mei ML, Zhao IS, Ito L, Lo EC-M, Chu C-H (2016) Prevention of secondary caries by silver diamine fluoride Int Dent J 66, 71-77.10.1111/idj.12207 ↗
29. 29. Zhao IS, Mei ML, Burrow MF, Lo EC-M, Chu C-H (2017) Effect of silver diamine fluoride and potassium iodide treatment on secondary caries prevention and tooth discolouration in cervical glass ionomer cement restoration. Int J Mol Sci 18, 340-351.10.3390/ijms18020340 ↗
30. 30. Knight GM, McIntyre JM, Mulyani (2006) The effect of silver fluoride and potassium iodide on the bond strength of auto cure glass ionomer cement to dentine. Aust Dent J 51, 42-45.10.1111/j.1834-7819.2006.tb00399.x ↗
31. 31. Hoshika S, De Munck J, Sano H, Sidhu SK, Van Meerbeek B (2015) Effect of conditioning and aging on the bond strength and interfacial morphology of glass-ionomer cement bonded to dentin. J Adhes Dent 17, 141-146.
32. 32. Van Duker M, Hayashi J, Chan DC, Tagami J, Sadr A (2019) Effect of silver diamine fluoride and potassium iodide on bonding to demineralized dentin. Am J Dent 32, 143-146.
33. 33. Gupta J, Thomas MS, Radhakrishna M, Srikant N, Ginjupalli K (2019) Effect of silver diamine fluoride-potassium iodide and 2% chlorhexidine gluconate cavity cleansers on the bond strength and microleakage of resin-modified glass ionomer cement J Conserv Dent 2019 22, 201-206.10.4103/JCD.JCD_485_18 ↗
34. 34. Wang L, Sakai VT, Kawai ES, Buzalaf MA, Atta MT (2006) Effect of adhesive systems associated with resin-modified glass ionomer cements. J Oral Rehabil 33, 110-116.10.1111/j.1365-2842.2006.01536.x ↗
35. 35. Cook NB, Feitosa SA, Patel A, Alfawaz Y, Eckert GJ, Bottino MC (2015) Bonding ability of paste-paste glass ionomer systems to tooth structure: in vitro studies. Oper Dent 40, 304-312.10.2341/14-030-L ↗
36. 36. Zhao IS, Chu S, Yu OY, Mei ML, Chu CH, Lo ECM (2019) Effect of silver diamine fluoride and potassium iodide on shear bond strength of glass ionomer cements to caries-affected dentine. Int Dent J 69, 341-347.10.1111/idj.12478 ↗
37. 37. Hendre AD, Taylor GW, Chávez EM, Hyde S (2017) A systematic review of silver diamine fluoride: effectiveness and application in older adults. Gerodontology 34, 411-419.10.1111/ger.12294 ↗
38. 38. Li Y, Liu Y, Psoter WJ, Nguyen OM, Bromage TG, Walters MA et al. (2019) Assessment of the silver penetration and distribution in carious lesions of deciduous teeth treated with silver diamine fluoride. Caries Res 53, 431-440.10.1159/000496210 ↗
39. 39. Willershausen I, Schulte D, Azaripour A, Weyer V, Briseño B, Willershausen B (2015) Penetration potential of a silver diamine fluoride solution on dentin surfaces. An ex vivo study. Clin Lab 61, 1695-1701.10.7754/Clin.Lab.2015.150401 ↗