Continuous and varied depth-of-cut turning of gray cast iron by using uncoated and TiN/Al2O3 coated silicon nitride-based ceramic tools
Source abstract
Abstract
Abstract Silicon nitride-based (Si3N4) ceramic cutting tools are particularly good for high speed machining of gray cast iron due to their high red hardness, wear resistance and chemical stability with gray cast iron. However, the intrinsic brittleness of Si3N4 ceramics makes the cutting tools easy to be damaged when subjected to impact force. In the present work, turning tests on gray cast iron were carried out by using uncoated and CVD TiN/Al2O3 coated Si3N4 cutting tools under continuous turning and varied depth-of-cut turning. Tool wear, tool life, chemical composition on worn flank faces and failure mechanism of the cutting tools after turning tests were studied. The results show that the improved cutting performance of the coated cutting tools can be attributed to the increasing wear resistance and toughness of the cutting tools with the covering of TiN/Al2O3 coatings, both in continuous and varied depth-of-cut turning. The dominant failure mechanism of the cutting tools was abrasive wear in continuous turning and a combination of abrasive wear and chipping in varied depth-of-cut turning. In addition, adhesive wear also found to play a role in the tools failure to some extent for both uncoated and coated Si3N4 cutting tools in continuous and varied depth-of cut turning.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Metal Alloys Wear and Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Cutting forces in turning of gray cast iron using silicon nitride based cutting tool10.1016/j.matdes.2008.09.041 ↗
2. Stokes · 2008
3. Trent · 2000
4. Wear behavior of Si3N4 ceramic cutting tool material against stainless steel in dry and water-lubricated conditions10.1016/S0272-8842(98)00040-6 ↗
5. Whitney · 1994
6. Structure and properties of PVD and CVD coated Al2O3 +TiC mixed oxide tool ceramics for dry on high speed cutting processes10.1016/j.jmatprotec.2005.02.089 ↗
7. Tribological properties of the PVD and CVD coatings deposited onto the nitride tool ceramics10.1016/j.jmatprotec.2005.04.032 ↗
8. How TiN coatings improve the performance of high speed steel cutting tools10.1016/0257-8972(90)90172-9 ↗
9. Tool life and wear mechanism of uncoated and coated milling inserts10.1016/S0043-1648(99)00074-5 ↗
10. Inclined impact-sliding wear tests of TiN/Al2O3/TiCN coatings on cemented carbide substrates10.1016/j.surfcoat.2011.09.067 ↗
11. CeramTec, SPK Tools for turning, 〈http://www.ceramtec.com/files/wz_spk-drehwerkzeuge_de_en_fr.pdf〉, 2010.
12. Cubic boron nitride tool wear in interrupted hard cutting10.1016/S0043-1648(99)00012-5 ↗
13. Turning of interrupted and continuous hardened steel surfaces using ceramic and CBN cutting tools10.1016/j.jmatprotec.2011.01.002 ↗
14. MIT, Ductile Iron Data for Design Engineer, 〈http://doc.diytrade.com/docdvr/229183/22426195/1310704970.pdf〉, 2001.
15. Documentation of tool wear progress in the machining of nodular ductile iron with silicon nitride-based ceramic tools10.1016/j.cirp.2011.03.083 ↗