Microstructure and mechanical properties of ZrB2–SiC joints fabricated by a contact-reactive brazing technique with Ti and Ni interlayers
Source abstract
Abstract
Abstract A contact-reaction brazing technique with Ti and Ni interlayers was used to join ZrB2–SiC ceramics. The influence of Ti–Ni stack methods and Ti content to the microstructure of the joint was investigated. It was found that Ni could infiltrate into ZrB2–SiC during the heating process and led to excessive interfacial reactions. The TiB whiskers could be in situ synthesized in all range of Ti concentration (55–79 at% Ti) with Ti/Ni/Ti stack foils. Due to the diffusion behavior of Ti, B atoms and low interfacial energy of TiB in TiNi phase, a cross woven structure of TiB whisker was produced in the brazing seam. The microhardness tests demonstrated tight bonding between TiB and the matrix. The highest shear strength of 134 MPa was obtained from 65 at% Ti.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Improving high temperature properties of hot pressed ZrB2–20vol% SiC ceramic using high purity powders10.1016/j.ceramint.2012.06.018 ↗
2. Processing and properties of zirconium diboride-based composites10.1016/S0955-2219(01)00284-9 ↗
3. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
4. Oxidation kinetics of hot-pressed ZrB2–SiC ceramic matrix composites10.1016/j.ceramint.2012.09.091 ↗
5. Wettability of zirconium diboride ceramics by Ag, Cu and their alloys with Zr10.1016/S1359-6462(02)00361-5 ↗
6. Liquid metal/ceramic interactions in the (Cu, Ag, Au)/ZrB2 systems10.1016/j.jeurceramsoc.2006.12.008 ↗
7. Reactive vs non-reactive wetting of ZrB2 by azeotropic Au–Ni10.1016/j.actamat.2007.07.037 ↗
8. Microstructural evolution and growth behavior of in situ TiB whisker array in ZrB2–SiC/Ti6Al4V brazing joints10.1111/jace.12629 ↗
9. ZrB2–SiC/Ti6Al4V joints: wettability studies using Ag- and Cu-based braze alloys10.1007/s10853-012-6790-7 ↗
10. M.L. Muolo, E. Ferrera, L. Morbelli, C. Zanotti, A. Passerone, Joining of zirconium boride based refractory ceramics to Ti6A14V, in: Proceedings of the International Symposium on Materials in a Space Environment, 540, 2003, 467–472.
11. Microstructural investigation of in situ TiB whiskers array reinforced ZrB2–SiC joint10.1016/j.jallcom.2012.03.016 ↗
12. Joining of zirconium diboride-based ultra high-temperature ceramic composites using metallic glass interlayers10.1016/j.msea.2007.01.015 ↗
13. Joining and integration of ZrB2-based ultra-high temperature ceramic composites using advanced brazing technology10.1007/s10853-010-4510-8 ↗
14. Joining ZrB2–SiC composites using glass interlayers10.1007/s10853-005-2813-y ↗
15. Diffusion bonding of ZrB2–SiC and Nb using dynamic compressed Ni foam interlayer10.1016/j.msea.2013.02.047 ↗
16. Diffusion bonding of ZrB2–SiC/Nb with in situ synthesized TiB whiskers array10.1016/j.jeurceramsoc.2012.07.005 ↗
17. Equilibrium between MB2 (M=Ti, Zr, Hf) UHTC and Ni: a thermodynamic database for the B–Hf–Ni–Ti–Zr system10.1016/j.calphad.2011.10.003 ↗
18. Villars · 1995
19. Rates of evaporation in a vacuum in liquid Ni–Ti alloys10.2355/isijinternational.38.789 ↗
20. Phase equilibria and transformations in a Ti–Zr–Si system10.1007/BF02664663 ↗
21. Hydrogenation characteristics of ternary alloys containing Ti4Ni2X (X=O, N, C)10.1016/S0925-8388(00)01118-X ↗
22. Jie · 2010
23. Brazing of Al2O3 to Ti–6Al–4V alloy with in situ synthesized TiB-whisker-reinforced active brazing alloy10.1016/j.ceramint.2011.05.004 ↗