journal article·2020-12

The effect of transition metal carbides MeC (Me = Ti, Zr, Nb, Ta, and W) on mechanical properties of B4C ceramics fabricated via pressureless sintering

Guanqi Liu, Shixing Chen, Yanwei Zhao, Yudong Fu, Yujin Wang

Ceramics International· Volume 46· Issue 17
Publisher page

Abstract

Abstract In this study, boron carbide-metallic boride (B4C-MeBx, Me = Ti, Zr, Nb, Ta, or W) multiphase ceramics were fabricated via in situ pressureless sintering at 2250 °C for 1 h. The effects of transition metal carbides, namely, TiC, ZrC, NbC, TaC, and WC, on the phase composition, microstructure, and mechanical properties of the ceramics were investigated. The results showed that MeC could facilitate the sintering densification of B4C by distributing second-phase particles uniformly throughout the B4C. Additionally, the main phases observed were B4C and (Me, W)Bx (Me = Ti, Zr, Nb, or Ta) due to the doping of a small amount of WC during the ball milling process. As a result, the mechanical properties of B4C-MeBx showed significant improvements when compared with those of single-phase B4C ceramics. B4C–NbB2 ceramics were found to exhibit the best mechanical properties, with an elastic modulus of 393.0 GPa, a hardness of 28.7 GPa, a flexural strength of 368.0 MPa, and a fracture toughness of 6.94 MPa m1/2.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Microstructural evolution during the infiltration of boron carbide with molten silicon10.1016/j.jeurceramsoc.2009.09.021 ↗
2. Atomic structure and vibrational properties of icosahedral α-boron and B4C boron carbide10.1016/S0927-0256(00)00009-4 ↗
3. Hardness and wear resistance of B4C ceramics prepared with several additives10.1016/j.matlet.2005.04.047 ↗
4. High temperature fracture of boron carbide: experiments and simple theoretical models10.1007/BF02403232 ↗
5. Characterization of solidified melt among materials of UO2 fuel and B4C control blade10.1080/00223131.2014.912567 ↗
6. Mechanical, tribological, and thermal properties of hot-pressed ZrB2 -B4C composite10.1111/ijac.12290 ↗
7. A Monte Carlo calculation of the formation of planetesimals from fluffy aggregates
8. Hot-pressing of MoSi2 reinforced B4C composites10.1016/j.ceramint.2014.06.135 ↗
9. Densification behaviour and mechanical properties of B4C-SiC intergranular/intragranular nanocomposites fabricated through spark plasma sintering assisted by mechanochemistry10.1016/j.ceramint.2016.10.150 ↗
10. Boron carbide: structure, properties, and stability under stress10.1111/j.1551-2916.2011.04865.x ↗
11. Effect of B4C addition on the microstructures and mechanical properties of ZrB2-SiC ceramics10.4191/KCERS.2010.47.6.578 ↗
12. Spark plasma sintering of superhard B4C-ZrB2 ceramics by carbide boronizing10.1111/jace.12284 ↗
13. Microstructure and mechanical properties of Cu-B4C and CuAl-B4C composites produced by hot pressing10.1007/s12598-019-01287-2 ↗
14. Mechanical and electrical properties of B4C-CrB2 ceramics fabricated by liquid phase sintering10.1016/S0272-8842(02)00120-7 ↗
15. Corrosion and tribocorrosion behavior of Ti-B4C composites joined with TiCuNi brazing alloy10.1007/s11665-019-04217-6 ↗
16. Study on ZrC-20vol.%SiCw ultrahigh temperature ceramics by hot pressing10.4028/www.scientific.net/AMR.557-559.772 ↗
17. Preparation of B4C-ZrB2 laminated composites by non-aqueous tape casting and hot-press sintering10.4028/www.scientific.net/KEM.697.494 ↗
18. Production and properties of B4C-TiB2 composites with isotropic eutectic microstructure10.1007/s11106-018-9970-4 ↗
19. SiC whisker-reinforced B4C-Si ceramic composites
20. Micro-structure, mechanical properties and comparison of monolithic and laminated Ti-B4C composite with Al doped10.1016/j.jallcom.2017.10.270 ↗
21. In situ fabrication of B4C-NbB2 eutectic composites by spark plasma sintering10.1111/jace.13083 ↗
22. Densification behavior and mechanical properties of spark plasma reaction sintered ZrB2-ZrC-B4C ceramics from B4C-Zr system10.1016/j.ceramint.2019.03.112 ↗
23. Effect of graphite content on properties of B4C-W2B5 ceramic composites by in-situ reaction of B-Gr-WC10.1111/jace.15474 ↗
24. Microstructure and mechanical properties of B4C-TiB2-SiC composites fabricated by spark plasma sintering10.1016/j.ceramint.2019.10.102 ↗
25. On the use of Ti-Si eutectic alloy as a novel sintering aid for B4C-TiB2-SiC ceramic composites10.1016/j.ceramint.2019.03.166 ↗
26. Size effect of B4C powders on metallurgical reaction and resulting tensile properties of Ti matrix composites by in-situ reaction from Ti-B4C system under a relatively low temperature10.1016/j.msea.2014.07.020 ↗
27. In-situ synthesis and densification of B4C-(Zr,Ti)B2 composites by pulsed electric current sintering
28. Densification behaviour and mechanical properties of pressureless-sintered B4C-CrB2 ceramics10.1023/A:1021027430338 ↗
29. Fabrication and properties of in-situ pressureless-sintered ZrB2/B4C composites10.1016/j.ceramint.2017.08.115 ↗
30. Effect of Si additions on the microstructure and mechanical properties of hot-pressed B4C10.1134/S0020168517040148 ↗
31. High-temperature plastic deformation of spark plasma sintered boron carbide-based composites: the case study of B4C-SiC with/without graphite (g)10.1016/j.jeurceramsoc.2015.12.016 ↗
32. Toughening B4C/Al ceramics by in-situ CeB6 particles in B4C
33. Synthesis of boron carbide by reactive-pulsed electric current sintering in the presence of tungsten boride10.1111/ijac.12575 ↗
34. High toughness and electrical discharge machinable B4C-TiB2-SiC composites fabricated at low sintering temperature10.1016/j.msea.2017.06.100 ↗
35. Preparation of B4C–SiC composite ceramics through hot pressing assisted by mechanical alloying10.1016/j.ijrmhm.2013.04.012 ↗
36. Comparing the effects of different sintering methods for ceramics on the physical and mechanical properties of B4C-TiB2 nanocomposites10.1016/j.ijrmhm.2015.04.003 ↗
37. In situ synthesis of B4C ceramics toughened by ZrB2 particles
38. Properties of B4C ceramics prepared by pressureless sintering
39. Effect of mechanical properties and impact angles on erosion behavior of B4C/TiB2 matrix ceramic nozzle materials
40. Microstructure and properties of C-SiC-B4C composites prepared by coating processing
41. Toughening and strengthening zirconia through the addition of a transient solid solution additive10.1016/j.jeurceramsoc.2011.08.030 ↗
42. Mechanisms of toughening and strengthening in ceramic-based nanocomposites10.1016/S0167-6636(02)00129-1 ↗
43. Electrical resistivity, elastic modulus, and debye temperature of titanium diboride10.1016/0022-5088(67)90115-4 ↗
44. Microstructure and mechanical properties of hot-pressed B4C/(W,Ti)C ceramic composites10.1016/S0272-8842(01)00113-4 ↗