journal article·2017-01

Calcium–magnesium aluminosilicate corrosion of barium–strontium aluminosilicates with different strontium content

Fengrui Jiang, Laifei Cheng, Yiguang Wang, Xuanxuan Huang

Ceramics International· Volume 43· Issue 1
Publisher page

Abstract

Abstract In this study, the hot corrosion of barium–strontium aluminosilicate (B 1− x S x AS) attacked by calcium–magnesium aluminosilicate (CMAS) was investigated at temperatures in the 1200–1400 °C range. Moreover, a corrosion mechanism based on the interdiffusion of Ba/Sr and Ca cations was also proposed. The proposed corrosion mechanism indicated the diffusion of Ba/Sr cations into the CMAS, and Ca cations into the B 1− x S x AS during the hot corrosion process. At 1200 °C, a thin corrosion zone was formed at the interface of B 1− x S x AS and CMAS due to weak diffusion of Ba/Sr and Ca cations. Further increase in the temperature led to an enhancement in the interdiffusion of Ba/Sr and Ca cations, thus significantly widening the corrosion zone. Moreover, oriental dendrites, identified as monoclinic B 1− x S x AS, were found to precipitate in the molten CMAS. Attributed to the faster diffusion rate of Sr cations compared to that of the Ba cations, B 1− x S x AS with a higher Sr content was found to be more prone to CMAS-induced corrosion due to the rapid loss of Sr.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Recycling and utilization of industrial and municipal waste in materials production · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Design, fabrication, and application of thermostructural composites (TSC) like C/C, C/SiC, and SiC/SiC composites10.1002/adem.200290001 ↗
2. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
3. SiC-matrix composites: nonbrittle ceramics for thermo-structural application10.1111/j.1744-7402.2005.02009.x ↗
4. Oxidation behaviour of a multi-layered ceramic-matrix composite (SiC)f/C/(SiBC)m10.1016/S0266-3538(00)00243-8 ↗
5. An improved long life duration CMC for jet aircraft engine applications
6. Degradation of SiC/SiC composite due to exposure at high temperatures in vacuum in comparison with that in air10.1016/j.compositesa.2003.09.006 ↗
7. Degradation mechanisms of a SiC fiber reinforced self-sealing matrix composite in simulated combustor environments10.1016/j.jeurceramsoc.2006.02.042 ↗
8. Accelerated oxidation of SiC CMC’s by water vapor and protection via environmental barrier coating approach10.1016/S0955-2219(02)00141-3 ↗
9. Internal friction behavior of C/SiC composites with environmental barrier coatings in corrosive environment10.1111/j.1744-7402.2010.02589.x ↗
10. Current status of environmental barrier coatings for Si-based ceramics
11. Water vapor corrosion behavior of scandium silicates at 1400°C10.1111/j.1551-2916.2008.02864.x ↗
12. Recession behavior of Lu2SiO5 under a high speed steam jet at high temperatures10.1016/j.ceramint.2010.11.029 ↗
13. Recession behavior of Yb2Si2O7 phase under high speed steam jet at high temperatures10.1016/j.corsci.2007.06.014 ↗
14. Upper temperature limit of environmental barrier coatings based on mullite and BSAS10.1111/j.1151-2916.2003.tb03466.x ↗
15. Corrosion of mullite by molten salts10.1111/j.1151-2916.1996.tb08951.x ↗
16. Preparation and molten salt corrosion research of composite environmental barrier coatings of Lu2Si2O7 and Lu2SiO5
17. Influence of temperature and hot corrosion on the micro–nanomechanical behavior of protective mullite EBCs10.1016/j.ijrmhm.2014.09.025 ↗
18. Review – volcanic ash and its influence on aircraft engine components10.1016/j.proeng.2014.12.604 ↗
19. Environmental degradation of thermal-barrier coatings by molten deposits10.1557/mrs.2012.230 ↗
20. Properties of CMAS glass from desert sand10.1016/j.ceramint.2014.11.072 ↗
21. Calcium-magnesium-alumina-silicate (CMAS) delamination mechanisms in EB-PVD thermal barrier coatings10.1016/j.surfcoat.2004.12.029 ↗
22. CMAS corrosion of EB PVD TBCs: identifying the minimum level to initiate damage10.1016/j.ijrmhm.2009.07.005 ↗
23. Calcium–magnesium aluminosilicate (CMAS) reactions and degradation mechanisms of advanced environmental barrier coatings10.1016/j.surfcoat.2013.08.036 ↗
24. Evaluation of CFCC liners with EBC after field testing in a gas turbine10.1016/S0955-2219(02)00142-5 ↗
25. CMAS degradation of environmental barrier coatings10.1016/j.surfcoat.2007.06.045 ↗
26. Chemical and mechanical consequences of environmental barrier coating exposure to calcium-magnesium-aluminosilicate10.1111/j.1551-2916.2011.04448.x ↗
27. Corrosion of barium aluminosilicates by water-vapour: an investigation from first principles10.1016/j.corsci.2009.05.040 ↗
28. Calcium-magnesium-aluminosilicate corrosion behaviors of rare-earth disilicates at 1400°C10.1016/j.jeurceramsoc.2013.05.030 ↗
29. Solid-state synthesis of ceramics in the BaO-SrO-Al2O3-SiO2 system10.1016/S0272-8842(03)00059-2 ↗
30. Thermal and chemical properties of diopside-wollastonite glass-ceramics in the SiO2–CaO–MgO system from raw materials10.1016/S0272-8842(02)00114-1 ↗
31. Phase transformations and melt structure of calcium metasilicate10.1023/A:1019735029277 ↗
32. Melting and crystallization of silicate systems relevant to thermal barrier boating damage
33. Hot corrosion behavior of barium aluminosilicate-coated C/SiC composites at 900°C10.1111/j.1551-2916.2009.03339.x ↗
34. Role of mineralizers on the hexacelsian to celsian transformation in the barium aluminosilicate (BAS) system10.1016/S0921-5093(02)00118-1 ↗