journal article·2012-09

Effects of electrolyte pattern on mechanical and electrochemical properties of solid oxide fuel cells

Bora Timurkutluk, Selahattin Celik, Serkan Toros, Cigdem Timurkutluk, Mahmut D. Mat, Yuksel Kaplan

Ceramics International· Volume 38· Issue 7
Publisher page

Abstract

Abstract In order to enhance the electrochemical performance and reduce the operation temperature of a conventional electrolyte supported solid oxide fuel cell (SOFC), a three layered electrolyte with various geometry is designed and fabricated. Novel three layered electrolytes comprise a dense and thin scandia alumina stabilized zirconia (ScAlSZ) electrolyte layer sandwiched between two hallow ScAlSZ electrolyte layers each having the same thickness as the support but machined into a filter like architecture in the active region with circular, rectangular and triangular cut off patterns. The percent of thin electrolyte layer in the active region is kept constant as 30% for all designs in order to investigate the effect of pattern geometry on the mechanical properties and the performance of the electrolytes. Single cells based on novel electrolytes are manufactured and electrochemical properties are evaluated. A standard electrolyte and electrolyte supported cell are also fabricated as a base case for comparison. Although the electrolyte having triangular patterns has the highest peak power at all operation temperatures considered, it exhibits the lowest flexural strength.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Fuel Cells and Related Materials · Perovskite Materials and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. A novel multilayer aqueous tape casting method for anode-supported planar solid oxide fuel cell10.1016/j.matlet.2011.04.077 ↗
2. Fabrication and evaluation of anode and thin Y2O3-stabilized ZrO2 film by co-tape casting and co-firing technique10.1016/j.jpowsour.2009.11.039 ↗
3. Performance improvement of anode-supported electrolytes for planar solid oxide fuel cells via a tape-casting/lamination/co-firing technique10.1016/j.jpowsour.2009.11.086 ↗
4. The effect of porosity gradient in a nickel/yttria stabilized zirconia anode for an anode-supported planar solid oxide fuel cell10.1016/j.jpowsour.2009.08.043 ↗
5. Preparation of YSZ electrolyte coatings for SOFC by electron beam physical vapor deposition combined with a sol infiltration treatment10.1016/j.mseb.2008.03.002 ↗
6. Characterization of thin-film YSZ deposited via EB-PVD technique in anode-supported SOFCs10.1149/1.2186209 ↗
7. Application of novel aerosol-assisted chemical vapor deposition techniques for SOFC thin films10.1016/j.ssi.2004.09.038 ↗
8. Synthesis and characterization of LSGM thin film electrolyte by RF magnetron sputtering for LT-SOFCS10.1016/j.ssi.2008.02.039 ↗
9. Gadolinia-doped ceria films deposited by RF reactive magnetron sputtering10.1016/j.ssi.2009.08.016 ↗
10. Low temperature solid oxide fuel cells with pulsed laser deposited bi-layer electrolyte10.1016/j.jpowsour.2006.09.102 ↗
11. Characterization of yttria-stabilized zirconia thin films grown by pulsed laser deposition (PLD) on various substrates10.1016/j.apsusc.2007.07.194 ↗
12. Thickness determination of large-area films of yttria-stabilized zirconia produced by pulsed laser deposition10.1016/j.apsusc.2005.07.145 ↗
13. Electrophoretic deposition for fabrication of YSZ electrolyte film on non-conducting porous NiO–YSZ composite substrate for intermediate temperature SOFC10.1016/j.jeurceramsoc.2006.04.175 ↗
14. Anode supported solid oxide fuel cells (SOFC) by electrophoretic deposition10.1016/j.ijhydene.2011.02.100 ↗
15. Fabrication of bilayered YSZ/SDC electrolyte film by electrophoretic deposition for reduced-temperature operating anode-supported SOFC10.1016/j.jpowsour.2006.11.087 ↗
16. Changes in physical and mechanical properties of SOFC Ni–YSZ composites caused by redox cycling10.1149/1.2883731 ↗
17. Characterization of the electrochemical performance of micro-tubular SOFC in partial reduction and oxidation conditions10.1016/j.jpowsour.2007.11.052 ↗
18. Current density dependence of changes in the microstructure of SOFC anodes during electrochemical oxidation10.1016/j.ssi.2009.08.003 ↗
19. Anode-supported planar SOFC with high performance and redox stability10.1016/j.elecom.2010.07.011 ↗
20. Degradation of SOFC anodes upon redox cycling: a comparison between Ni/YSZ and Ni/CGO10.1149/1.3271101 ↗
21. Redox stable Ni–YSZ anode support in solid oxide fuel cell stack configuration10.1016/j.jpowsour.2010.11.047 ↗
22. Crack severity in relation to non-homogeneous Ni oxidation in anode-supported solid oxide fuel cells10.1016/j.jpowsour.2010.09.002 ↗
23. Destruction modes of anode-supported SOFC caused by degrees of electrochemical oxidation in redox cycle10.1149/1.3328453 ↗
24. A possible solution to the mechanical degradation of Ni–yttria stabilized zirconia anode-supported solid oxide fuel cells due to redox cycling10.1016/j.jpowsour.2010.03.043 ↗
25. A simple bilayer electrolyte model for solid oxide fuel cells10.1016/S0167-2738(02)00758-0 ↗
26. Ce0.8Gd0.2O2−δ ceramics derived from commercial submicron-sized CeO2 and Gd2O3 powders for use as electrolytes in solid oxide fuel cells10.1016/j.jpowsour.2003.12.029 ↗
27. Densification of plasma sprayed YSZ electrolytes by spark plasma sintering (SPS)10.1016/S0955-2219(02)00421-1 ↗
28. Development of yttria-stabilized zirconia thin films via slurry spin coating for intermediate-to-low temperature solid oxide fuel cells10.1016/j.jpowsour.2006.01.079 ↗
29. Fabrication of tubular electrolytes for solid oxide fuel cells using strontium- and magnesium-doped LaGaO3 materials10.1016/S0955-2219(00)00257-0 ↗
30. Bismuth based oxide electrolytes structure and ionic conductivity10.1016/S0955-2219(99)00009-6 ↗
31. A screen-printed Ce0.8Sm0.2O1.9 film solid oxide fuel cell with a Ba0.5Sr0.5Co0.8Fe0.2O3−δ cathode10.1016/j.jpowsour.2006.02.048 ↗
32. Demonstration of high efficiency intermediate-temperature solid oxide fuel cell based on lanthanum gallate electrolyte10.1016/j.jallcom.2005.04.158 ↗
33. Preparation and sintering of Ce1−xGdxO2−x/2 nanopowders and their electrochemical and EPR characterization10.1016/j.ssi.2004.03.034 ↗
34. Oxygen permeability of gadolinium-doped ceria at high temperature10.1016/S0955-2219(03)00555-7 ↗
35. Novel structured gadolinium doped ceria based electrolytes for intermediate temperature solid oxide fuel cells10.1016/j.jpowsour.2011.07.047 ↗
36. A solid oxide fuel cell with a gadolinia-doped ceria anode: preparation and performance10.1016/S0167-2738(99)00111-3 ↗
37. Chemically induced stresses in gadolinium-doped ceria solid oxide fuel cell electrolytes10.1016/S0167-2738(96)00588-7 ↗
38. Physical chemical and electrochemical properties of pure and doped ceria10.1016/S0167-2738(99)00318-5 ↗
39. Increasing power density of LSGM-based solid oxide fuel cells using new anode materials10.1149/1.1378289 ↗
40. A solid oxide fuel cell based on Sr- and Mg-doped LaGaO electrolyte: the role of a rare-earth oxide buffer10.1016/S0925-8388(00)00626-5 ↗
41. Interface reactions in the NiO–SDC–LSGM system10.1016/S0167-2738(00)00744-X ↗
42. Oxide-ion conducting ceramics for solid oxide fuel cells10.1023/A:1004813305237 ↗
43. Characterization of scandia stabilized zirconia prepared by glycine nitrate process and its performance as the electrolyte for IT-SOFC10.1016/j.ssi.2005.01.004 ↗
44. Electrolytes for solid oxide fuel cell10.1016/j.jpowsour.2006.06.062 ↗
45. Degradation of the electrical conductivity in stabilised zirconia system. Part II: Scandia-stabilised zirconia10.1016/j.ssi.2004.07.039 ↗
46. Electrical conductivity of the ZrO2–Ln2O3 (Ln=lanthanides) system10.1016/S0167-2738(98)00540-2 ↗
47. Ionic conductivity and morphology in Sc2O3 and Al2O3 doped ZrO2 films prepared by the sol–gel method10.1016/S0167-2738(97)00423-2 ↗
48. Mechanical properties of 10mol% Sc2O3–1mol% CeO2–89mol% ZrO2 ceramics10.1016/j.jpowsour.2009.11.016 ↗
49. Phase stability and sintering behavior of 10mol% Sc2O3–1mol% CeO2–ZrO2 ceramics
50. Stability of solid oxide fuel cell components10.1016/S0167-2738(01)00831-1 ↗
51. Structure and impedance of ZrO2 doped with Sc2O3 and CeO210.1016/j.matlet.2004.07.065 ↗
52. Characterization of ZrO2 co-doped with Sc2O3 and CeO2 electrolyte for the application of intermediate temperature SOFCs10.1016/j.ssi.2004.07.013 ↗
53. Electrical conductivity of ZrO2-Sc2O3 doped with HfO2 CeO2, and Ga2O310.1149/1.1366622 ↗
54. Development of high-performance electrolyte in SOFC10.1016/0167-2738(94)90158-9 ↗
55. Al2O3 solubility in the fast ion conductor 0.88ZrO2–(0.12−x)Sc2O3–xAl2O3 determined by 27Al NMR10.1016/j.ssi.2003.12.043 ↗
56. Polarization effects in intermediate temperature, anode-supported solid oxide fuel cells10.1149/1.1391566 ↗
57. Improvement of mechanical and electrical properties of scandia-doped zirconia ceramics by post-sintering with hot isostatic pressing10.1111/j.1151-2916.2000.tb01600.x ↗
58. Performance evaluation of anode-supported solid oxide fuel cells with thin film YSZ electrolyte10.1016/j.ijhydene.2004.01.009 ↗
59. Densification and properties of zirconia prepared by three different sintering techniques10.1016/j.ceramint.2006.07.005 ↗
60. Effect of nano-grain size on the ionic conductivity of spark plasma sintered 8YSZ electrolyte10.1016/j.ijhydene.2011.09.018 ↗
61. Processing of nanocrystalline 8mol% yttria-stabilized zirconia by conventional microwave-assisted and two-step sintering10.1016/j.msea.2008.03.023 ↗
62. Strength and fracture of glass and ceramics