Abstract

Abstract The degradability in an acidic environment and the release of different ions, such as Na+, Ca2+, Al3+ and F− from a calcium fluoro-aluminosilicate glass (used in glass ionomer cements) during different exposure times at 37 °C has been the object of this study. The formation of a leached layer on the surface of the glass has proved to be an important factor in the ionic release from the glass. The structural change in the silicate network of the glass during the dissolution and formation of the leached layer on the surface of the glass has been analyzed by Fourier transform infrared (FTIR) spectrometer. The present study has investigated topographic profiles as a function of time through atomic force microscope (AFM). Also, the formation of the leached layer on the surface of the glass has been described with AFM by measuring the corrosion depth for different times of acidic treatment.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Building materials and conservation · Glass properties and applications · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Wilson · 1998
2. Clinical performance of glass-ionomers10.1016/S0142-9612(97)00139-7 ↗
3. Mount · 1994
4. Glass ionomer dental restoratives10.1016/S0079-6700(01)00006-5 ↗
5. Influence of glass composition on the properties of glass polyalkenoate cements. Part IV. Influence of fluorine content10.1016/S0142-9612(99)00216-1 ↗
6. Method for enhancing the fluoride release of glass-ionomer cement10.1016/0142-9612(96)89659-1 ↗
7. Fluoride release of glass ionomer10.1111/j.1708-8240.1994.tb00862.x ↗
8. The glass ionomer cement the source of soluble fluoride10.1016/S0142-9612(01)00352-0 ↗
9. Caries inhabitation of glass ionomers
10. The effects of adding fluoride compounds to a fluoride-free glass ionomer cement on subsequent fluoride and sodium release10.1016/S0142-9612(02)00467-2 ↗
11. Study on the setting chemistry of glass ionomer cements10.1016/0267-6605(91)90072-N ↗
12. Reactivity of fluoride containing calcium alumino silicate glasses used in dental glass ionomer cements10.1177/00220345980770120901 ↗
13. IR and NMR analyses of hardening and maturation of glass ionomer cement10.1177/00220345960750120201 ↗
14. Dental ceramics, British standard BS EN ISO. 6872, 1999.
15. Paul · 1982
16. Buffering and ion-release by a glass–ionomer cement under near-neutral and acidic conditions10.1016/S0142-9612(02)00014-5 ↗
17. Adhesion to dentin and physical properties of a light-cured glass ionomer liner/base10.1177/00220345910700011201 ↗
18. 1974
19. 1975
20. Characterization of some glasses in the system SiO2, Na2O.RO by infrared spectroscopy10.1016/S0254-0584(02)00215-8 ↗
21. FTIR studies on the effect of network connectivity in the cement forming ability of sol–gel glasses in the SiO2–Al2O3–CaO–CaF2 system10.4028/www.scientific.net/KEM.192-195.749 ↗