Surface characterization of Mo-implanted 6H–SiC by high temperature non-reactive wetting tests with the Ni–56Si alloy
Source abstract
Abstract
The effects of Mo ion implantation into SiC monocrystalline substrates and succeeding annealing treatments on the interfacial characteristics of 6H-SiC were investigated by means of wettability tests. Ni (reactive) and the Ni-56Si alloy (non-reactive) have been used as liquid phases as a means to evidence the influence of surface and interfacial tensions on solid-liquid interactions. The variations of contact angle as a function of Mo implantation and of temperature are analyzed and discussed. The results indicated that a significant improvement of wettability was mainly related to the increase of surface energy ( ?SV) of SiC substrate and to the presence of Mo, rather than to the surface roughness of the ceramic substrate. With increasing annealing temperature, the contact angle of the Ni-56Si/SiC system increased as a result of the crystallization of the SiC amorphous surface and the loss of Mo at the substrate surface due to oxidation and diffusion/vaporization. The influence of these phenomena on technological processes such as metal-ceramic brazing is also taken into consideration.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Silicon Carbide Semiconductor Technologies · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Ceramics
2. Fabrication of mullite-bonded porous silicon carbide ceramics by in situ reaction bonding10.1016/j.jeurceramsoc.2006.06.003 ↗
3. Plasma active sintering of silicon carbide10.1016/j.msea.2006.09.134 ↗
4. Reactive wetting of Ag–Cu–Ti on SiC in HRTEM10.1016/S1359-6454(97)00394-7 ↗
5. Wetting behaviour and interfacial microstructure of palladium- and silver-based braze alloys with C–C and SiC–SiC composites10.1007/s10853-010-4647-5 ↗
6. Wettability and interfacial reaction in SiC/Ni plus Ti system10.1023/A:1015416312807 ↗
7. Wettability of Ni–Cr filler on SiC ceramic and interfacial reactions for the SiC/Ni–51Cr system10.1016/j.scriptamat.2011.02.027 ↗
8. Wettability of Co–V, and PdNi–Cr–V system alloys on SiC ceramic and interfacial reactions10.1016/j.scriptamat.2006.08.067 ↗
9. Influence of oxygen partial pressure on the wetting of SiC by a Co–Si alloy10.1016/j.msea.2007.11.090 ↗
10. Spreading of Cu–Si alloys on oxidized SiC in vacuum: experimental results and modelling10.1016/S1359-6454(01)00397-4 ↗
11. Influence of atmosphere on the wettability of alpha-SiC by non-reactive Cu–Si alloys10.1007/BF00278110 ↗
12. Influence of interfacial reaction rates on the wetting driving force in metal/ceramic systems10.1007/BF02663868 ↗
13. The role of surface chemistry on spreading kinetics of molten silicides on silicon carbide10.1023/B:INTS.0000012297.30968.02 ↗
14. Wetting and bonding of Ni–Si alloys on silicon carbide10.1016/S1359-6454(98)00374-7 ↗
15. Wetting and interfacial behavior of Ni–Si alloy on different substrates10.1007/s10853-009-3858-0 ↗
16. Correlation between the oxidation state of alpha-SiC and its wettability with non-reactive (Sn) or reactive (Ni) metallic components and their binary Si-alloys10.1016/S1359-6454(97)00044-X ↗
17. Relationship between wettability and reactivity in Fe/SiC system10.1016/0956-7151(94)00336-G ↗
18. Wettability of silicon-carbide by liquid silver and binary silver silicon alloy10.1016/0167-577X(94)90010-8 ↗
19. Bonding and wetting in non-reactive metal/SiC systems: weak or strong interfaces?10.1016/S0921-5093(99)00274-9 ↗
20. Wettability and interfacial bonding in Au–Si/SiC system10.1016/0956-7151(93)90041-P ↗
21. The wettability of silicon carbide by Au–Si alloys10.1016/S0921-5093(97)00718-1 ↗
22. Wettability improvement of carbon ceramic materials by mono and multi energy plasma pulses10.1016/j.surfcoat.2009.02.070 ↗
23. The influence of nickel coating on the wettability of aluminum on ceramics10.1016/S1359-835X(02)00161-6 ↗
24. An investigation of the effect of SiC reinforcement coating on the wettability of Al/SiC system10.1177/0021998308092217 ↗
25. Ion-implantation effects in silicon-carbide10.1016/0168-583X(93)90703-9 ↗
26. The effect of titanium ion implantation into carbon ceramic on its wettability by liquid copper10.1016/j.vacuum.2007.01.063 ↗
27. An automatic technique for measuring the surface-tension of liquid metals10.1080/02619180.1989.11753417 ↗
28. High temperature tensiometry
29. Wetting and interactions of Ni- and Co-based superalloys with different ceramic materials10.1007/s10853-009-3801-4 ↗
30. Ziegler · 1985
31. J.F. Ziegler, SRIM-2008.03. Available from: 〈www.SRIM.org〉
32. Experimental investigations and thermodynamic descriptions of the Ni–Si and C–Ni–Si systems10.1007/s11661-999-0249-8 ↗
33. Wettability of SiC by liquid pure metals10.2320/matertrans1960.29.742 ↗
34. Wettability and interfacial energies in SiC-liquid metal systems10.1007/BF02403656 ↗
35. Surface tension and contact angles in some liquid metal-solid ceramics systems at elevated temperatures
36. Survey on wetting of SiC by molten metals10.1016/j.ceramint.2010.01.001 ↗
37. Measurement of contact angle and work of adhesion at high temperature10.1007/s10853-005-1945-4 ↗
38. Kinetic control of silicon carbide/metal reactions10.1016/S0921-5093(98)00899-5 ↗
39. Ion implantation and annealing effects in silicon carbide10.1557/PROC-438-241 ↗
40. Ion-beam modifications of mechanical and dimensional properties of silicon carbide10.1088/0022-3727/45/46/465301 ↗
41. Ion implantation-induced damage depth profile determination in SiC by means of RBS/C and bevelling technique10.1016/j.nimb.2006.06.005 ↗
42. RBS-channeling studies on damage production by MeV ion implantation in Si(111) wafers10.1016/S0921-5107(01)00617-1 ↗
43. A first-principles thermodynamic approach to ordering in Ni–Mo alloys10.1016/S1359-6454(01)00235-X ↗
44. Ion-beam induced damage and annealing behaviour in SiC10.1016/S0168-583X(98)00083-4 ↗
45. Neutron irradiation effects in SiC10.1016/j.nimb.2009.05.029 ↗
46. Visible light laser irradiation: a tool for implantation damage reduction10.4028/www.scientific.net/MSF.457-460.941 ↗
47. Use of a solid-state oxygen pump to study oxidation kinetics of Cr and Mo10.1023/A:1004641328140 ↗
48. Vapor pressure of molybdenum trioxide10.1149/1.2425719 ↗