Positive effect of codoping Yb3+ on the super-long persistent luminescence of Cr3+-doped zinc aluminum germanate
Source abstract
Abstract
Abstract A series of novel near-infrared (NIR) long persistent phosphors of Zn1.2Al1.6Ge0.2O4: Cr3+, Yb3+ was synthesized by a solid state method. The crystal structure of Zn1.2Al1.6Ge0.2O4 was identified. Yb3+ ions were effective codopants for improving the NIR persistent luminescence intensity even after 100 h of decay. The persistent luminescence decay curves and the thermo-luminescence spectra were analyzed. Results indicated that the increase in efficient electron trap concentration induced by doping Yb3+ ions was a major factor in the improvement of the NIR persistent luminescence. Moreover, short-wave infrared (SWIR = 900–1700 nm) emission of Yb3+ was be excited by UV and visible light through charge transfer transition of O2-–Yb3+ and energy transfer from Cr3+ to Yb3+, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Luminescence Properties of Advanced Materials · Luminescence and Fluorescent Materials · Perovskite Materials and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Nanoprobes with near-infrared persistent luminescence for in vivo imaging10.1073/pnas.0702427104 ↗
2. Functional Near Infrared-Emitting Cr3+/Pr3+ Co-Doped Zinc Gallogermanate Persistent Luminescent Nanoparticles with Superlong Afterglow for in Vivo Targeted Bioimaging10.1021/ja404243v ↗
3. Five-Nanometer ZnSn2O4: cr, Eu Ultra-small nanoparticles as new near infrared-emitting persistent luminescent nanoprobes for cellular and deep tissue imaging at 800 nm
4. Controlling electron trap depth to enhance optical properties of persistent luminescence nanoparticles for in vivo imaging10.1021/ja204504w ↗
5. Magnetic-NIR persistent luminescent dual-modal ZGOCS@MSNs@Gd2O3 core–shell nanoprobes for in vivo imaging10.1021/acs.chemmater.7b00087 ↗
6. Quantum dots for live cells, in vivo imaging, and diagnostics10.1126/science.1104274 ↗
7. Lanthanide-doped luminescent nanoprobes: controlled synthesis, optical spectroscopy, and bioapplications10.1039/c3cs60060b ↗
8. The in vivo activation of persistent nanophosphors for optical imaging of vascularization, tumours and grafted cells10.1038/nmat3908 ↗
9. Red and near infrared persistent luminescence nano-probes for bioimaging and targeting applications10.1039/C4RA08847F ↗
10. ZnGa2O4:Cr3+: a new red long-lasting phosphor with high brightness10.1364/OE.19.010131 ↗
11. A strategy for developing near infrared long-persistent phosphors: taking MAlO3:Mn4+,Ge4+ (M = La, Gd) as an example10.1039/c3tc32075h ↗
12. Sunlight-activated long-persistent luminescence in the near-infrared from Cr3+-doped zinc gallogermanates10.1038/nmat3173 ↗
13. Tunable trap depth in Zn(Ga1−xAlx)2O4:cr,bi red persistent phosphors: considerations of high-temperature persistent luminescence and photostimulated persistent luminescence10.1039/c3tc31462f ↗
14. Storage of visible light for long-lasting phosphorescence in chromium-doped zinc gallate10.1021/cm403050q ↗
15. Photostimulated near-infrared persistent luminescence as a new optical read-out from Cr3+-doped LiGa5O8
16. Tailoring of the trap distribution and crystal field in Cr3+-doped non-gallate phosphors with near-infrared long-persistence phosphorescence10.1038/am.2015.38 ↗
17. A review on how lanthanide impurity levels change with chemistry and structure of inorganic compounds10.1149/2.001302jss ↗
18. Trap depth engineering of SrSi2O2N2:Ln2+,Ln3+ (Ln2+ = Yb, Eu; Ln3+ = Dy, Ho, Er) persistent luminescence materials for information storage applications10.1021/acsami.7b17271 ↗
19. Controlled electron–hole trapping and detrapping process in gdalo3 by valence band engineering10.1021/acs.jpcc.6b00129 ↗
20. Germanium substitution endowing Cr3+-doped Zinc aluminate phosphors with bright and super-long near-infrared persistent luminescence10.1016/j.actamat.2018.06.020 ↗
21. Considerable improvement of long-persistent luminescence in germanium and tin substituted ZnGa2O410.1021/cm304101n ↗
22. Order and disorder around Cr3+ in chromium doped persistent luminescent AB2O4 spinels10.1039/C5CP01097G ↗
23. Controlling disorder in the ZnGa2O4:Cr3+ persistent phosphor by Mg2+ substitution10.1039/C6CP06443D ↗
24. New function of the Yb3+ ion as an efficient emitter of persistent luminescence in the short-wave infrared10.1038/lsa.2016.124 ↗
25. Up-conversion emission color tuning in NaLa(MoO4)2: Nd3+/Yb3+/Ho3+ excited at 808 nm10.1016/j.ceramint.2017.02.041 ↗
26. Synthesis, up-conversion luminescence and thermometry of Yb3+/Er3+ co-doped La2.4Mo1.6O8 phosphors10.1039/C6DT03059A ↗
27. The importance of inversion disorder in the visible light induced persistent luminescence in Cr3+ doped AB2O4 (A = Zn or Mg and B = Ga or Al)10.1039/C4CP03866E ↗
28. Broadband near-infrared down-shifting by Yb-O charge-transfer band in Yb3+ singly doped tellurite glasses10.1111/jace.13959 ↗
29. Synthesis, crystal structure, and enhanced luminescence of garnet-type Ca3Ga2Ge3O12:Cr3+ by codoping Bi3+10.1111/jace.13553 ↗