Abstract We have used a complex sol–gel process to synthesize a family of compounds LiNi x Co 1− x O 2 ( x = 0, 0.25, 0.5, 0.75, 1). These compounds are candidates for electrode materials in high-energy-density batteries. Starting sols were prepared from x Ni 2+ + (1 − x ) Co 2+ acetates/ascorbic acid aqueous solutions by alkalizing with LiOH and NH 3 . With thermal treatment in air, nickel carbonates formed in quantities roughly proportional to Ni concentration. The carbonate impurities could not be fully removed by heating in air to high temperatures. Because formation of pure layered oxides was inhibited by the presence of the carbonates, we developed a new way to remove them from just-formed precursors by treating the intermediate phases (those formed after calcination at 750 °C) with concentrated HNO 3 and H 2 O 2 . All resulting powders were phase pure by X-ray diffraction and were easily friable. Various electrochemical properties of compacts prepared from these powders were measured.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. The effects of sintering time on the structure and electrochemical properties of Li(Ni0.8Co0.2)O210.1016/S0378-7753(00)00452-3 ↗
2. Synthesis conditions and oxygen stoichiometry effects on Li insertion into the spinel LiMn2O410.1149/1.2054941 ↗
3. The use of acetates as precursors for the low-temperature synthesis of LiMn2O4 and LiCoO2 intercalation compounds10.1016/0022-4596(91)90231-6 ↗
4. Synthesis and preliminary electrochemical characterization of LiNi0.5Co0.5O2 powders obtained by the complex sol–gel process (CSGP)
5. Synthesis of LixNi0.85Co0.15O2 by the PVA-precursor method and charge–discharge characteristics of a lithium ion battery using this material as cathode10.1016/S0378-7753(99)00271-2 ↗
6. Electrochemical characterization of lithiated mixed nickel–cobalt oxides (LiNi0.5Co1−0.5O2) prepared by sol–gel process10.1007/BF02375715 ↗
7. Particulate sol–gel synthesis and electrochemical characterization of LiMO2 (M=Ni, Ni0.75Co0.25) powders10.1016/S0378-7753(98)00091-3 ↗
8. Divalent cation incorporated Li(1+x)MMgxO2(1+x) (M=Ni0.75Co0.25): viable cathode materials for rechargeable lithium-ion batteries10.1016/S0378-7753(00)00393-1 ↗
9. Syntheses of LiMn2O4, LiCoO2 and LiNi0.8Co0.2O2 by the PVA-precursor method and their use as a cathode in the lithium-ion rechargeable battery10.1023/A:1006610831799 ↗
10. Synthesis and electrochemical characterization of LiNi1−yCoyO2 powders obtained by complex sol–gel process10.1557/PROC-575-97 ↗
11. Some comments on the synthesis of LiNixCo1−xO2 powders by thermal decomposition of organic precursors
12. Synthesis and preliminary electrochemical characterization of LixMn2O4±δ (x=0.55–1.1) powders obtained by the complex sol–gel process (CSGP)
13. Thermal conversion of gels to YBa2Cu3Ox, Bi2Sr2CaCu2Ox, and (Bi, Pb)2Sr2Ca2Cu3Ox and their decarbonization by low-temperature treatment with nitric acid10.1557/JMR.1996.0001 ↗
14. A. Deptuła, T. Olczak, W. Łada, Polish Patent 168,176 (31 January 1996).
15. A. Deptuła, W. Łada, T. Olczak, M.T. Lanagan, S.E. Dorris, K.C. Goretta, R.B. Poeppel, Polish Patent 172,618 (2 June 1997).
16. Applied infrared spectrometry, fundamentals
17. Pre-conditioned layered electrodes for lithium batteries10.1016/j.jpowsour.2005.05.081 ↗