Abstract Starting from TiB2, Mo, Co, and C powders, TiB2-based ceramics for cutting tools were prepared by hot-pressing at 1900 °C. The densification, microstructure and mechanical properties of TiB2–Mo–Co and TiB2–Mo–Co–C samples were evaluated. More importantly, the cutting performance of these ceramics were examined by high-speed turning of Ti6Al4V alloy (vc = 150 m/min, ap = 0.5 mm). It was found that the hardness of these two specimens was comparable (~19 GPa) and the tool life of TiB2–Mo–Co was longer than that of TiB2–Mo–Co–C. In order to investigate the wear behavior, the dominant wear mode of TiB2-based cutting tools with different feed rate was compared with commercial WC-Co cutting tool. The combination of microstructure and composition results revealed that the superior cutting performance of TiB2-based ceramic cutting tools could be mainly attribute to their better oxidation resistance, better high-temperature mechanical properties, and lower affinity with titanium alloy than WC-Co composite tools.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Orthopaedic implants and arthroplasty
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Heat generation and temperature prediction in metal cutting: a review and implications for high speed machining10.1016/j.ijmachtools.2005.07.024 ↗
2. Effect of machining parameters and cutting edge geometry on surface integrity of high-speed turned Inconel 71810.1016/j.ijmachtools.2007.08.004 ↗
3. A comparative study of the cutting forces in high speed machining of Ti-6Al-4V and Inconel 718 with a round cutting edge tool10.1016/j.jmatprotec.2008.10.013 ↗
4. Influence of cutting speed on cutting force, flank temperature, and tool wear in end milling of Ti-6Al-4V alloy10.1007/s00170-013-5433-8 ↗
5. The influences of tool wear on Ti6Al4V cutting temperature and burn defect10.1007/s00170-015-8093-z ↗
6. Machinability of titanium alloys (Ti6Al4V and Ti555.3)10.1016/j.jmatprotec.2008.06.020 ↗
7. Tool wear mechanisms involved in crater formation on uncoated carbide tool when machining Ti6Al4V alloy10.1007/s00170-015-7668-z ↗
8. Diffusion wear in dry cutting of Ti–6Al–4V with WC/Co carbide tools10.1016/j.wear.2008.04.024 ↗
9. Wear mechanisms analysis for turning Ti-6Al-4V—towards the development of suitable tool coatings10.1007/s00170-011-3427-y ↗
10. Lathe turning of titanium using pulsed laser deposited, ultra‐hard boride coatings of carbide inserts10.1081/MST-120018958 ↗
11. Wear mechanisms of new tool materials for Ti-6AI-4V high performance machining10.1016/S0007-8506(07)60534-4 ↗
12. Tribological and wear performance of carbide tools with TiB2 PVD coating under varying machining conditions of TiAl6V4 aerospace alloy10.3390/coatings7110187 ↗
13. Knowledge based coating design of CVD TiN-TiBN-TiB2 architecture10.1016/j.ijrmhm.2017.11.040 ↗
14. Processing and properties of monolithic TiB2 based materials10.1179/174328006X102529 ↗
15. Effects of TiC content and melt phase on microstructure and mechanical properties of ternary TiB2-based ceramic cutting tool materials10.1016/j.msea.2014.03.036 ↗
16. Effect of metallic dopants on the microstructure and mechanical properties of TiB210.1016/j.jeurceramsoc.2015.03.027 ↗
17. Cutting performance and wear mechanism of TiB2-B4C ceramic cutting tools in high speed turning of Ti6Al4V alloy10.1016/j.ceramint.2018.05.209 ↗
18. Fracture toughness determinations by indentation10.1111/j.1151-2916.1976.tb10991.x ↗
19. ISO 1832-2012. Indexable Inserts for Cutting Tools - Designation.
20. Phase Evolution, microstructure and hardness of TiB2-based Co containing composite by SHS under pseudo-isostatic pressure10.2355/isijinternational.52.1698 ↗
21. Influences of metallic Co and mechanical alloying on the microstructural and mechanical properties of TiB2 ceramics prepared via pressureless sintering10.1016/j.jeurceramsoc.2011.10.033 ↗
22. Effects of sintering additives on microstructure and mechanical properties of TiB2 –WC ceramic–metal composite tool materials10.1016/j.ijrmhm.2011.07.008 ↗
23. The effect of surface oxides during hot pressing of TiB210.1111/j.1551-2916.2009.02923.x ↗
24. Tribo-energetic correlation of tool thermal properties to wear of WC-Co inserts in high speed dry machining of aeronautical grade titanium alloys10.1016/j.wear.2008.04.023 ↗
25. Understanding the diffusion wear mechanisms of WC-10%Co carbide tools during dry machining of titanium alloys10.1016/j.wear.2017.07.003 ↗
26. Results from bending tests on submicron and micron WC–Co grades at elevated temperatures10.1016/S0263-4368(01)00072-5 ↗
27. Experimental strategy to study the mechanical behaviour of hardmetals for cutting tools10.1016/S0263-4368(98)00078-X ↗
28. Ultra-high elevated temperature strength of TiB2-based ceramics consolidated by spark plasma sintering10.1016/j.jeurceramsoc.2016.08.009 ↗
29. Densification and high-temperature mechanical properties of hot pressed TiB2–(0–10 wt.%) MoSi2 composites10.1016/j.scriptamat.2009.05.031 ↗