Strengthening/toughening of 2D C/SiC composites by coating

Y.P. Xie, L.F. Cheng, L.J. Li, Z.X. Meng, L.T. Zhang

Ceramics International· Volume 40· Issue 5
Publisher page

Abstract

Abstract SiC and SiCw/SiC coatings were prepared on two-dimensional carbon fiber reinforced silicon carbide ceramic matrix composites (2D C/SiC), and strengthening/toughening of the composite by the coatings was investigated. After coating, the density of the C/SiC composites was increased effectively and the mechanical properties were improved significantly. Compared with SiC coating, SiCw/SiC coating showed the more significant effect on strength/toughness of the composites. Coatings had two effects: surface strengthening and matrix strengthening. The latter was the dominant effect. The surface strengthening can increase the crack initiation stress, while the matrix strengthening can enhance the crack propagation resistance. The former effect increased the strength and the latter effect increased the toughness.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. The CVI-processing of ceramic matrix composites
2. Structural ceramic composites10.1016/S1359-0286(99)00046-7 ↗
3. Effect of heat treatment on the thermal expansion of 2D and 3D C/SiC composites from room temperature to 1400°C
4. Fiber-reinforced silicon carbide
5. Development of a new cost-effective ceramic composite for re-entry heat shield applications10.1016/S0094-5765(97)00220-8 ↗
6. C/C-SiC composites for space applications and advanced friction systems10.1016/j.msea.2005.08.204 ↗
7. Advanced ceramic matrix composite materials for current and future propulsion technology applications10.1016/j.actaastro.2004.05.052 ↗
8. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
9. Slurry based multilayer environmental barrier coatings for silicon carbide and silicon nitride ceramics—I. Processing10.1016/j.surfcoat.2010.06.029 ↗
10. The coat-mix procedure using carbon fillers10.1016/S0008-6223(96)00120-0 ↗
11. Influence of SiC nanowires on the properties of SiC coating for C/C composites between room temperature and 1500°C10.1016/j.corsci.2011.05.046 ↗
12. Effect of SiC coating and heat treatment on damping behavior of C/SiC composites10.1016/j.msea.2007.06.049 ↗
13. Oxidation behavior of 2D C/SiC with a multi-layer CVD SiC coating10.1016/j.surfcoat.2005.03.009 ↗
14. SiC whisker-toughened SiC oxidation protective coating for carbon/carbon composites10.1016/j.carbon.2005.09.026 ↗
15. Comparison of the mechanical hysteresis of carbon/ceramic-matrix composites with different fiber preforms10.1016/j.carbon.2008.12.025 ↗
16. Fabrication of laminated SiCw/SiC ceramic composites by CVI10.1016/j.jeurceramsoc.2013.02.019 ↗
17. A new method of assessing cardiac autonomic function and its comparison with spectral analysis and coefficient of variation of R–R interval10.1016/S0165-1838(96)00112-9 ↗