Microstructure evolution and properties of dissimilar YIG/MTC joint fabricated with bismuth-based glass ceramic

Qianqian Chen, Panpan Lin, Tiesong Lin, Peng He

Ceramics International· Volume 50· Issue 8
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Magneto-Optical Properties and Applications · Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Mechanistic study of the effect of Ca-Sn co-doping on the microwave dielectric properties and magnetic properties of YIG10.1016/j.ceramint.2022.07.209 ↗
2. Study on Bi3+-Al3+ co-doped YIG for co-firing YIG-Al0.2/NZF ferrite composite substrates10.1016/j.jeurceramsoc.2022.11.021 ↗
3. Polycrystalline Bi substituted YIG ferrite processed via low temperature sintering10.1016/j.jallcom.2016.10.201 ↗
4. Concentrated solar energy used for sintering magnesium titanates for electronic applications10.1016/j.apsusc.2017.09.224 ↗
5. Effect of consolidation parameters on structural, microstructural and electrical properties of magnesium titanate ceramics10.1016/j.ceramint.2016.03.088 ↗
6. A new design of the YIG/MTC joint brazed by bismuth-based glass10.1016/j.jeurceramsoc.2018.12.014 ↗
7. Novel glass-ceramic SOFC sealants from glass powders and a reactive silicone binder10.1016/j.jeurceramsoc.2018.05.024 ↗
8. Effect of Al4B2O9 and Al18B4O33 whiskers synthesized in situ on the evolution of microstructure and mechanical properties of white fused alumina and Cubitron glass-ceramic composites10.1016/j.jeurceramsoc.2022.12.062 ↗
9. Glass-ceramic joining material for sodium-based battery10.1016/j.ceramint.2017.03.170 ↗
10. Joining alumina ceramic by using glass ceramic filler with high crystallinity for high temperature application10.1016/j.ceramint.2019.06.285 ↗
11. Application of Nd2O3-Al2O3-SiO2 glass solder for joining of silicon carbide components10.1016/j.jeurceramsoc.2016.01.020 ↗
12. Development of a gastight sealing material for ceramic components10.1016/S0955-2219(02)00097-3 ↗
13. Cordierite-mullite coating for SiCf/SiC composites10.1016/S0955-2219(01)00535-0 ↗
14. Joining of machined SiC/SiC composites for thermonuclear fusion reactors10.1016/j.jnucmat.2008.02.020 ↗
15. Magnetic properties of low temperature sintered LiZn ferrites by using Bi2O3-Li2CO3-CaO-SnO2-B2O3 glass as sintering agent10.1016/j.ceramint.2017.12.192 ↗
16. Improved sintering characteristics and gyromagnetic properties of low temperature sintered Li.42Zn.27Ti.11Mn.1Fe2.1O4 ferrite ceramics modified with Bi2O3-ZnO-B2O3 glass additive10.1016/j.ceramint.2018.04.134 ↗
17. Effect of a BaO-CuO-Bi2O3-B2O3 glass flux, and its processing on the dielectric properties of BaTiO310.1016/j.ceramint.2014.08.121 ↗
18. Improving sintering behavior of MWCNT/BaTiO3 ceramic nanocomposite with Bi2O3-B2O3 addition10.1016/j.ceramint.2017.11.144 ↗
19. Microstructure evolution and mechanical properties of ZnAl2O4-reinforced Al2O3/Al2O3 joints brazed with a bismuth borate zinc glass10.1016/j.matdes.2017.01.053 ↗
20. Microstructure and characterization of interfacial phases of sapphire/sapphire joint bonded using Bi2O3-B2O3-ZnO glass10.1016/j.jeurceramsoc.2016.10.010 ↗
21. Evolutionary mechanism of YBO3 whisker and its effect on the properties of YIG ferrite joint brazed by Bi2O3-B2O3-SiO2-ZnO glass10.1016/j.ceramint.2020.08.211 ↗
22. Microstructural evolution of Li-Ti ferrite/composite braze/Li-Ti ferrite joints reinforced by Bi5(Ti3Fe)O15 whiskers10.1016/j.jeurceramsoc.2016.06.039 ↗
23. Microstructure evolution and properties of dielectric magnesium titanate ceramic joints fabricated with bismuth glasses10.1016/j.ceramint.2020.08.070 ↗
24. Y. Leng, Y. Chen, Y. Yang, Y. Si, T. Xie, H. Wang, F. Meng, H. Ren, H. Lin. Tailoring the Efficient Laser-Absorption-Melting Behavior of Bi2O3-B2o3-ZnO-Nd2O3 Glass for the OLED Encapsulation. DOI: 10.1111/jace.18911.10.1111/jace.18911 ↗
25. Investigation of the glass forming regularity and thermal behavior of lead-free V2O5-TeO2-RO (R = Ca, Sr, Ba) low temperature sealing glass for electronics packaging10.1016/j.jallcom.2023.172561 ↗
26. Properties and structures of Bi2O3-B2O3-TeO2 glass10.1016/j.jmst.2012.11.003 ↗
27. Effect of ZnO content on microstructure, crystallization behavior, and thermal properties of xZnO-30B2O3-(65-x)Bi2O3-5BaO glass10.1016/j.jnoncrysol.2018.12.036 ↗
28. Investigation of SiO2-B2O3-ZnO-Bi2O3 glass frits on the interface reaction of silver front contacts10.1016/j.jallcom.2020.157646 ↗
29. Review of non-reactive and reactive wetting of liquids on surfaces10.1016/j.cis.2007.04.009 ↗
30. Effects of roughness on the wettability of high temperature wetting system10.1016/j.surfcoat.2016.01.047 ↗
31. Dynamic wetting of various liquids: theoretical models, experiments, simulations and applications10.1016/j.cis.2023.102861 ↗
32. In-situ synthesis of novel Co2FeO4 needle-like phases for structural and functional integration10.1016/j.jmrt.2021.07.012 ↗
33. Structural features of lead iron phosphate glasses10.1016/S0022-3093(02)01021-9 ↗
34. Dielectric properties of P2O5-Na2O-Li2O glasses containing WO3, CoO or Fe2O310.1016/j.ssc.2006.12.024 ↗
35. A new strategy to fabricate YIG ferrite joint with novel magnetic Bi2O3-CoO-Fe2O3-B2O3 glass10.1016/j.matdes.2022.110521 ↗
36. Improvement of mechanical and dielectric properties of PIP-SiCf/SiC composites by using Ti3SiC2 as inert filler10.1016/j.ceramint.2014.12.108 ↗
37. Microstructure and properties of functional magnesium titanate ceramic joint brazed by bismuth-borate glass10.1016/j.jeurceramsoc.2019.07.005 ↗
38. Structure and hyperfine interactions of Bi9Ti3Fe5O27 multiferroic ceramic prepared by sintering and mechanical alloying methods10.1016/j.jnoncrysol.2010.05.043 ↗