Abstract
Abstract The effects of Cr 2 O 3 derived from Cr(NO 3 ) 3 ·9H 2 O precursor on the densification, microstructure and mechanical properties of zirconia-toughened alumina (ZTA) ceramics were investigated. The Cr 2 O 3 content in ZTA varied from 0 to 0.8 wt%. Cr 2 O 3 derived from Cr(NO 3 ) 3 ·9H 2 O can form solid solutions with Al 2 O 3 and ZrO 2 in ZTA more efficiently than Cr 2 O 3 additive directly added to ZTA. The precursor-derived Cr 2 O 3 can significantly promote the densification of ZTA and nearly fully dense ZTA composites were obtained by pressureless sintering at 1540 °C for 2 h. In contrast, the effect of directly added Cr 2 O 3 additive on densification of ZTA was limited due to its low amount of dissolution in ZTA. ZTA with 0.5 wt% Cr 2 O 3 derived from Cr(NO 3 ) 3 ·9H 2 O had fine microstructure and its fracture toughness was as high as 4.67±0.03 MPa m 1/2 which was about 30% higher than that of undoped ZTA and ZTA with 0.5 wt% Cr 2 O 3 . ZTA with 0.5 wt% precursor-derived Cr 2 O 3 had the maximum Vickers hardness about 18.10±0.15 GPa. Higher content of Cr 2 O 3 (0.8 wt% or higher) would have adverse effect on the densification due to the vaporization and condensation of Cr-containing species during pressureless sintering.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Effect of ceria on the physical, mechanical and thermal properties of yttria stabilized zirconia toughened alumina10.1016/S0921-5093(02)00368-4 ↗
2. Physical and mechanical properties of Ta2O5 doped zirconia-toughened alumina (ZTA) composites10.1016/j.ceramint.2015.01.039 ↗
3. Microstructural coarsening of zirconia-toughened alumina composites10.1111/j.1551-2916.2005.00374.x ↗
4. Alumina ceramics with partially stabilized zirconia for cutting tools10.1016/S0924-0136(02)00232-7 ↗
5. The relationship between microstructure and fracture toughness of zirconia toughened alumina (ZTA) added with MgO and CeO210.1016/j.ijrmhm.2013.07.002 ↗
6. Mechanical properties of Al2O3/ZrO2 composites10.1016/S0955-2219(02)00043-2 ↗
7. Structural evolution of ZTA composites during synthesis and processing10.1016/j.jeurceramsoc.2014.10.031 ↗
8. Effect of Fe2O3 doping on sintering of yttria-stabilized zirconia10.1016/j.jeurceramsoc.2012.07.035 ↗
9. Development of Ce-PSZ-/Y-PSZ-toughened alumina inserts for high-speed machining steel10.1111/ijac.12181 ↗
10. Effect of the composition and sintering process on mechanical properties and residual stresses in zirconia-alumina composites10.1016/j.jeurceramsoc.2004.09.025 ↗
11. Synthesis of zirconia toughened alumina (ZTA) fibers for high performance materials10.1016/j.jeurceramsoc.2015.10.028 ↗
12. The effects of CeO2 addition on the physical, microstructural and mechanical properties of yttria stabilized zirconia toughened alumina (ZTA)10.1016/j.ijrmhm.2012.08.010 ↗
13. The effects of MgO addition on microstructure, mechanical properties and wear performance of zirconia-toughened alumina cutting inserts10.1016/j.jallcom.2010.03.054 ↗
14. Effect of Cr2O3 addition on microstructural evolution and mechanical properties of Al2O310.1016/S0955-2219(00)00023-6 ↗
15. Effects of Cr2O3 addition on the mechanical properties, microstructure and wear performance of zirconia-toughened-alumina (ZTA) cutting inserts10.1016/j.jallcom.2011.09.092 ↗
16. Sintering behavior of Cr2O3–Al2O3 ceramics10.1016/S0955-2219(99)00161-2 ↗
17. C-diffusion during hot press in the Al2O3–Cr2O3 system10.1016/S1359-6454(02)00393-2 ↗
18. Effect of solid solution formation on densification of hot-pressed ZrC ceramics with MC (M=V, Nb, and Ta) additions10.1016/j.jeurceramsoc.2011.10.045 ↗