journal article·2007-04

Mechanical properties of Al4SiC4 bulk ceramics produced by solid state reaction

Xiao-xiao Huang, Guang-wu Wen

Ceramics International· Volume 33· Issue 3
Publisher page

Abstract

Abstract The mechanical properties at ambient and high temperature of Al4SiC4 bulk ceramics prepared by solid state reaction were investigated. By increasing the sintering temperature slightly, the room temperature bending strength increased up to 318 MPa, whereas, the fracture toughness decreased with the increase of the sintering temperatures. The high temperature bending strengths of the Al4SiC4 ceramics exhibited anomalous increases within certain temperature ranges especially at 1300 °C in air with the highest value of 449.7 MPa, i.e. about 1.5 times of that at room temperature (300 MPa). The self-healing behavior of the flaws on the specimen surface due to the oxidation of the surface layer of the Al4SiC4 ceramics is considered to be the main strength-enhancing mechanism at high temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. X-ray crystallographic data on aluminum silicon carbide—Al4SiC4 and Al4Si2C510.1007/BF00551719 ↗
2. Reaction in Al–Ti–C powders and its relation to the formation and stability of TiC in Al at high temperatures10.1016/S1359-6462(00)00356-0 ↗
3. Phase relation associated with the aluminum blast furnace: aluminum oxycarbide melts and Al–C–X (X=Fe, Si) liquid alloy10.1007/BF02656164 ↗
5. Preparation and oxidation of Al4SiC410.1557/JMR.2002.0113 ↗
6. Thermal conductivity and temperature dependence of linear thermal expansion coefficient of Al4SiC4 sintered bodies prepared by pulse electronic current sintering10.2109/jcersj.111.348 ↗
7. Fabrication and oxidation resistance of Al4SiC4 body10.2109/jcersj.110.1010 ↗
8. Temperature dependence of electrical resistivity of the Al4SiC4 sintered bodies prepared by pulse electronic current sintering10.2109/jcersj.111.267 ↗
9. Stacking fault analysis in layered materials10.1016/S1466-6049(01)00143-X ↗
10. Processing of in situ toughened B-W-C composites by reaction hot pressing of B4C and WC10.1016/S1359-6462(00)00502-9 ↗
11. Reaction synthesis of TiB2–TiC composites with enhanced toughness10.1016/S1359-6454(01)00034-9 ↗
12. Fabrication and properties of laminated Al2O3/TiC composites10.1016/S0272-8842(01)00007-4 ↗
13. Microcracking in B4C–TiB2 composites10.1111/j.1151-2916.1995.tb08671.x ↗
14. Crack growth resistance of microcracking brittle materials10.1111/j.1151-2916.1993.tb07757.x ↗
15. The mechanical behaviour of ceramics matrix composites10.1016/0001-6160(89)90291-5 ↗
16. Cao · J. Am. Ceram. Soc. · 1990 · 73 · 169110.1111/j.1151-2916.1990.tb09814.x ↗
17. Fundamental condition for the existence of microcrack clouds in monophase ceramics10.1016/0955-2219(91)90048-5 ↗
18. R. Bacon, W. Smith, Extended abstracts, in: Proceedings of the Second Conference on Industrial Carbon and Graphite, London, 1965, p. 203.
19. Crack healing behavior of structure ceramics under constant and cyclic stress at high temperature10.2109/jcersj.110.741 ↗
20. High temperature mechanical behaviour of liquid phase sintered silicon carbide10.1016/S0955-2219(97)00163-5 ↗
21. Oxidation of polycrystalline silicon carbide ceramics10.1016/S0272-8842(96)00051-X ↗