Synthesis and microstructure evolution of WCoB based cermets during spark plasma sintering

Tong Zhang, Haiqing Yin, Cong Zhang, Ruijie Zhang, Zi Yang, Sharon Elder, Xue Jiang, Zhenghua Deng, Guoqiang Yang, Qingjun Zheng, Xuanhui Qu

Ceramics International· Volume 45· Issue 14
Publisher page

Abstract

Abstract WCoB based cermets were prepared by spark plasma sintering at sintering temperature among 600°C-1200 °C. The phase evolution was investigated by detecting density behavior, phase composition, microstructure and mechanical properties during sintering process. The sintering process can be divided into three stages: powder densification, solid phase reaction and liquid phase sintering. WCoB hard phase forms at 1000 °C during solid phase sintering, showing better mechanical properties than Co2B, especially on Vicker's hardness. WCoB hard phase forms on the basis of Co2B binary boride and its content increases in liquid phase sintering stage with high density. The Vicker's hardness and transverse rupture strength (TRS) reach the maximum value of 1262 Hv and 1212 MPa at 1200 °C and 1170 °C, respectively. The fracture toughness reaches the maximum value of 21.8 MPa m1/2 at 1050 °C, and the inter-granular fracture is the main fracture mechanism.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. New multiple-boride base hard alloy
2. Corrosion resistance of boride base cermets in a molten aluminum alloy10.2497/jjspm.41.994 ↗
3. Metal injection molding process of Mo2FeB2 boride base cermets
4. Sintering mechanisms of Cr-containing Mo2NiB2 base hard alloys10.2497/jjspm.41.1037 ↗
5. Effects of Cr on the microstructure and mechanical properties of WCoB base hard alloys10.2497/jjspm.40.38 ↗
6. Development of ternary-boride-based hard cladding material10.1016/S0025-5408(01)00824-8 ↗
7. Development and application of high strength ternary boride base cermets10.1016/j.jssc.2006.01.023 ↗
8. Preparation and properties of WCoB cermet
9. Untersuchungen in den dreistoffen (Mo,W)–(Fe,Co,Ni)–B
10. The crystal structure of MoCoB and related compounds10.1107/S0567740868003432 ↗
11. Crystal structures of the compounds MoCoB, WCoB and WFeB
12. Preparation and some properties of boride diffusion layers on hard WC–TiC–Co alloys10.1016/0022-5088(81)90197-1 ↗
13. Microstructure development of WCoB–TiC based hard materials10.1016/S0263-4368(02)00104-X ↗
14. Microstructure, mechanical and tribological properties of WC-WCoB coating10.1016/j.jeurceramsoc.2018.07.004 ↗
15. Influence and effectivity of Sm2O3 and Cr3C2 grain growth inhibitors on sintering of WCoB–TiC based cermets10.1016/j.ceramint.2015.07.049 ↗
16. VC and Cr3C2 doped WCoB-TiC ceramic composites prepared by hot-pressing10.1016/j.ijrmhm.2017.06.005 ↗
17. Comparison of reactive and non-reactive spark plasma sintering routes for the fabrication of monolithic and composite ultra high temperature ceramics (UHTC) materials10.3390/ma6051566 ↗
18. Spark plasma sintering behavior of nanocrystalline WC–10Co cemented carbide powders10.1016/S0921-5093(02)00605-6 ↗
19. Bulk TiB2-based ceramic composites with improved mechanical property using Fe–Ni–Ti–Al as a sintering aid10.3390/ma7107105 ↗
20. Microstructure and mechanical properties of TiB2-CNTs composites prepared by spark plasma sintering10.1166/sam.2018.3392 ↗
21. Effect of Cr doping on the mechanical properties and electronic structure of WCoB ternary boride by first-principles calculations
22. Effect of Mn doping on mechanical properties and electronic structure of WCoB ternary boride by first-principles calculations10.1088/1674-1056/27/10/107101 ↗
23. First-principles study on the mechanical properties and electronic structure of V doped WCoB and W2CoB2 ternary borides10.3390/ma12060967 ↗
24. Inhomogeneous electron gas10.1103/PhysRev.136.B864 ↗
25. Self-consistent equations including exchange and correlation effects10.1103/PhysRev.140.A1133 ↗
26. First principles methods using CASTEP10.1524/zkri.220.5.567.65075 ↗
27. Bjurström · 1933
28. Compounds and pseudo-binary alloys with the CuAl2 (C16)-type structure I. Preparation and X-ray results10.1016/0022-5088(72)90028-8 ↗
29. Special points for Brillouin-zone integrations10.1103/PhysRevB.13.5188 ↗
30. B-Co reference phase diagrams
31. Modeling hardness of polycrystalline materials and bulk metallic glasses10.1016/j.intermet.2011.03.026 ↗
32. Effect of initial Co content on the microstructure, mechanical properties and high-temperature oxidation resistance of WCoB-TiC ceramic composites10.1016/j.ceramint.2017.10.046 ↗
33. Neck formation and self‐adjusting mechanism of neck growth of conducting powders in spark plasma sintering10.1111/j.1551-2916.2005.00777.x ↗
34. Hardness to toughness relationship of fine-grained WC-Co hardmetals10.1016/S0263-4368(98)00028-6 ↗
35. A novel rapid route for synthesizing WC–Co bulk by in situ reactions in spark plasma sintering10.1016/j.msea.2008.09.007 ↗