Pore structure of reactively synthesized nanolaminate Ti3SiC2 alloyed with Al
Source abstract
Abstract
Abstract Ti3SiC2 has the unique properties integrating the advantages of metals and ceramics, and good open pore structure when alloyed with Al. In this work, porous Ti3SiC2 compounds with different Al/Si atom ratios were prepared through the reactive synthesis of elemental powders at 1300 °C. The results indicate that the phase compositions are determined by Al element mole number, and that the pore structure can be controlled through varying Ti particle size. The MAX phase transits from Ti3SiC2 with Al element mole number no more than 0.6 to Ti3AlC2 with Al element mole number in the range of 0.8–1.2. When Al element mole number is 0.6, the porous compound has a single MAX phase of Ti3SiC2 with uniform microporous structure and high bending strength. Porous Ti3SiC2 alloyed with 0.6Al has a slow linear increase rate of 0.0083%/μm in open porosity with increasing Ti particle size, and a strict linear relationship between the maximum aperture and Ti particle size with the increase rate of 0.0342 μm/μm. The pore structure formed by the phase transition mechanism for porous MAX phase has the smallest tortuosity factor compared with that formed by the clearance mechanism and the Kirkendall effect.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced biosensing and bioanalysis techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Compositional dependence of epitaxial Tin+1SiCn MAX-phase thin films grown from a Ti3SiC2 compound target10.1116/1.5065468 ↗
2. Synthesis of single-phase Ti3SiC2 from coarse elemental powders and the effects of excess Al10.1016/j.ceramint.2018.09.270 ↗
3. Oxidation behavior of reactively synthesized porous Ti3(Si,Al)C2 compound at 800°C in ambient air10.1016/j.ceramint.2019.05.051 ↗
4. Microstructure and mechanical properties of in situ synthesized (TiB2+TiC)/Ti3SiC2 composites10.1016/j.ceramint.2011.06.066 ↗
5. Machinability of Ti3SiC2 with layered structure synthesized by hot pressing mixture of TiCx and Si powder10.1016/j.jeurceramsoc.2012.04.021 ↗
6. Porous Ti3SiC2 fabricated by mixed elemental powders reactive synthesis10.1016/j.jeurceramsoc.2014.11.006 ↗
7. Characterization and application of porous Ti3SiC2 ceramic prepared through reactive synthesis10.1016/j.matdes.2015.03.061 ↗
8. Reactive synthesis of porous nanolaminate Ti3(Si,Al)C2 intermetallic compound10.1016/j.matchemphys.2017.12.076 ↗
9. Irradiation damage in Ti3(Si,Al)C2: a TEM investigation10.1111/j.1744-7402.2010.02523.x ↗
10. Improving the oxidation resistance of Ti3SiC2 by forming a Ti3Si0.9Al0.1C2 solid solution10.1016/j.actamat.2004.04.015 ↗
11. Fabrication of Ti-Al micro/nanometer-sized porous alloys through the Kirkendall effect10.1002/adma.200602398 ↗
12. Criterion to control self-propagation high temperature synthesis for porous Ti-Al intermetallics10.1179/003258910X12707304455266 ↗
13. Rapid synthesis of ternary carbide Ti3SiC2 through pulse-discharge sintering technique from Ti/Si/TiC powders10.1007/s11661-002-0320-1 ↗
14. Synthesis and characterization of quaternary Ti3Si(1-x)AlxC2 MAX phase materials10.1016/j.ceramint.2015.02.088 ↗
15. Effects of the Al content on pore structures of porous Ti3AlC2 ceramics by reactive synthesis10.1016/j.ceramint.2013.09.004 ↗
16. Fabrication of porous nickel-copper alloy with controlled micro-sized pore structure through the Kirkendall effect10.1016/j.matchemphys.2015.07.050 ↗
17. Evolution of the porous structure during non-isothermal sintering of fine powders
18. Sintering kinetics at isothermal shrinkage: effect of specific area on the initial sintering stage of fine zirconia powder10.1111/j.1551-2916.2006.01341.x ↗
19. Estimating permeability of porous media based on modified Hagen-Poiseuille flow in tortuous capillaries with variable lengths10.1007/s10404-016-1783-5 ↗
20. Tortuosity factor for porous FeAl intermetallics fabricated by reactive synthesis10.1016/S1003-6326(11)61446-5 ↗
21. Solute segregation effect on grain boundary migration and Hall-Petch relationship in CrMnFeCoNi high-entropy alloy10.1080/02670836.2019.1570679 ↗
22. Factors affecting the property of porous Ti3SiC2 metal ceramic fabricated through pressureless sintering10.1007/s10934-015-0006-x ↗
23. An approach to defining tortuosity and cementation factor in carbonate reservoir rocks10.1016/j.petrol.2007.05.010 ↗
24. A novel experimental setup to study the Hagen-Poiseuille and Bernoulli equations for a gas and determination of the viscosity of air10.1088/0143-0807/36/6/065046 ↗
25. Fabrication of porous stainless steel 316L for biomedical applications
26. A novel water leaching and sintering process for manufacturing highly porous stainless steel10.1016/j.scriptamat.2006.03.039 ↗
27. The fabrication and the properties of gradient porous titanium by centrifugal deposition and sintering10.4028/www.scientific.net/AMR.1042.38 ↗