Abstract

Abstract The Si3N4 coating and Si3N4 coating with Si3N4 whiskers as reinforcement (Si3N4w-Si3N4) were prepared by chemical vapor deposition (CVD) on two-dimensional silicon nitride fiber reinforced silicon nitride ceramic matrix composites (2D Si3N4f/Si3N4 composites). The effects of process parameters of as-prepared coating including the preparation temperature and volume fraction of Si3N4w on the microstructure and mechanical properties of the composites were investigated. Compared with Si3N4 coating, Si3N4w-Si3N4 coating shows more significant effect on the strength and toughness of the composites, and both strengthening and toughening mechanism were analyzed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Fabrication and high-temperature mechanical properties of 2.5D Si3N4f/BN fiber-reinforced ceramic matrix composite10.1016/j.matdes.2015.12.048 ↗
2. Analysis of existing radioparent refractory materials, composites and technology for creating high-speed rocket radomes. Part 2. Comparative analysis of the main properties of materials used for creating rocket radomes10.1007/s11148-010-9308-3 ↗
3. Low-observable radomes composed of composite sandwich constructions and frequency selective surfaces10.1016/j.compscitech.2008.03.016 ↗
4. Processing, microstructure, mechanical properties of Si3N4 obtained by slip casting and pressureless sintering10.1016/S0272-8842(01)00006-2 ↗
5. Design and fabrication of porous Si3N4-Si2N2O in situ composite ceramics with improved toughness10.1016/j.matdes.2016.08.023 ↗
6. Relationship between microstructure, toughening mechanisms, and fracture toughness of reinforced silicon nitride ceramics10.1111/j.1151-2916.1995.tb08031.x ↗
7. Fabrication of gel cast BN/Si3N4 composite ceramics from surface-coated BN powder10.1016/j.msea.2014.12.050 ↗
8. Evans AG, Marshall DB, editors. The Mechanical Behavior of Ceramic Matrix Composites1989.10.1016/B978-0-08-034341-9.50251-5 ↗
9. The physics and mechanics of fibre-reinforced brittle matrix composites10.1007/BF00355946 ↗
10. Perspective on the development of high‐toughness ceramics10.1111/j.1151-2916.1990.tb06493.x ↗
11. Effect of intermediate heat treatment on mechanical properties of SiC/SiC composites with BN interphase prepared by ICVI10.1016/j.jeurceramsoc.2010.12.018 ↗
12. Carbon/silicon carbide composites prepared by chemical vapor infiltration combined with silicon melt infiltration10.1016/S0008-6223(98)00310-8 ↗
13. Three‐dimensional carbon/silicon carbide composites prepared by chemical vapor infiltration10.1111/j.1151-2916.1997.tb03069.x ↗
14. Effect of coating defects on oxidation behavior of three dimensional C/SiC composites from room temperature to 1500°C10.1023/A:1021089411141 ↗
15. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
16. Preparation of an oxidation protection coating for c/c composites by low pressure chemical vapor deposition10.1016/S0008-6223(00)00086-5 ↗
17. Protective multilayer coatings for carbon‐carbon composites10.1016/S0008-6223(01)00151-8 ↗
18. Oxidation behavior of 2D C/SiC with a multi-layer CVD SiC coating10.1016/j.surfcoat.2005.03.009 ↗
19. SiC whisker-toughened SiC oxidation protective coating for carbon/carbon composites10.1016/j.carbon.2005.09.026 ↗
20. Strengthening/toughening of 2D C/SiC composites by coating10.1016/j.ceramint.2013.12.007 ↗
21. Toughening behavior in whisker‐reinforced ceramic matrix composites10.1111/j.1151-2916.1988.tb05791.x ↗
22. Fracture and flexural characterization of SiCw/SiC composites at room and elevated temperatures10.1007/BF01184593 ↗
23. Mechanical and dielectric properties of two types of Si3N4 fibers annealed at elevated temperatures10.3390/ma11091498 ↗
24. Fabrication of laminated SiCw/SiC ceramic composites by CVI10.1016/j.jeurceramsoc.2013.02.019 ↗
25. Microstructure and mechanical properties of three-dimensional carbon/silicon carbide composites fabricated by chemical vapor infiltration10.1016/S0008-6223(98)00076-1 ↗