journal article·2011-05

Sintering behavior of nanostructured WC–Co composite

Akshay Kumar, K. Singh, O.P. Pandey

Ceramics International· Volume 37· Issue 4
Publisher page

Abstract

Abstract Sintering of nanocrystalline WC–Co, retaining the nanoscaled grain sizes is a matter of great interest. Many non traditional methods have been used to achieve this goal as the required result has not been achieved using the traditional method of liquid phase sintering. The present study is an attempt to find out the limitations of traditional sintering method and optimize it to get nanocrystalline WC–Co composites. The effect of temperature, time and composition variation has been studied to see the sintering behavior of nanostructured WC–Co composite. Detailed X-ray diffraction (XRD) analysis as well as microstructural examination showed that sintering at 1350 °C for 1 h with 5% binder composition (Co) is a set of critical temperature, time and composition which can provide the required results. The grain growth is through coalescence. At critical conditions the majorities of WC grains are faceted and attains the shape of prismatic and basal facets.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Schwartzkopf · 1960
2. Grain growth during the early stage of sintering of nanosized WC–Co powder10.1016/j.ijrmhm.2007.04.006 ↗
3. Processing and properties of nanostructured WC–Co10.1016/0965-9773(92)90063-4 ↗
4. Synthesis of nanostructured WC–12wt% Co coating using mechanical milling and high velocity oxygen fuel thermal spraying10.1007/s11661-000-0289-6 ↗
5. Synthesis of nanosized tungsten carbide powder by the chemical vapor condensation process10.1016/j.scriptamat.2004.01.015 ↗
6. Two-step synthesis of nanostructured tungsten carbide-cobalt powders10.1016/S1359-6462(01)00668-6 ↗
7. Synthesis and processing of nanostructured WC–Co materials10.1023/A:1016553426227 ↗
8. Nanostructured WC/Co composite powder prepared by high energy ball milling10.1016/j.scriptamat.2003.08.009 ↗
9. Reduction of WO3 to nano-WC by thermo-chemical reaction route10.1016/j.physe.2008.11.016 ↗
10. Optimization of processing parameters for the synthesis of tungsten carbide (WC) nanoparticles through solvo thermal route10.1016/j.physe.2010.06.002 ↗
11. Nanocrystalline materials10.1016/0079-6425(89)90001-7 ↗
12. Rearrangement and pore size evolution during WC–Co sintering below the eutectic temperature10.1016/j.actamat.2004.12.017 ↗
13. Dilatometric study of the sintering mechanism of nanocrystalline cemented carbides10.1016/0965-9773(96)00014-1 ↗
14. Schubert · 2000
15. Grain growth during the early stage of sintering of nanosized WC–Co powder10.1016/j.ijrmhm.2007.04.006 ↗
16. Conversion from nano- to micron-sized structures: experimental observations10.1016/j.jeurceramsoc.2003.10.033 ↗
17. Study of nanostructured WC–Co composites10.1016/0263-4368(95)92675-A ↗
18. An experimental study of the sintering of nanocrystalline WC–Co powders10.1016/j.ijrmhm.2005.04.014 ↗
19. Variation of WC grain shape with carbon content in the WC–Co alloys during liquid-phase sintering10.1016/S1359-6462(02)00464-5 ↗
20. Size-induced transition-temperature reduction in nanoparticles of ZnS10.1103/PhysRevB.60.9191 ↗
21. Grain growth control in microwave sintering of ultrafine WC–Co composite powder compacts
22. Initial stage sintering of binderless tungsten carbide powder under microwave radiation10.1016/j.ceramint.2010.09.036 ↗
23. Synthesis, sintering, and mechanical properties of nanocrystalline cemented tungsten carbide – a review10.1016/j.ijrmhm.2008.07.011 ↗
24. X-ray line broadening from filled aluminum and wolfram10.1016/0001-6160(53)90006-6 ↗
25. Comparison of X-ray analysis methods used to determine the grain size and strain in nanocrystalline materials10.1080/01418619908210391 ↗
26. Sintering of binderless tungsten carbide10.1016/j.ceramint.2009.10.017 ↗
27. Effect of particle size and strain in nanocrystalline SnO2 according to doping concentration of ruthenium10.1016/j.solidstatesciences.2006.02.008 ↗
28. Quantitative theory of diffusional activated sintering10.2298/SOS0601027G ↗