Abstract The influence of Al 2 O 3 addition on the oxidation behavior of Si-B-C ceramics at 1200 °C in O 2 /H 2 O (40/60) atmosphere was studied. Results showed that Al 2 O 3 was enriched in the oxidized layer, and impeded the crystallization of oxide (cristobalite) during cooling. Denser oxidized layer and less weigh change were observed. Infrared spectra indicated that the addition of Al 2 O 3 could weaken the tendency of bridged oxygen atoms (Si-O-Si, Si-O-Al) to become non-bridged oxygen atoms (Si-O-H) and enhance the degree of interconnection of the structural units. The above phenomenon was attributed to the fact that the bridging oxygen bond between Al and Si was not broken but protonated. The protonated bridging oxygen (Al-O(H)-Si) still acts as a linkage in the glass network, which results in higher viscosity of the aluminosilicates melt and lower reaction activity with steam, thereby significantly improving the oxidation resistance of Si-B-C in O 2 /H 2 O atmosphere.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Ceramic matrix composites10.1098/rsta.1995.0048 ↗
2. Microstructure and tensile properties of BN/SiC coated Hi-Nicalon, and Sylramic SiC fiber preforms10.1023/A:1019692514089 ↗
3. Fabrication of SiCf/SiC composites by alternating current electrophoreticdeposition (AC-EPD) and hot pressing10.1016/j.jeurceramsoc.2014.09.011 ↗
4. Boron-bearing species in ceramic matrix composites for long-term aerospace applications10.1016/j.jssc.2003.03.005 ↗
5. Oxidation behaviour of a boron carbide based material in dry and wet oxygen10.1023/A:1010133703284 ↗
6. Fatigue behavior of a Hi-Nicalon™/SiC-B4C composite at 1200°C in air and steam10.1016/j.msea.2011.11.049 ↗
7. Oxidation behavior of 2D C/SiC composites coated with multi-layer SiC/Si–B–C/SiC coatings under wet oxygen atmosphere10.1016/j.apsusc.2015.06.153 ↗
8. Oxidation behaviors and mechanisms of CVD Si-B-C ceramic in wet oxygen from 700°C to 1400°C10.1016/j.jeurceramsoc.2016.05.050 ↗
9. Oxidation behavior of a multi-layered ceramic-matrix composite (SiC)f/C/(SiBC)m10.1016/S0266-3538(00)00243-8 ↗
10. Oxidation behavior of a boron carbide based material in dry and wet oxygen10.1023/A:1010133703284 ↗
11. High-temperature oxidation of AlN–SiC–TiB2 ceramics in air10.1016/j.jeurceramsoc.2004.12.008 ↗
12. Oxidation behavior of AlN-SiC-TiB2 ceramics synthesized by SHS-HIP10.1016/j.jallcom.2008.11.090 ↗
13. High-temperature corrosion of AlN-based composite ceramic in air and in combustion products of commercial fuel. II. Corrosion of ceramic composites in the AlN–SiC–TiB2 system in air and in combustion products of kerosene and diesel fuel, powder
14. Effect of Al2O3 content on BaO-Al2O3-B2O3-SiO2 glass sealant for solid oxide fuel cell10.1016/j.ceramint.2009.09.045 ↗
15. Structure and crystallization of B2O3-Al2O3-SiO2 glasses10.1016/j.physb.2008.11.198 ↗
16. Cordierite–mullite coating for SiCf/SiC composites10.1016/S0955-2219(01)00535-0 ↗
17. Effect of Al2O3 content on BaO-Al2O3-B2O3-SiO2 glass sealant for solid oxide fuel cell10.1016/j.ceramint.2009.09.045 ↗
18. Wuhan Institute of Building Materials, East China Institute of Chemical Technology, Zhejiang University, Glass Process Principle, China Building Industry Press, 1981, pp. 71–76.
19. Microstructural evolution during the infiltration of boron carbide with molten silicon10.1016/j.jeurceramsoc.2009.09.021 ↗
20. General relationship for the thermal oxidation of silicon10.1063/1.1713945 ↗
21. Reaction of silicon carbide and silicon(IV) oxide at elevated temperature10.1111/j.1151-2916.1992.tb04232.x ↗
22. Thermodynamic measurement of (Al2O3+B2O3) system by double Knudsen cell mass spectrometry10.1016/j.jct.2009.06.002 ↗
23. Study of thermal stability of fumed silica based thermal insulating composites at high temperatures10.1016/j.compositesb.2011.06.023 ↗
24. Effect of Al2O3 powder on properties of fumed silica thermal insulating composites using mechanofusion technique
25. Wuhan Institute of Building Materials, East China Institute of Chemical Technology, Zhejiang University, Glass Process Principle, China Building Industry Press, 1981, pp. 228–234.
26. Bourhis · 2008 · 86
27. Application of IR spectra in the studies of heavy metal cations immobilization on natural sorbents10.1016/j.molstruc.2008.12.028 ↗
28. The FTIR studies of gels and thin films of Al2O3-TiO2 and Al2O3-TiO2-SiO2 systems10.1016/j.saa.2011.12.018 ↗
29. An infrared spectroscopic study of water-related species in silica glasses10.1016/0022-3093(95)00631-1 ↗
30. FTIR and NMR evidence of aluminosilicate microspheres bioactivity tested in simulated body fluid10.1016/j.jnoncrysol.2015.10.039 ↗
31. Application of FTIR and Raman spectroscopy to characterisation of bioactive materials and living cells10.1155/2003/893584 ↗
32. Investigation of the surface reactivity of a sol-gel derived glass in the ternary system SiO2-CaO-P2O510.1016/j.apsusc.2008.05.340 ↗
33. Alternating current electrophoretic deposition of antibacterial bioactive glass-chitosan composite coatings10.3390/ijms150712231 ↗
34. The Two-component bands at about 4500 and 800cm−1 in infrared spectra of hydroxyl-containing silicas. Interpretation in terms of Fermi resonance10.1016/S0022-3093(01)00487-2 ↗
35. SiC recession caused by SiO2 scale volatility under combustion conditions: II, Thermodynamics and gaseous-diffusion model10.1111/j.1151-2916.1999.tb02005.x ↗
36. Molecular mechanisms for corrosion of silica and silicate glasses10.1016/0022-3093(94)90708-0 ↗
37. Water solubility in calcium aluminosilicate glasses investigated by first principles techniques10.1016/j.jssc.2010.08.031 ↗
38. Wuhan Institute of Building Materials, East China Institute of Chemical Technology, Zhejiang University, Glass Process Principle, China Building Industry Press, 1981, pp. 17–18.
39. A multinuclear magnetic resonance study of the structure of hydrous albite glasses10.1016/0016-7037(89)90169-5 ↗
40. The interaction between water and aluminosilicate magmas10.1016/0009-2541(92)90068-G ↗
41. Proton environments in hydrous aluminosilicate glasses: a 1H MAS, 1H/27Al, and 1H/23Na TRAPDOR NMR study10.1021/jp990726l ↗
42. Structural implications of water dissolution in haplogranitic glasses from NMR spectroscopy: influence of total water content and mixed alkali effect10.1016/S0016-7037(01)00623-8 ↗
43. An ab initio calculation of the 17O and 1H NMR parameters for various OH groups: implications to the speciation and dynamics of dissolved water in silicate glasses10.1021/jp0040751 ↗
44. Dissolution mechanisms of water in depolymerized silicate melts: constraints from 1H and 29Si NMR spectroscopy and ab initio calculations10.1016/j.gca.2004.08.016 ↗
45. Water dissolution in albite melts: constrains from ab initio NMR calculations10.1016/S0016-7037(02)01000-1 ↗