Prepress-assisted controllable preparation of SiC coating: A novel route to enhanced dynamic oxidation resistance
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Flame retardant materials and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Enhancing oxidation resistance of PCS-derived ceramic coatings on titanium alloys by SiC whiskers10.1016/j.corsci.2024.112670 ↗
2. Dense and hard amorphous SiC coatings via non-reactive DC magnetron sputtering from alloy target: high thermal stability and oxidation resistance10.1016/j.jallcom.2025.180695 ↗
3. Oxidation protective silicon carbide coating for C/SiC composite modified by a chromium silicide–chromium carbide outer layer10.1016/j.msea.2015.07.081 ↗
4. Anomalous high-temperature oxidation behavior of SiC coatings on Cf/SiC composites: degradation mechanisms and microstructural evolution from 1200 °C to 1400 °C10.1016/j.compositesb.2025.112605 ↗
5. Effect of heat treatment on microstructure and oxidation resistance of SiO2-B4C-glass coating on alumina-carbon refractories10.1016/j.ceramint.2024.12.219 ↗
6. Improved oxidation resistance of CVD-SiC coating at 1300 °C by Ti addition10.1016/j.jeurceramsoc.2025.117289 ↗
7. Oxidation protective MoSi2-SiC-Si coating for graphite materials prepared by slurry dipping and vapor silicon infiltration10.1016/j.ceramint.2017.12.122 ↗
8. Microstructure evolution and growth mechanism of core-shell silicon-based nanowires by thermal evaporation of SiO10.1007/s40145-022-0620-4 ↗
9. Si-evaporation-reacted Si-HfB2-CrSi2-SiC ceramic coatings: long-term oxidation behaviors at 900–1600 °C and ablation protection performance at 2300 °C10.1016/j.ceramint.2025.09.094 ↗
10. Oxidative protection of a carbon-bonded carbon fiber composite with double-layer coating of MoSi2-SiC whisker and TaSi2-MoSi2-SiC whisker by slurry method10.1016/j.ceramint.2017.04.140 ↗
11. Preparation of SiC/SiC-CrSi2-ZrB2 bilayer coating on C/C composites by a collaborative design and its oxidation behaviors at 1773 K and 1973 K10.1016/j.ceramint.2025.05.070 ↗
12. Advanced anti-ablation C/C composites: structural design strategies and future perspective10.1016/j.mattod.2024.09.004 ↗
13. Improved oxidation and thermal shock resistance of SiC-Si coating with a SiCw/PyC network structure toughened buffer layer
14. A self-healing HfB2-SiC-TaSi2 coating with outstanding long-term ablation resistance above 2000 °C
15. Investigation on the oxidation and ablation behaviors of HfB2-SiC-Si/SiC-Si coatings for carbon/carbon composites10.1016/j.corsci.2021.109638 ↗
16. Evaluation of theoretical models describing the scratch adhesion test based on experimental results10.1080/00218464.2023.2285466 ↗
17. A theory of friction and wear during the abrasion of metals10.1016/0043-1648(62)90235-1 ↗
18. The effect of nitrogen content on the critical normal force in scratch testing of TiN films10.1016/0040-6090(87)90378-6 ↗
19. CVD-grown SiC nanowires-reinforced SiC coating on C/C composites: focusing on antioxidation, thermal shock and high-temperature gas erosion resistance10.1016/j.surfcoat.2024.131584 ↗
20. Evaluation of the long-term adhesion properties of thermal barrier coatings reinforced with SiC-ZrB2 particles under thermal cycling conditions10.1016/j.ceramint.2024.10.358 ↗
21. Plasma-sprayed nanostructured YSZ thermal barrier coatings: thermal insulation capability and adhesion strength10.1016/j.ceramint.2017.03.074 ↗
22. Ablation behaviors and mechanism of ZrC-SiC-Si/SiC-Si double-layered coatings on C/C composite under plasma flame at 3000 °C10.1016/j.corsci.2023.111200 ↗
23. Influence of temperature, oxygen partial pressure, and microstructure on the high-temperature oxidation behavior of the SiC layer of TRISO particles10.1016/j.jeurceramsoc.2024.116913 ↗
24. Modeling passive/active transition in high-temperature dry oxidation of reaction-sintered SiC for innovative fuel matrix in high-temperature gas-cooled reactors10.1016/j.jeurceramsoc.2023.12.031 ↗
25. Microstructural evolution of SiC coating on C/C composites exposed to 1500 °C in ambient air10.1016/j.ceramint.2018.09.255 ↗
26. The effect of temperature and roughness of the substrate surface on the microstructure and adhesion strength of EB-PVD ZrO2-%8wtY2O3 coating10.1016/j.ceramint.2019.09.217 ↗
27. UHTC coating reinforced by HfC nanowires against ablation for C/C composites10.1016/j.surfcoat.2017.01.014 ↗
28. Fracture toughness of additively manufactured tungsten-rhenium via surface scratch technique10.1016/j.ijrmhm.2025.107290 ↗
29. Effect of sintering temperature on microstructure and properties of SiC coatings for carbon materials10.1016/j.surfcoat.2007.11.014 ↗
30. Accelerated water-oxygen corrosion mechanism of HfB2-SiC/SiC coating on the surface of C/C composites10.1016/j.ceramint.2025.01.230 ↗
31. A critical evaluation of indentation techniques for measuring fracture toughness: i, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
32. Influence of β-SiC phase contents on hardness and elastic modulus of multilayered diamond/β-SiC composite coatings10.1016/j.surfcoat.2025.132340 ↗
33. Effect of porous pre-coating on the phase composition and oxidation protective performance of SiC coating by gaseous silicon infiltration10.1016/j.surfcoat.2024.130597 ↗
34. On the grain size dependence of shock responses in nanocrystalline sic ceramics at high strain rates10.1016/j.actamat.2020.09.044 ↗
35. A peridynamic model for coupled thermo-mechanical-oxygenic analysis of C/C composites with SiC coating10.1016/j.compstruct.2023.117441 ↗