Influence of cover thickness on the ballistic performance of silicon carbide subjected to large-scale tungsten projectiles

Dujun Luo, Yangwei Wang, Fuchi Wang, Huanwu Cheng, Bowen Zhang, Zongjia Li

Ceramics International· Volume 47· Issue 11
Publisher page

Abstract

Abstract Al alloy was the optimal metal cover material for confined silicon carbide (SiC) against blunt tungsten-heavy-alloy projectiles based on a previous research. In this study, the influence of the aluminium (Al) alloy plate thickness on the ballistic performance of SiC was investigated to determine the optimal plate thickness. In addition, the ballistic responses of covered ceramic composite structures under various impact velocities were examined. The failure features of the cover plates and ceramic were elaborated based on tests and simulation analyses. The penetration weight calculated using the measured residual penetration was applied to characterise the ballistic performance of ceramic armour modules. The results showed that thin and thick cover plates could increase the loading rate of the ceramic pressure, thus attenuating their buffering effects on the ceramic. Therefore, the determination of the optimal cover plate thickness must simultaneously meet the requirements of stiffness and the reduced ceramic pressure loading rate. The optimal thickness for the Al alloy cover plate was 4 mm for lateral and back confined ceramic against blunt projectiles in this paper, which was obtained via a numerical simulation. Finally, the buffering effect of the cover plate on enhancing the structural ballistic performance varied with the impact velocities of the projectiles. This study provides insights for covered ceramic armour applications.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Velocity Impact and Material Behavior · Structural Response to Dynamic Loads · Electromagnetic Launch and Propulsion Technology

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Penetration resistance of armor ceramics: dimensional analysis and property correlations10.1016/j.ijimpeng.2015.06.025 ↗
2. Recent advances in hybrid lattice-cored sandwiches for enhanced multifunctional performance10.1016/j.eml.2016.11.009 ↗
3. Ballistic performance of armour ceramics: influence of design and structure. Part 210.1016/j.ceramint.2010.05.022 ↗
4. Enhanced ballistic performance of confined multi-layered ceramic targets against long rod penetrators through interface defeat10.1016/S0020-7683(99)00196-1 ↗
5. Impact of conical tungsten projectiles on flat silicon carbide targets: transition from interface defeat to penetration10.1016/j.ijimpeng.2005.04.004 ↗
6. Tungsten long-rod penetration into confined cylinders of boron carbide at and above ordnance velocities10.1016/S0734-743X(00)00072-5 ↗
7. Inelastic deformation mechanisms and damage in structural ceramics subjected to high-velocity impact10.1111/j.1744-7402.2010.02489.x ↗
8. Penetration of confined silicon carbide targets by tungsten long rods at impact velocities from 1.5 to 4.6 km/s10.1016/0734-743X(95)00064-H ↗
9. The influence of confinement on the penetration of ceramic targets by KE projectiles at 1.8 and 2.6 km/s10.1016/j.ijimpeng.2006.09.029 ↗
10. Behner · 2008
11. Penetration dynamics and interface defeat capability of silicon carbide against long Rod impact10.1016/j.ijimpeng.2010.10.011 ↗
12. Influence of lateral dimensions, obliquity, and target thickness toward the efficiency of unconfined ceramic tiles for the defeat of rod penetrators10.1016/j.ijimpeng.2018.07.006 ↗
13. An investigation on failure mechanisms of ceramicmetal armour subjected to the impact of tungsten projectile10.1016/j.ijimpeng.2010.07.004 ↗
14. Effect of composite covering on ballistic fracture damage development in ceramic plates10.1016/j.ijimpeng.2016.09.010 ↗
15. A detailed computational analysis of interface defeat, dwell and penetration for a variety of ceramic targets
16. Design, analysis and testing of an unconfined ceramic target to induce dwell
17. Mechanics of dwell and post-dwell penetration10.1179/174367509X12535211569512 ↗
18. An analytical model for dwell and interface defeat10.1016/j.ijimpeng.2004.07.013 ↗
19. Leavy · 2006
20. On improving ballistic limit of bi-layer ceramicmetal armor10.1016/j.ijimpeng.2016.09.015 ↗
21. Response of silicon carbide to high velocity impact10.1063/1.1468903 ↗
22. Response of boron carbide subjected to high-velocity impact10.1016/j.ijimpeng.2007.08.003 ↗
23. The influence of metal cover plates on ballistic performance of silicon carbide subjected to large-scale tungsten projectile10.1016/j.matdes.2020.108659 ↗
24. Ballistic performance of ceramic targets against 25mm APDS-T projectile
25. Ballistic performance of confined 99.5%-Al203 ceramic tiles10.1016/S0734-743X(97)00006-7 ↗
26. Effect of cover plate on the ballistic performance of ceramic armor10.3390/ma14010001 ↗
27. Dwell and penetration of tungsten heavy alloy long-rod penetrators impacting unconfined finite-thickness silicon carbide ceramic targets10.1016/j.ijimpeng.2016.04.008 ↗
28. Interface defeat studies of long-rod projectile impacting on ceramic targets10.1016/j.dt.2019.05.021 ↗
29. Effects of hardness of steel on ceramic armour module against long rod impact10.1016/j.ijimpeng.2017.08.004 ↗
30. A numerical investigation of penetration in multilayered material/structure systems10.1016/S0020-7683(97)60353-4 ↗
31. Fracture characteristics of three metals subjected to various strains, strain rates, temperatures and pressures10.1016/0013-7944(85)90052-9 ↗
32. Simulation of damage and failure processes of interpenetrating SiC/Al composites subjected to dynamic compressive loading10.1016/j.actamat.2014.06.045 ↗
33. Implementation and Validation of the Johnson-Holmquist Ceramic Material Model in LS-DYNA
34. Influence of length scale on the transition from interface defeat to penetration in unconfined ceramic targets
35. Impact of metallic projectiles on ceramic targets: transition between interface defeat and penetration10.1016/S0734-743X(99)00152-9 ↗