Pressureless sintered SiC matrix toughened by in situ synthesized TiB2: Process conditions and fracture toughness

Wei Wang, Jingbao Lian, Hongqiang Ru

Ceramics International· Volume 38· Issue 3
Publisher page

Abstract

Abstract This paper reports the fabrication of SiC toughened by in situ synthesized TiB2 based on pressure-less sintering technique using TiO2, B4C, C and SiC as starting materials. The process conditions were investigated in detail, including the pre-sintering temperatures, carbon contents, differently sized TiO2 powders, TiB2 volume contents, final sintering temperature and time. These conditions were found to have great influence on the TiB2 toughened SiC in terms of relative density, TiB2 particle size and fracture toughness. Homogeneous dispersion of in situ synthesized TiB2 secondary phase was confirmed to enhance the KIC of the SiC matrix. The KIC of SiC toughened by in situ synthesized TiB2 (15 vol%) reaches 6.3 MPa m1/2, which is among the highest values reported so far on TiB2 reinforced SiC composites based on the pressure-less sintering technique using TiO2 as Ti source.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Mechanical properties and oxidation behavior of a hot pressed SiC-15vol% TiB2 composite
2. Microstructure and materials properties of SiC–TiB2 particulate composites
3. Improvements in mechanical properties in SiC by addition of TiC particles10.1111/j.1151-2916.1984.tb19174.x ↗
4. Microstructure and mechanical properties of hot-pressed SiC–TiC composites10.1007/BF01184969 ↗
5. Microstructure and densification of ZrB2–SiC composites prepared by spark plasma sintering10.1016/j.jeurceramsoc.2009.01.011 ↗
6. Sintering of in situ synthesized SiC–TiB2 composites with improved fracture toughness10.1111/j.1151-2916.1992.tb05600.x ↗
7. SiC matrix composites reinforced with internal synthesized TiB210.1007/BF00544201 ↗
8. In situ HIP synthesis of TiB2/SiC ceramic composites
9. In situ synthesized TiB2 toughened SiC10.1016/0955-2219(95)00116-6 ↗
10. Pressureless-sintered SiC–TiB2 composite through internal synthesis method10.1007/BF00722857 ↗
11. Microstructural and mechanical characterization of SiC-submicron TiB2 composites10.1016/S0955-2219(98)00227-1 ↗
12. Toughening of SiC matrix with in situ created TiB2 particles10.1016/j.ceramint.2010.06.001 ↗
13. A critical evaluation of indentation techniques for measuring fracture toughness-II strength method10.1111/j.1151-2916.1981.tb10321.x ↗
14. New relation for the porosity dependence of the effective tensile modulus of brittle materials10.1023/B:JMSC.0000026961.12735.2a ↗
15. Effect of TiB2 in situ synthesized on presintering process and reaction of B4C and Al during fabricating B4C–TiB2–Al composite10.1007/s10853-009-3466-z ↗
16. Influence of the oxidation on the surface properties of silicon carbide10.1016/j.tca.2005.01.038 ↗
17. Study on SiC matrix composites toughened by in situ synthesized TiB2
18. Effect of microstructure on fracture of brittle materials: unified approach10.1016/j.tafmec.2006.03.005 ↗
19. Grain-size dependence of fracture energy in ceramics: I. Experimental10.1111/j.1151-2916.1981.tb10300.x ↗